Global ETD Search
Search theses and dissertations gathered from participating repositories worldwide. Every result links back to the library that holds it. No account is needed.
Results 1 to 9 of 9 for “"Kirkendall voids"”
-
Roles of Interfacial Reaction on Mechanical Properties of Solder Interfaces
… interface. Further aging induced numerous voids along the Cu3Sn/Cu interface. These interfacial voids were different from Kirkendall voids. Their formation was explained on basis of vacancy condensation at the interface as the Bi segregants reduced the number of effective Cu vacancy sink …
-
Environmental-(S)TEM of dynamic Catalyst Nanostructures
… of cation vacancies lead to the formation of Kirkendall voids and ultimately hollow NiO structures. Nanoparticle based catalysts for industrial methanation reactions were studied using ESTEM. The study focuses on the origin of enhanced catalytic activity via the addition of a ceria promoter. …
-
Reliability of high-density lead-free solder interconnections under thermal cycling and mechanical shock loading
… reliability considerably due to the formation of Kirkendall voids in the Cu3Sn intermetallic layers.
-
Advanced metallization for screen-printed solar cells
… of the process conditions to minimize the Kirkendall void formation while maintaining an adequate thickness of localized back surface field is presented. Cell efficiency of over 20% is demonstrated on solar grade p-type CZ substrate. An alternative approach is investigated in which deep …
-
Grain boundary and Se diffusion investigations in CdSe-CdTe thin-film photovoltaics
… layer. The results showed that both devices have voids at the inter-diffusion layer, although for the 400 nm CdSe sample voids were more numerous. Rapid diffusion of Se along the CdTe grain boundaries led to small grains at the interface region, due to Kirkendall voids and solute pinning of the …
-
Die-Attachment on Copper by Nanosilver Sintering: Processing, Characterization and Reliability
… interface from the reliability issue related to Kirkendall voids, which often took place in tin (Sn) -based solder joints.
-
Effect of Surface Treatment on Joint Performance and Fracture Morphology in Adhesively Bonded Al-Si Coated Ultra-High Strength Steel
… coating morphology included microcracks and Kirkendall voids, which facilitated coating delamination. The intermetallic coating delamination was associated with a measured SLS joint rotation of 2.5°-2.8° for all three thermal treatments, while the measured joint strength decreased as the …
-
Nanoscale Material Characterization of Silicon Nanowires for Application in Reconfigurable Nanowire Transistors
… proportional to the cross-sectional area. The voids were formed by the reduced diffusivity of Ni in Ni2Si phase in comparison to phases with lower percent of Ni. This indicates that the reason behind the phenomenon is coalition of Kirkendall voids and thus dependent on volume diffusion. From …
-
Optimisation d'un procédé de soudage par difusion à l'état solide pour réaliser des circuits imprimés : Application au système Au-Cu-Sn
… a permis d'observer une diminution des vides de Kirkendall lors de la consommation de la phase B par les composés binaires.Des essais de nanoindentation ont été réalisés pour mesurer les propriétés mécaniques des différentes composés intermétalliques, dont la phase B (avec un module d'Young de …