Global ETD Search

Search theses and dissertations gathered from participating repositories worldwide. Every result links back to the library that holds it. No account is needed.

Results

Showing 1 to 20 of 193 for “"Melt spinning"”.

  1. The melt spinning of nylon-66

    … be 17,500.</p><p>The shear viscosity of nylon-66 melt was determined using an Instron Rheometer. The shear visocosity decreases with shear rate in the range of 200-1200 sec<sup>-1</sup>. The effect of moisture on the shear viscosity was determined by studying samples with moisture contents of 0.43 …

    ut-knoxville Repository record for The melt spinning of nylon-66 (opens in a new tab)

  2. Dynamics of steady and unsteady melt spinning

    … work involves an overall study of isothermal melt spinning, including both steady state and unsteady state spinning ("draw resonance"). A systematic study of two commercial polypropylenes was carried out as a function of the variables which one normally associates with draw resonance and in …

    utk-theses Repository record for Dynamics of steady and unsteady melt spinning (opens in a new tab)

  3. Melt Spinning of the Fine PEEK Filaments

    The production of fine filaments using the melt spinning process needs considerable effort. A thermoplastic melt is stretched from the spinneret under a constant take-up speed. The high performance thermoplastic PEEK is solidified in the melt spinning process in a small distance and short time. …

    qucosa-diss

  4. Experimental and analytical studies of melt spinning and spunbonding

    … and analytical studies were carried out on the melt spinning and spunbonding processes. Experimental studies consisted mainly of developing and using an improved technique to measure the temperature of the running fiber during single filament melt spinning. This technique is based on the …

    utk-theses Repository record for Experimental and analytical studies of melt spinning and spunbonding (opens in a new tab)

  5. Melt Spinning of Carbon Fibers from Asphaltene-Additive Blend

    … was blended with ASP at 5, 10, and 15 wt.% to melt-spun CFs. Adding PS enhanced the fiber spinnability and influenced the CFs mechanical properties. Nuclear Magnetic Resonance (NMR) and Fourier Transform Infrared Spectroscopy (FTIR) analyses revealed that increasing the PS content led to …

    calgary Repository record for Melt Spinning of Carbon Fibers from Asphaltene-Additive Blend (opens in a new tab)

  6. Radial Temperature Differences During the Melt Spinning of Fibers

    The production of glass and synthetic fibers by melt spinning is an important industrial process. Mathematical models of the process are needed to study the effects of rapid cooling and draw-down in the quench zone. In this investigation, a numerical model was developed to predict the temperature …

    clemson Repository record for Radial Temperature Differences During the Melt Spinning of Fibers (opens in a new tab)

  7. Melt spinning of continuous filaments by cold air attenuation

    … followed by mechanical drawing. A modified melt spinning apparatus with high-speed air nozzle was designed and fabricated to produce continuous polypropylene filaments by cold air drawing only. With this setup, the fiber is quenched and simultaneously attenuated by a symmetric cold air jet. …

    gatech Repository record for Melt spinning of continuous filaments by cold air attenuation (opens in a new tab)

  8. PLANAR-FLOW MELT SPINNING: PROCESS STABILITY AND MICROSTRUCTURAL CONTROL

    Various melt spinning embodiments have been developed over the past 30 years and have been widely used, particularly at bench-scale for the production of metallic glasses. Much of the processing science has been developed 'as-needed' by the metallurgical community. Commercial scale-up has been …

    cornell Repository record for PLANAR-FLOW MELT SPINNING: PROCESS STABILITY AND MICROSTRUCTURAL CONTROL (opens in a new tab)

  9. Development of aliphatic polyketone fibers by melt spinning and drawing

    … improve the chain flexibility and to reduce the melting point.</p> <p>Melt spinning followed by drawing of polyketones yields filaments that have high tensile strength that could be used for industrial applications such as tire cords. Polyketones as resins have extremely good chemical, …

    ut-knoxville Repository record for Development of aliphatic polyketone fibers by melt spinning and drawing (opens in a new tab)

  10. Characterization of hollow fiber properties during the melt spinning process.

    Substitution of hollow fibers for solid fibers would not only preserve the web properties (opacity and compression), but would actually improve the strength of each fiber. Hence, hollow fibers could be substituted for solid fibers in nonwoven webs. The final web would be lighter and cheaper that …

    oklahoma-thes Repository record for Characterization of hollow fiber properties during the melt spinning process. (opens in a new tab)

  11. A study of melt spinning, drawing and twisting of PET monofilament

    … as evidenced by a decay in spinnability, melt viscosity and molecular weight. The extruder was used to prepare large quantities of homogeneous samples for drawing and twisting studies.</p><p>All spun samples were amorphous. Changes in variables which produced greater spinline stress such …

    ut-knoxville Repository record for A study of melt spinning, drawing and twisting of PET monofilament (opens in a new tab)

Page 1 of 10