Global ETD Search
Search theses and dissertations gathered from participating repositories worldwide. Every result links back to the library that holds it. No account is needed.
Results
Showing 1 to 20 of 43 for “"Metallographic examination"”.
-
Thermo-mechanical fatigue of polycrystalline, directionally solidified and single crystal nickel base superalloys repaired by laser beam welding
… gas tungsten arc and baseline alloy conditions. Metallographic examination of laser beam welds and the associated heat affected zone were conducted by scanning electron microscopy and energy dispersive spectroscopy. The impact of laser beam welding on thermo-mechanical fatigue properties of …
-
Hydrogen Embrittlement of A High Strength Low Alloy Pipeline Steel
… did not affect the rate of crack propagation. Metallographic examination indicated that the orientations of inclusions played an important role in determining the path of crack propagation and delamination.</p>
-
The Aging Kinetics and Properties of Isothermally-Transformed Martensite in 18-Nickel 300 Grade Maraging Steel
… of annealed martensite in the overaged steel. Metallographic examination is conducted with both optical and electron microscopy as a supplementary study. The microstructure of severely banded specimens and other selected samples is discussed.
-
Superplasticity in an aluminum-zinc alloy
… This investigation consists of correlated metallographic examination, X-ray diffraction analysis, and tensile testing of Al-Zn binary alloys of 17 per cent, 20 percent, and 23 per cent Aluminum at specific stages of treatment. Special attention is focused on the heat evolution which follows …
-
The relationship of interfacial energy to graphite shape in the Fe-C system.
… examined. The graphite form was established by metallographic examination. An average ƔLV of 1152 dynes/cm was determined for the Fe-C alloys (4.6% C) at approximately 1300°C, the average contact angle being 128°. No significant change occurred with additions of Ni ( 0.85%) and Mn ( 1.65%). …
-
Correlation of surface finish and cover gas with weld defects in autogenous AL 5083 laser beam welds
… cover gas and surface finish. The subsequent metallographic examination revealed no correlation between surface finish and porosity, but that the cover gas selection strongly influenced the type and quantity of pores formed. In the second part, laser welds were made varying only the cover gas …
-
Scale formation and adhesion to mild steels during reheating for hot working.
… oxidation behaviour was studied by metallographic examination of the scale and scale/metal interface and by thermo-gravimetric techniques.The amount of oxidation was found to increase rapidly with temperature and only approximately parabolically with time. Deviations' from classic …
-
The Isostatic Compaction and Hydrostatic Extrusion of Some Metal Powders
… <p>Results of mechanical testing, metallographic examination and x-ray diffraction analyses of some atomized iron powder compacts are presented, together with a metallographic examination of compacted spherical superalloy powders. From these it is concluded that extensive plastic …
-
High temperature deformation and failure in aluminum-alumina particulate metal matrix composites
… characteristics were ascertained through metallographic examination of the fractured samples - both perpendicular and parallel to the fracture surface, and through numerical simulations of the collar compression test on the as-cast MMC . The reinforcing particles were found to enhance the …
-
A study of the retention of metastable-phases in quenched uranium-niobium-zirconium ternary alloys
… related to the niobium and zirconium contents. Metallographic examination of the samples having a monoclinic structure indicated that these samples had a Widmanstatten structure. The DPH hardness of all alloys regardless of crystal structure was found to be related to the niobium and zirconium …
-
The cutting performance of sialon ceramic tools
… involves a correlation of wear measurement and metallographic examination of the wear area with the measurable cutting data. Four main tool failure modes are recognised: (a) flank and crater wear (b) grooving wear (c) deformation wear and (d) brittle failure Results indicate catastrophic edge …
-
Τα κράματα του χαλκού της Εποχής του Χαλκού στο Αιγαίο και την Κύπρο: πρώτες ύλες και τεχνολογία
… composition and provenance of the metal, while metallographic examination was employed to reconstruct the manufacturing technology of the artefacts. The results contribute to a more comprehensive understanding of technological choices, metal circulation, and the development of copper metallurgy …
-
The Metallography of dental amalgams
… during preparation of amalgam specimens for metallographic examination has had scant reference in the dental literature, and therefore it is the primary concern of this thesis to elucidate some of the factors which produce porosity as an artefact on polished surfaces of amalgam specimens. The …
-
The Effect of Forging Reduction on the Properties of a Die Steel
… which, although apparently present on metallographic examination, was not confirmed by chemical and micro-probe analyses. Even so the micro hardness varied in a random manner. Increasing forging reductions did not affect mechanical properties measured in the longitudinal direction. …
-
A study of the weld heat affected zone of carbon manganese microalloyed steel
… been investigated by Charpy Impact tests and Metallographic examination. The real HAZs were obtained from bead-on-plate deposits made by Submerged Arc Welding at 3.6 and 6.3KJ/mm. These experiments provided toughness, microstructural and welding thermal cycle data. Welding Simulation, combined …
-
Structure-property relations in epoxy metal-ion polymers
… x-ray diffraction, infrared spectroscopy, and metallographic examination. Insolubility of the metal-ion ligands in EPON 828, resulting from their ionic nature, necessitated the development of a solution polymerization based on acetone. The effect of molecular structure on the internal friction …
-
The growth and deformation of cobalt crystals
… The thin twins have a {11 2̄̅̅1}habit plane. Metallographic examination of crystals pulled to large extensions and electro-polished to remove slip lines showed small needle-like markings, probably fine twins. In addition to the deformation work, certain observations have been made concerning …
-
Heat transfer analysis of the plasma spray deposition process
… of pores found in the coating after subsequent metallographic examination. Different size and distribution of pores found at different locations of the zirconia based coating appear consistent with a qualitative understanding of the evolution of temperature in the coatings examined. Pores …
-
A novel approach to integrating design into manufacturing and materials education through the fabrication of a scale model cannon
… The cannons were then tested and destroyed for metallographic examination. A quasi-experimental two by two factorial design was used to evaluate the effects of the innovative laboratory treatment compared with the effects of standard laboratory treatment. Assessment was performed using two …
-
Fatigue and corrosion fatigue crack growth resistance of RQT501 steel.
… applied cathodic polarisation (-9 . SO mV/SCE). Metallographic examination has been carried out to evaluate grain size and inclusion distribution, size and morphology. To enable a comparison between short and long fatigue crack growth, smooth shallow hour-glass specimens have been used to study …
Page 1 of 3