Global ETD Search

Search theses and dissertations gathered from participating repositories worldwide. Every result links back to the library that holds it. No account is needed.

Results 1 to 20 of 43 for “"Metallurgical bonding"”

  1. Evaluation of Repair Configurations on the Tensile Strength and Fracture Behavior of Directed Energy Deposition Repaired H13 Tool Steel

    … by restoring damaged regions while maintaining metallurgical bonding with the substrate. However, the mechanical reliability of repaired components remains a challenge due to the influence of repair configuration on microstructural evolution, defect formation, and fracture behavior. This study …

    ohiolink Repository record for Evaluation of Repair Configurations on the Tensile Strength and Fracture Behavior of Directed Energy Deposition Repaired H13 Tool Steel (opens in a new tab)

  2. Effect of cast iron surface treatment on interfacial adhesion of Al/Fe compound cast structure

    … around a solid ferrous insert to form a metallurgical bonding at the Al/Fe interface. This Metallurgical bonding provides the integrity of the component, and therefore requires to be strong enough to withstand all stresses during the casting process as well as the consumption stage. The …

    chalmers Repository record for Effect of cast iron surface treatment on interfacial adhesion of Al/Fe compound cast structure (opens in a new tab)

  3. Bond Improvement of Al/Cu Joints Created by Very High Power Ultrasonic Additive Manufacturing

    … smart materials. UAM has had limited success bonding dissimilar materials and thus Very High Power Ultrasonic Additive Manufacturing (VHP UAM), which increases the amplitude (from 26μm to 52μm) and normal force (from 2.5kN to 33kN), has been introduced to address this deficiency. </p><p>Al3003 …

    ohiolink Repository record for Bond Improvement of Al/Cu Joints Created by Very High Power Ultrasonic Additive Manufacturing (opens in a new tab)

  4. Evaluation of Cold Spray Process for Solid-State Welding

    … ubiquitous microvoids resulting from inadequate metallurgical bonding in CSWed area. These microvoids act as initiation sites for microcracks. To guide future optimization efforts, a failure mechanism in the CSWed parts is established. This research underscores the importance of addressing …

    calgary Repository record for Evaluation of Cold Spray Process for Solid-State Welding (opens in a new tab)

  5. Modification of plasma sprayed wear and corrosion resistant coatings by high-density infrared heating

    … porosity, inhomogenous phases, and limited metallurgical bonding to the substrate can lead to a decrease in wear and corrosion resistance. As will be shown in this presentation, modification of the plasma sprayed coating structure by a high-density infrared (plasma arc) lamp can eliminate or …

    iastate Repository record for Modification of plasma sprayed wear and corrosion resistant coatings by high-density infrared heating (opens in a new tab)

  6. Development of Ti-6Al-4V Coating onto Ti-6Al-4V Substrate Using Low Pressure Cold Spray and Pulse Gas Dynamic Spray

    … high hardness, adhesion strength over 40 MPa, metallurgical bonding, similar to bulk material wear rate, no oxide and nitride phases inside coating were measured.

    ottawa-retro Repository record for Development of Ti-6Al-4V Coating onto Ti-6Al-4V Substrate Using Low Pressure Cold Spray and Pulse Gas Dynamic Spray (opens in a new tab)

  7. Investigation of Magnetic Pulse Welding on Lap Joint of Similar and Dissimilar Materials

    … state impact welding technology that may provide metallurgical bonding without melting and solidification, and there is no significant heat affected zone (HAZ). It shares the same physical principle with explosive welding (EXW) and is good for workpiece with length scale in the order of millimeter …

    ohiolink Repository record for Investigation of Magnetic Pulse Welding on Lap Joint of Similar and Dissimilar Materials (opens in a new tab)

  8. MECHANICAL BEHAVIOR OF COLD SPRAYED CU-NI COATING

    … the coating, which showed signs of the stronger metallurgical bonding with the substrate. Annealed cold spray coating itself can bear significant load and strengthen the substrate. Thus, cold spray coating with appropriate post-processing treatment can potentially reinforce and even repair the …

    nps Repository record for MECHANICAL BEHAVIOR OF COLD SPRAYED CU-NI COATING (opens in a new tab)

  9. Pinless Friction Stir Spot Welding of Ti-6Al-4V Alloy for Aerospace Application

    … been a major challenge. Also, achieving strong metallurgical bonding has been challenging due to the relatively low thermal conductivity and refractory nature of the titanium alloys.</p> <p>In Ti-6Al-4V alloy, the basic understanding of the relationships among the welding variables, processing …

    utk-theses Repository record for Pinless Friction Stir Spot Welding of Ti-6Al-4V Alloy for Aerospace Application (opens in a new tab)

  10. EFFECT OF DUAL NANOPARTICLES REINFORCEMENT AND HEAT TREATMENT ON THE MECHANICAL AND TRIBOLOGICAL PROPERTIES OF COLD SPRAYED ALUMINUM COATINGS

    … oxidation, no phase transformation, and good metallurgical bonding when applied to a substrate. However, drawbacks such as porosity and low ductility limits its practical application. Heat treatments to CS coatings were successful in overcoming the drawbacks but sacrificed hardness for …

    nps Repository record for EFFECT OF DUAL NANOPARTICLES REINFORCEMENT AND HEAT TREATMENT ON THE MECHANICAL AND TRIBOLOGICAL PROPERTIES OF COLD SPRAYED ALUMINUM COATINGS (opens in a new tab)

  11. Sintered nanoporous copper die-attach interconnections: Syntheis and characterization

    … of assembly parameters to enable good metallurgical bonding between nanoporous Cu and Cu metallizations. The initial assembly trials gave promising results and Cu-Cu joints with shear strengths>40MPa were achieved.

    gatech Repository record for Sintered nanoporous copper die-attach interconnections: Syntheis and characterization (opens in a new tab)

  12. Microestrutura e propriedades de desgaste e corrosão de revestimentos à base de FeCrMoNbB e de CrCoNi produzidos por plasma com arco transferido

    … production of thick, dense coatings with good metallurgical bonding between the substrate and the coating. The two alloys were gas-atomized and subsequently characterized by scanning electron microscopy (SEM), optical microscopy (OM), X-ray diffraction (XRD), and differential scanning …

    brazil-ufscar Repository record for Microestrutura e propriedades de desgaste e corrosão de revestimentos à base de FeCrMoNbB e de CrCoNi produzidos por plasma com arco transferido (opens in a new tab)

  13. Lightweight alloy design for laser-based additive manufacturing

    … which traditionally suffers from weak metallurgical bonding. By developing thermodynamic models to guide the selection of intermediate elements, robust joints were achieved, thus enabling reliable multi-material structures. The obtained joint strength is the highest compared to all …

    soton Repository record for Lightweight alloy design for laser-based additive manufacturing (opens in a new tab)

  14. Quasi-Static, Cyclic, and Fracture Characteristics of Plasma Transferred Wire Arc (PTWA) Thermal Sprayed AlSi Cylinder Bores

    … oxides, re-solidified particles, and interfacial metallurgical bonding) using laser scanning confocal microscope, scanning and transmission electron microscope (SEM and TEM). Residual stress through the thickness of the coating was measured using x-ray diffraction (XRD) and hole-drilling method. …

    waterloo Repository record for Quasi-Static, Cyclic, and Fracture Characteristics of Plasma Transferred Wire Arc (PTWA) Thermal Sprayed AlSi Cylinder Bores (opens in a new tab)

  15. Process-structure-property-performance relationships and scalable repair strategies in additive friction stir deposition of high strength aluminum alloys.

    … the repair interfacial integrity and overall bonding quality to determine optimal tool paths that promote enhanced metallurgical bonding at the groove repair interface. Chapter three quantified how heat input conditions and temperature profiles influence interfacial bonding strength in deep …

    baylor Repository record for Process-structure-property-performance relationships and scalable repair strategies in additive friction stir deposition of high strength aluminum alloys. (opens in a new tab) Embargoed until 2031-08-15

  16. Laser Directed Energy Deposition Repair of Laser Powder Bed Fusion Maraging Steel Components

    … This thesis investigates strategies to optimize metallurgical bonding at the repair interface of LPBF-produced HPDC inserts. Simulated repair coupons with varying sidewall inclination angles were evaluated using scanning electron microscopy with energy-dispersive X-ray spectroscopy (SEM-EDS) to …

    waterloo Repository record for Laser Directed Energy Deposition Repair of Laser Powder Bed Fusion Maraging Steel Components (opens in a new tab)

  17. Friction Stir Welding And Processing On Titanium Alloys

    … pressure results in creation of a joint by metallurgical bonding. Because the temperature of the material during the welding process is below that of the melting point, FSW has numerous advantages over conventional fusion welding. Friction consolidation (FC) is also a solid-state process …

    south-carolina Repository record for Friction Stir Welding And Processing On Titanium Alloys (opens in a new tab)

  18. Exploration of the power-powder-molten pool (PPM) interaction mechanism in laser deposition additive manufacturing (LDAM) process

    Due to advantages of metallurgical bonding, minimal stress and distortion and comparable mechanical properties with traditional processing method, Laser Deposition Additive Manufacturing (LDAM) has become one of the core technologies in laser additive remanufacturing, metallic coating, and special …

    ttu Repository record for Exploration of the power-powder-molten pool (PPM) interaction mechanism in laser deposition additive manufacturing (LDAM) process (opens in a new tab)

  19. Friction Stir Welding of Dissimilar Metals

    … aluminum-copper, aluminum-titanium, etc.) or no metallurgical bonding for immiscible combinations (such as magnesium-copper, steel-copper, etc.). For metallurgical miscible combinations, brittle intermetallic compounds formed at the welded interface created the crack initiation and propagation …

    unt Repository record for Friction Stir Welding of Dissimilar Metals (opens in a new tab)

  20. Spot impact welding of aluminum sheet

    … Forge welding, resistance welding, and roll bonding have either adapted or given way to friction stir welding, ultrasonic welding, and explosive welding to name a few. This process had been the hidden but to a few skilled craftsmen. Today, however, those sufficiently skilled to operate …

    ohiolink Repository record for Spot impact welding of aluminum sheet (opens in a new tab)

Page 1 of 3