Showing 1 to 20 of 36 for “"Liquation"”.

  1. Weldability of Modified 800H alloys

    … discussed in this dissertation in terms of HAZ liquation cracking and HAZ softening tendency. Fundamental studies of the mechanisms of HAZ liquation cracking and HAZ softening behavior in Modified 800H alloy are addressed. This research is part of a DOE project entitled "Investigation of Welding …

    utk-theses Repository record for Weldability of Modified 800H alloys (opens in a new tab)

  2. Microstructural Analysis of Linear Friction Welded Joint in Nickel-Base Inconel 738 Superalloy

    … in nature, has been attributed to the liquation of various phases in the alloy, subsequent wetting of the grain boundaries by the liquid and decohesion along one of the solid-liquid interfaces due to on-cooling tensile stresses. To address the problem of liquation cracking in weldments, …

    manitoba Repository record for Microstructural Analysis of Linear Friction Welded Joint in Nickel-Base Inconel 738 Superalloy (opens in a new tab)

  3. Evaluation of the Potential for Weld-Related Cracking in Cast 20Cr-32Ni-1Nb Heat-Resistant Stainless Steel

    … exposure this alloy exhibits problems with liquation cracking in the base metal heat-affected zone (HAZ) during repair welding. In the work presented herein, two heats of material from centrifugally-cast manifold components were evaluated to quantify the potential susceptibility to HAZ …

    ut-knoxville Repository record for Evaluation of the Potential for Weld-Related Cracking in Cast 20Cr-32Ni-1Nb Heat-Resistant Stainless Steel (opens in a new tab)

  4. Fiber laser welding of nickel-based superalloy Inconel 718

    … in the laser welding of IN 718 is that liquation cracking occurs. In the present work, autogenous fiber laser welding of IN 718 was used to study the effects of welding parameters and different pre-weld heat treatments on liquation cracking. Contrary to previous studies, a dual effect of …

    manitoba Repository record for Fiber laser welding of nickel-based superalloy Inconel 718 (opens in a new tab)

  5. A study of laser-arc hybrid weldability of nickel-base INCONEL 738 LC superalloy

    … to heat-affected zone (HAZ) intergranular liquation cracking. An improvement in weldability could be realized by the deployment of innovative welding processes and/or the modification of the materials’ microstructural characteristics. Laser-arc hybrid welding is a relatively new welding …

    manitoba Repository record for A study of laser-arc hybrid weldability of nickel-base INCONEL 738 LC superalloy (opens in a new tab)

  6. Mechanisms of Hot-Cracking During Electron Beam Powder Bed Fusion of Co-29Cr-10Ni-7W Alloy

    … is not clear as to whether solidification or liquation cracking is the initiation mechanism and how these two contribute to crack growth during EB-PBF of difficulty-to-weld alloys. The major aim of this work is to understand the solidification, how cracks develop and the contributions of …

    auckland-tech Repository record for Mechanisms of Hot-Cracking During Electron Beam Powder Bed Fusion of Co-29Cr-10Ni-7W Alloy (opens in a new tab)

  7. Heat Affected Zone Cracking of Allvac 718Plus Superalloy during High Power Beam Welding and Post-weld Heat Treatment

    … superalloy was associated with grain boundary liquation. However, despite a more extensive liquation of grain boundaries and grain interior in the HAZ of high heat input welds, no cracking occurred. This was attributed to the combination of lower welding stresses generated during cooling, and …

    manitoba Repository record for Heat Affected Zone Cracking of Allvac 718Plus Superalloy during High Power Beam Welding and Post-weld Heat Treatment (opens in a new tab)

  8. Weldability of nuclear grade austenitic stainless steels

    … cracking was found to depend on grain boundary liquation. The content of the "harmful elements" was considered as a significant factor affecting the base metal HAZ hot cracking susceptibility since the "harmful elements" (such as S and P) may decrease the liquation temperature and thus, increase …

    ut-knoxville Repository record for Weldability of nuclear grade austenitic stainless steels (opens in a new tab)

  9. A study on laser weldability improvement of newly developed Haynes 282 superalloy

    … (HAZ) cracking in the alloy is the sub-solidus liquation reaction of intergranular M5B3 borides in the material. Further weldability study showed that the HAZ liquation cracking problem worsens with reduction in welding heat input, which is normally necessary to produce the desired weld geometry …

    manitoba Repository record for A study on laser weldability improvement of newly developed Haynes 282 superalloy (opens in a new tab)

  10. A study of arc weldability of γ′-strengthened cobalt-based superalloy

    … of HAZ cracking in this alloy is intergranular liquation due to the subsolidus liquation reaction of the MC-type carbides and γ′ precipitates, which are identified by electron microscopy and spectroscopy to be present in the material before welding. Detailed weldability studies reveal that the …

    manitoba Repository record for A study of arc weldability of γ′-strengthened cobalt-based superalloy (opens in a new tab)

  11. High temperature cracking of nickel chromium austenitic steels.

    … (solidification cracking in the weld metal and liquation cracking in the HAZ (Heat Affected Zone) ): Type 2 - separations associated with relatively clean grain boundaries caused by grain boundary sliding in the solid state and they are synonymous with creep rupture. This form of cracking is …

    sheffield-hallam Download PDF for High temperature cracking of nickel chromium austenitic steels. (opens in a new tab)

  12. A microstructural study of HAZ cracking in conventionally and directionally cast polycrystalline and single crystal IN-738 LC

    … intergranular in nature and associated with liquation of secondary solidification products (such as MC carbides,  -  eutectic phases), and solid state reaction products ( precipitate particles) that are present along the grain boundaries in the pre-weld material. The current research was …

    manitoba Repository record for A microstructural study of HAZ cracking in conventionally and directionally cast polycrystalline and single crystal IN-738 LC (opens in a new tab)

  13. Dissimilar Joining of Al (AA2139) – Mg (WE43) Alloys Using Friction Stir Welding

    … at interface due to formation of IMCs caused by liquation during FSW. A good strength sound weld was obtained using processing parameter of 1200 rev/min rotational speed; 76.2 mm/min traverse speed; 1.5 degree tilt and 0.13 mm offsets towards aluminum. The crack faded away as the tool was offset …

    unt Repository record for Dissimilar Joining of Al (AA2139) – Mg (WE43) Alloys Using Friction Stir Welding (opens in a new tab)

  14. The Effects of Weld Thermal Cycles on Additively Manufactured 316L Stainless Steel

    … hardening region, recrystallization region, and liquation region. The additively manufactured 316L shows poor ductility compared to wrought 316L stainless steel. Also, there is a noticeable difference in ductility between laser pattern. Finally, ductility after the thermal cycle shows higher than …

    calpoly Repository record for The Effects of Weld Thermal Cycles on Additively Manufactured 316L Stainless Steel (opens in a new tab)

  15. Weldability and microstructural analysis of nuclear grade austenitic stainless steels

    … (fusion zone solidification cracking and HAZ liquation cracking) of modified nuclear grade and standard austenitic stainless steels. Extensive microstructural characterization using state-of-the art analytical electron microscopy (TEM and STEM) as well as SEM (EDAX) and OLM was performed to …

    utk-theses Repository record for Weldability and microstructural analysis of nuclear grade austenitic stainless steels (opens in a new tab)

  16. Characterisation of aluminium armour alloy AA7017-T651

    … maintained below 0.3wt% in order to prevent liquation cracking and hence allow them to be welded. These medium strength Al-Zn-Mg(-Cu) alloys are mostly found in light weight armoured vehicles due to their weldability, low density and good ballistic performance. There is however very little …

    birmingham Download PDF for Characterisation of aluminium armour alloy AA7017-T651 (opens in a new tab)

  17. Evaluation of the hot cracking sensitivity of 316 NG, 347 and 304 stainless steels using the hot ductility test and the modified subscale varestraint test

    … at the ZDT is related to the grain boundary liquation, there are two types of secondary cracks; first one is along the grain boundary which is roughly parallel to the fracture surface, second one is along the preferentially melted segregation bands. In AISI 347, the second type of secondary …

    ut-knoxville Repository record for Evaluation of the hot cracking sensitivity of 316 NG, 347 and 304 stainless steels using the hot ductility test and the modified subscale varestraint test (opens in a new tab)

  18. Influence of Phase Transformations on the Residual Stress Evolution and Cracking Tendency in CM247LC Nickel-base Superalloy

    … at the grain boundary as well as constitutional liquation of the MC carbide particles is identified as a source of cracking. Thiscracking tendency is correlated to the crystallographic misorientation between adjacent grains. It is found that cracking only occurs at grain boundaries misoriented …

    utk-theses Repository record for Influence of Phase Transformations on the Residual Stress Evolution and Cracking Tendency in CM247LC Nickel-base Superalloy (opens in a new tab)

Page 1 of 2