Global ETD Search
Search theses and dissertations gathered from participating repositories worldwide. Every result links back to the library that holds it. No account is needed.
Results 1 to 14 of 14 for “"Low-k films"”
-
Surface processing of nanoporous low dielectric constant thin films
… have been carried out on MSQ-based porous low-k films in resolving some key issues in the low-k materials and copper damascene integration. Nanoporous low-k films were treated by using low frequency NH3 plasma in order to form a surface densified layer, which can effectively seal the porous …
-
Characterization of Interfacial Mechanical Properties Using Wedge Indentation Method
… of the submicron thin film structures. Following the hypothetical operations of indentation-induced interface delamination introduced by Marshall and Evans, the analytical solution for interface toughness in terms of strain energy release rate is derived, where the indentation induced …
-
Plasma-enhanced chemical vapor deposition of low dielectric constant materials
… dioxide (SCCO2) were used to create nanoporous low dielectric constant (low-k) films. A material with low dielectric constant (~2) is needed to reduce the crosstalk noise and the dissipated power in these circuits. Amorphous SiC:H/SiO/C:H films were deposited using PECVD. Aimealing treatments …
-
Effects of Plasma, Temperature and Chemical Reactions on Porous Low Dielectric Films for Semiconductor Devices
Low-dielectric (k) films are one of the performance drivers for continued scaling of integrated circuit devices. These films are needed in microelectronic device interconnects to lower power consumption and minimize cross talk between metal lines that "interconnect" transistors. Low-k materials …
-
Adhesion Comparison of Low Dielectric Constant Thin Films Using Four Point Bend and Nanoscratch Testing
… with mechaincal and adhesion failure in low dielectric constant (low-k) thin films. In this thesis the four point bend test and nanoscratch test method was used for evaluating adhesion of boro-phosphate-silicate glass (BPSG) and tetraethylorthosilicate (TEOS) low-k thin films to silicon …
-
Control of Plasma Etching of Semiconductor Surfaces
… beam was used on porous silicon dioxide based low-k films to remove silanol groups that were generated due to the damage of films during pattern transfer. At H2 atom beam process at 150 C moved close to 60% silanol groups were removed in less than 3 min with an etching rate of 15 A/min. The …
-
High Temperature Water as an Etch and Clean for SiO2 and Si3N4
… and clean of thermally grown SiO2, Si3N4, and low-k films. High temperature deuterium oxide (HT-D2O) behaves similarly to HTW; however, it dissociates an order of magnitude less than HTW resulting in an equivalent reduction in reactive species. This allowed for the effects of reactive specie …
-
Ultra-thin MFI zeolite films: Synthesis, Characterization and Progress Toward Industrial Applications
… progress towards synthesis of even thinner films and membranes has been made. The discovery of a novel deposition technique enables the transfer of monolayers of nanosheets to silicon wafers. By intergrowing them, the thinnest-ever MFI films have been synthesized. In future, this technique …
-
Deposition and characterization studies of boron carbon nitride (BCN) thin films prepared by dual target sputtering
… good candidate for being hard, dense, pore-free, low-k dielectric with values in the range of 1.9 to 2.1. Excellent mechanical properties such as adhesion, high hardness and good wear resistance have been reported in the case of sputtered BCN thin films. Problems posed by high hardness materials …
-
Plasma Interactions on Organosilicate Glass Dielectric Films and Emerging Amorphous Materials- Approach to Pore Sealing and Chemical Modifications
… studies of nanoporous organosilicate glass (OSG) films point to the separate roles of radicals vs. VUV photons in the carbon abstraction. The studies indicate that reaction with O2 in presence of VUV photons (~123 nm) result in significant carbon abstraction within the bulk and that the kinetics …
-
Interaction between plasma and low-k dielectric materials
… scaling of devices, integration of porous ultra low-κ dielectric materials into Cu interconnect becomes necessary. Low-k dielectric materials usually consist of a certain number of methyl groups and pores incorporated into a SiO₂ backbone structure to reduce the dielectric constant. They are …
-
Chemically Optimized Cu Etch Bath Systems for High-Density Interconnects and the FTIR Operando Exploration of the Nitrogen Reduction Reaction on a Vanadium Oxynitride Electrocatalyst
… the Cu etch bath and was able to predict a 35% lower etch rate that was not predicted by the three current monitoring methods (ORP, specific gravity, and conductivity). Application of this UV-Vis ATR probe confirmed that two industrial etch baths, in identical working conditions, confirmed a …
-
Supercritical Carbon Dioxide Processing of Silicon Wafer Surfaces
… to satisfy the demand for better performance. Low-k and porous low-k dielectrics are introduced to further reduce the RC delay of interconnects and improve signal transmission. The conventional wet and dry processing approaches, however, face problems with highly porous structures and changes …