Results 1 to 5 of 5 for “"Nanolamellar"”

  1. Physical Properties of Copper Niobium Nanolamellar Composites Fabricated by Accumulative Roll Bonding

    Nanolamellar composites with high interface density have increased strength due to interfaces serving as barriers to dislocation movement and high radiation damage resistance. However, these interfaces also serve as barriers to electron motion, reducing the electrical resistivity and thermal …

    unm Repository record for Physical Properties of Copper Niobium Nanolamellar Composites Fabricated by Accumulative Roll Bonding (opens in a new tab)

  2. Bottom-Up Multiferroic Nanostructures

    … by synthesizing a spontaneously phase separated nanolamellar BaTiO3-CoFe2O4 bi-crystal. The superlattice is magnetoelectric with a frequency dependent coupling. The BaTiO3 component is a ferroelectric relaxor with a Vogel-Fulcher temperature of 311 K. Since the material can be produced by …

    maryland Repository record for Bottom-Up Multiferroic Nanostructures (opens in a new tab)

  3. Microstructure Evolution and Mechanical Behavior of Laser Additively Manufactured Alloys with Heterogeneous Microstructures

    … energy deposition-fabricated directional nanolamellar AlCoCrFeNi2.1, comprised of face-centered cubic (fcc) and ordered body-centered cubic (B2) phases. The eutectic high entropy alloys that are loaded along three orientations present obvious mechanical anisotropy: (i) Samples HEA0, loaded …

    toronto-retro Repository record for Microstructure Evolution and Mechanical Behavior of Laser Additively Manufactured Alloys with Heterogeneous Microstructures (opens in a new tab)

  4. Évolution des microstructures et mécanismes de densification d'un alliage TiAl lors du frittage par Spark Plasma Sintering

    Ce travail porte sur l'évolution microstructurale d'un alliage TiAl lors du frittage par un procédé appelé Spark Plasma Sintering (SPS). Les poudres initiales, élaborées par atomisation, sont constituées principalement d'une phase métastable. Les transformations qui accompagnent le retour à …

    star-france Repository record for Évolution des microstructures et mécanismes de densification d'un alliage TiAl lors du frittage par Spark Plasma Sintering (opens in a new tab)

  5. Conversion de monocristaux et de poudres de MoAlB et V2AlC par la méthode du sel fondu

    Les carbures (MAX) et borures (MAB) de métaux de transition sont des solides nanolamellaires qui combinent la dureté céramique avec la conductivité métallique. Depuis la découverte des MXènes par Naguib et al. en 2011, grâce à la gravure sélective des phases MAX parentes, plus de 30 compositions de …

    star-france Repository record for Conversion de monocristaux et de poudres de MoAlB et V2AlC par la méthode du sel fondu (opens in a new tab)