Global ETD Search
Search theses and dissertations gathered from participating repositories worldwide. Every result links back to the library that holds it. No account is needed.
Results 1 to 10 of 10 for “"Iron sulfide scale"”
-
Iron Sulfide Scale Removal Using Alternative Dissolvers
Iron sulfide scales create well deliverability and integrity problems such as reduced production rates and damage to well tubulars. Problems associated with the use of HCl to remove these scales such as high corrosion rate, H2S generation, and scale reprecipitation, have required the use of …
-
Evaluation of High Pressure / High Temperature, Eco-Friendly Iron Sulfide Scale Dissolver
A high pressure, high temperature iron sulfide dissolver is not currently on the market. While a dissolver that meets these conditions needs to be developed, the corrosion rate of the dissolver, as well as the hydrogen sulfide evolution need to be considered. Although mineral acids are commonly …
-
Kinetics of Iron Carbonate and Iron Sulfide Scale Formation in CO<sub>2</sub>/H<sub>2</sub>S Corrosion
<p>Kinetics of iron carbonate and iron sulfide scale formation in CO<sub>2</sub>/H<sub>2</sub>S corrosion was investigated by individually studying iron carbonate formation in pure CO<sub>2</sub>corrosion, iron sulfide formation in N<sub>2</sub>/H<sub>2</sub>S corrosion, and the mixed iron …
-
Solubility, Precipitation Kinetic, and Chemical Control of Iron Sulfide
The iron sulfides (FeS) constitute a diverse group of solids and dissolved complexes, many of which play critical roles in the natural system, such as marine sedimentation and biochemical processes. It has also become a significant problem in various industrial processes, such as water and …
-
EIS Investigation of Carbon Dioxide and Hydrogen Sulfide Corrosion Under Film Forming Conditions
… see the effect of different saturation values of iron carbonate and iron sulfide in the bulk solution on the corrosion rate of the sample. The experiments were conducted in a large scale (1000 lit) hastelloy flow loop at a fixed temperature of 60°C and total pressure of 7.9 bar. All experimental …
-
Corrosion of Steel at High Temperature in Naphthenic Acid and Sulfur Containing Crude Oil Fractions
… mechanism of naphthenic acids in sulfur environments became a necessity in designing and operating efficiently the refinery equipment. Thus in 2004 Institute of Corrosion and Multiphase Technology started the Naphthenic Acids Project financed by ExxonMobil Research and Engineering Company …
-
Multiphase Flow Effects on Naphthenic Acid Corrosion of Carbon Steel
… of carbon steel in the presence or absence of an iron sulfide corrosion product layer, at elevated temperature and fluid flow velocities, using a small-scale annular flow rig (AFR). In parallel, it examines the hydrodynamics of a multiphase flow mixture at room temperature and high flow velocities …
-
Optimization and Thermal Stability of the THPS and NH4Cl Blend to Dissolve Iron Sulfide (FeS) Scale at HP/HT Conditions
Iron sulfide scales of different forms exist in sour oil/gas-producing wells as well as seawater injection wells. Traditionally, they are dissolved using HCl and other inorganic acids. In the past decade, a tetrakis (hydroxymethyl) phosphonium sulfate (THPS) and ammonium chloride blend have shown …
-
Κρυστάλλωση θειούχων αλάτων του σιδήρου (ΙΙ) σε υδατικά διαλύματα
Iron (II) sulfide scale formation is closely related to many of the problems impeding the efficient use of geothermal resources in most ofthe installations around the world. Geothermal fluids may contain high amounts of dissolved H2S or sulfide anions. Iron ions may be also found in the hot brines …
-
Formation of Sulfide Scales and Their Role in Naphthenic Acid Corrosion of Steels
… been conducted to investigate the corrosion and scale formation rates of CS-A106 and 5Cr-A182 exposed to different acid concentrations and varying amounts of sulfur compounds. The experiments were designed to determine the effect of time, temperature and acid concentration on the formation and …