Global ETD Search
Search theses and dissertations gathered from participating repositories worldwide. Every result links back to the library that holds it. No account is needed.
Results 1 to 6 of 6 for “"Minicomposites"”
-
USE OF SINGLE TOW CERAMIC MATRIX MINICOMPOSITES TO DETERMINE FUNDAMENTAL ROOM AND ELEVATED TEMPERATURE PROPERTIES
… of damage in various ceramic fiber reinforced minicomposites with different fiber volume fractions and interphases was investigated employing several non-destructive evaluation techniques. A new technique is used to determine matrix crack content based on a damage parameter derived from speed …
-
Multimodal approach for the in-situ investigation of high temperature tensile behavior and damage progression in SiCf/SiC ceramic matrix minicomposites
… properties and AE-estimated damage events of the minicomposites. Tests were conducted from 1200°C up to 1482°C using a conventional slit furnace. The decline in mechanical strength properties as test temperature was increased was related to the weakening of SiC fibers and the boron nitride …
-
Optimisation de la liaison interfaciale dans les composites à matrice céramique renforcés par des fibres Hi-Nicalon S
… avec l’interphase BN. Des composites modèles, minicomposites élaborés par voie CVI (Chemical Vapor Infiltration) sont utilisés comme base de travail. La quantification de la force de la liaison interfaciale s’effectue en évaluant l’énergie de liaisons interfaciales Gci issues d’essais de …
-
Rupture différée en fatigue statique aux très hautes températures (800° - 1300°) des fils Hi-Nicalon, des composites Hi-Nicalon/Type PyC/SiC et des composites Hi-Nicalon/Type PyC/B4C
… Hi-Nicalon à l’échelle multifilamentaire, des minicomposites de type Hi-Nicalon/PyC/SiC et Hi-Nicalon/type PyC/B4C a été étudiée à l’aide de moyens d’essais spécifiques et innovants. Des essais de fatigue statique sous air aux très hautes températures (900°C-1300°C) avec mesure des déformations …
-
Low modulus, oxidation-resistant interface coatings for SiC/SiC composites
… probably at the matrix-coating interface. Minicomposites that contained tows coated using MOD were too weak to be tested for tensile strength. This necessitated the deposition of a thin (~ 30 nm) layer of carbon both on the tows before depositing CMZP coating to protect the fibers as well …
-
Dépôt CVD sur fil SiC chauffé par micro-ondes à partir de précurseurs non halogénés pour application aéronautique
… visée, des tests sur composites modèles (minicomposites) ont été menés. Ils ont permis d’évaluer le comportement des interphases en oxydation/corrosion et sur le plan mécanique, à partir de traitement en température sous air humide et d’essais de traction simple et d’indentation (push-out).