Showing 1 to 12 of 12 for “"Kissing bond"”.
-
ONSET OF KISSING BOND FORMATION FOR VARYING LEVELS OF BONDLINE CONTAMINATION IN CFRP
… the aerospace industry. CFRP utilizes adhesive bonding as the primary joining method and may suffer from a defect known as a kissing bond. This occurs when there is very close contact between the CFRP substrate and the adhesive yet very low bond strength. This makes kissing bonds very difficult …
-
Microstructure-property development and defect characterization of Al-X friction welds for automotive applications
… were evaluated, with a special focus on the kissing bond defect, which can have a substantial effect on the microstructure and properties of the FSW joints. It was found that the length of the kissing bond had a reasonably linear relation with heat input (HI), which depends mostly on the tool …
-
DETECTION OF DEFECTS IN COMPOSITE LAMINATES WITH VIBRO-ULTRASONIC METHODS
… methods for detection of delamination and kissing bond defects in composite laminates. It has been demonstrated through a series of experiments and simulations that while delaminations and dry contact kissing bonds can be detected with nonlinear vibro-acoustic/ultrasonic procedures, …
-
The development of non-collinear non destructive evaluation of aircraft materials
… was selected to investigate sensitivity over kissing bonds, a type of defect of great interest in the aerospace industry mainly due to the luck of conventional procedures that can detect them. Initially, a set-up of two partially closed interfaces was designed to simulate a kissing bond; an …
-
BOND STRENGTH EVALUATION IN ADHESIVE JOINTS USING NDE AND DIC METHODS
Adhesive bonding of graphite epoxy composite laminates to itself or traditional metal alloys in modern aerospace and aircraft structural applications offers an excellent opportunity to use the most efficient and intelligent combination of materials available thus providing an attractive package for …
-
3D printed strain sensors for soft sensing and actuation
… near-zero air gap, i.e., adjacent tracks form a kissing bond, can achieve a gauge factor of ~2300 perpendicular to the raster orientation and a gauge factor of ~1 parallel to the raster orientation. The maximum directional selectivity of this ultra-sensitive sensor is 50.5, which is unprecedented …
-
Fabrication, testing and analysis for non-destructive inspection of bonded composite joints
… issue with using CFRP is creating a reliable bonded joint for joining and repair applications during both manufacturing and services/maintenance. For various reasons, using conventional fasteners is not desirable for creating CFRP joints. Instead, adhesives are widely used to bond CFRP to …
-
Detection of kissing bonds with non-collinear nonlinear ultrasound
The development of cost effective and reliable bonded structures ideally requires an NDT method to detect the presence of poor quality, weak, or kissing bonds. If these bonds are more compliant in tension than in compression stress-strain nonlinearities provide a possible route to detection with …
-
Fatigue Behaviour of Aluminum Friction Stir Welds Under Highway Bridge Conditions
… lives were observed in the specimens with “kissing bond” defects at the weld root (on the order of approximately 1 mm in depth), 2) toe flash, undercut, and worm hole defects, as well as surface improvement by polishing were seen to have a much lower influence on fatigue performance, 3) a …
-
Probabilistic Strain-Based Fracture Mechanics Analysis of Weldments
… misalignment, toe flash, lack of penetration or “kissing bond”, and wormhole defects. As fatigue testing becomes time-consuming and expensive, numerical modelling and simulation provide complementary ways to assess the effects of parameter variations on fatigue performance. With this in mind, a …
-
Tool eccentricity in thick-plate aluminum alloy friction stir welds
… alloy. However, it was found that, when a 0.2 mm kissing bond defect is present, the ‘soft zone’ of the periodic band could deviate the fracture path to force it to propagate through the stir zone, which can be potentially detrimental to the joint integrity. Finally, concerning the FSW process, it …
-
Weak bond detection in composites using solitary waves
… using adhesives. This research focuses on bonded composite structures. A prevailing problem in bonded joints is the indeterminate nature of the strength of the adhesive bond. Low strength bonds, i.e., weak bonds, are very difficult to detect and may become the cause of catastrophic failure. …