  1. Standoff Screws Used In Composite Joists

    … failure modes, concrete rib failures, and longitudinal splitting of solid concrete slabs, are presented.

    vt Repository record for Standoff Screws Used In Composite Joists (opens in a new tab)

  2. Radiographic determination of the lay-up influence on fatigue damage development under bearing/bypass conditions

    … coupons recorded the extent of damage, mostly longitudinal splitting and bearing failure, as a function of the cycle count. The following lay-ups were included: [45/90/-45/02/45/02/-45/0]s, [04/45/03/90/0]s, [±5/65/(±5)2/-65/±5]s, and [±5/65/(±5)2/-65/5/65]s, In particular, the objective was to …

    gatech Repository record for Radiographic determination of the lay-up influence on fatigue damage development under bearing/bypass conditions (opens in a new tab)

  3. Characterizing the fatigue damage in non-traditional laminates of carbon fiber composites using radiography

    … laminates recorded the extent of damage, mostly longitudinal splitting, as a function of the cycle count. The following lay-ups were included in the experiment: [45/90/-45/02/45/02/-45/0]s, [±5/65/(±5)2/-65/±5]s, and [±5/65/(±5)2/-65/5/65]s. More specifically, the objective of this study was to …

    gatech Repository record for Characterizing the fatigue damage in non-traditional laminates of carbon fiber composites using radiography (opens in a new tab)

  4. Further Investigation of Standoff Screws Used in Composite Joists

    … failure modes, concrete cone failures and longitudinal splitting, are presented.

    vt Repository record for Further Investigation of Standoff Screws Used in Composite Joists (opens in a new tab)

  5. Longitudinal Slab Splitting in Composite Girders

    Longitudinal slab splitting in composite hot rolled girders and joist girders was investigated. Two different type of framing configurations were studied with two tests conducted per configuration. The framing configurations were designated as either flush-framed or haunched, which describes the …

    vt Repository record for Longitudinal Slab Splitting in Composite Girders (opens in a new tab)

  6. Roller Compaction: Mechanistic understanding of ribbon splitting and sticking

    … desired (intact ribbon) and undesired (ribbon splitting/sticking) bond formation. The phenomenon of ribbon splitting/sticking could originate from either process or formulation related causes; due to the imbalanced combination of material mechanical properties and stress application which has …

    whiterose Download PDF for Roller Compaction: Mechanistic understanding of ribbon splitting and sticking (opens in a new tab)

  7. Micromechanics characterization of sublaminate damage

    … For a laminate containing transverse crack and longitudinal splitting the displacements and stresses in the fibers and the matrix arc obtained, and the growth of damage is investigated by using a point stress failure criterion. The investigation includes fiber stress distribution in zero degree …

    must-thes Repository record for Micromechanics characterization of sublaminate damage (opens in a new tab)

  8. Experimental and Numerical Characterisation of Fatigue Damage in Z-pinned Composite Structures

    … SEM images show the same failure mechanisms, longitudinal splitting and tensile fibre failure, in in fatigued and non-fatigued specimens.<br/>The findings from the micro mechanical study were transferred into a phenomenological model and validated with bespoke meso-scale Double Cantilever Beam …

    bristol Repository record for Experimental and Numerical Characterisation of Fatigue Damage in Z-pinned Composite Structures (opens in a new tab) Download PDF for Experimental and Numerical Characterisation of Fatigue Damage in Z-pinned Composite Structures (opens in a new tab)

  9. Effects of GFRP Reinforcement on the Compressive Behaviour of Square SPF Timber Columns

    … to higher strains. Failure modes involving longitudinal splitting were eliminated amongst reinforced specimens, and the damage was localized to a small area of wood characterized by wood fibre crushing. The thinnest reinforcement arrangements provided least improvement; samples with other …

    waterloo Repository record for Effects of GFRP Reinforcement on the Compressive Behaviour of Square SPF Timber Columns (opens in a new tab)

  10. The use of optical techniques to assess the damage tolerance of composite materials

    … transverse cracking, delaminations and longitudinal splitting, verified through the use of X-ray computed tomography (CT).<br/><br/>Finally, future improvements are recommended with an aim of future users applying the optical methodologies to a greater range of loading scenarios and to …

    soton Download PDF for The use of optical techniques to assess the damage tolerance of composite materials (opens in a new tab)

  11. The residual strength determination due to fatigue loading by fracture mechanics in notched composite materials

    … strength was attributed to the elliptical hole, longitudinal splitting, matrix cracking (reduction moduli of plies), crack propagation and local delamination. Due to the thin through-the-thickness notched laminate, two-dimensional FEM was used and interlaminar stresses were not considered. …

    vt Repository record for The residual strength determination due to fatigue loading by fracture mechanics in notched composite materials (opens in a new tab)

  12. The Fatigue Behaviour of Tension Lap Spliced Reinforced Concrete Beams Strengthened with Fibre Reinforced Polymer Wrapping

    … that exceeded the fatigue life limits for a longitudinal bar. As expected, these beams failed by fatigue rupture of the longitudinal steel bars. The GFRP and CFRP sheets increased the fatigue strength (measured as the applied load range for a given fatigue life) of the wrapped beams for all …

    waterloo Repository record for The Fatigue Behaviour of Tension Lap Spliced Reinforced Concrete Beams Strengthened with Fibre Reinforced Polymer Wrapping (opens in a new tab)

  13. BEHAVIOUR OF SLOTTED AND FLEXIBLE PERFOBOND RIB SHEAR CONNECTORS

    … perfobond ribs, failure was triggered by the longitudinal splitting of the concrete slab along the line of the shear connector, followed by the crushing of concrete in the bearing zone immediately in front of the perfobond rib. A considerable deformation was observed in the perfobond rib …

    sask Repository record for BEHAVIOUR OF SLOTTED AND FLEXIBLE PERFOBOND RIB SHEAR CONNECTORS (opens in a new tab)

  14. Timber and Timber-Timber Composite (TTC) Beams with Openings: Laboratory Experimentation and Nonlocal Finite Element Simulation

    … tensile stresses perpendicular to the grain and longitudinal splitting shear stresses. Furthermore, quasi-brittle failure of the timber in shear and tension (promoted by openings) leads to localisation of strain, spurious sensitivity of finite element (FE) simulations with respect to mesh size …

    unsw Repository record for Timber and Timber-Timber Composite (TTC) Beams with Openings: Laboratory Experimentation and Nonlocal Finite Element Simulation (opens in a new tab)