Global ETD Search

Search theses and dissertations gathered from participating repositories worldwide. Every result links back to the library that holds it. No account is needed.

Results

Showing 1 to 20 of 54 for “"Ni-based superalloy"”.

  1. Development of Multicomponent EAM Potential for Ni-Based Superalloy

    We initiated the development of multi-component EAM potentials for Aluminides and Carbides, key phases in Ni-based Superalloys. The goal is to utilize the MD simulation to understand the deformation dynamics that contribute to the formation of voids and creep initiation. For this purpose, we …

    mo-state Repository record for Development of Multicomponent EAM Potential for Ni-Based Superalloy (opens in a new tab)

  2. In situ diagnostics of damage accumulation in Ni-based superalloy

    <p>There has been a significant interest in capturing how the damage is initiated and accumulated in polycrystalline Ni-based superalloys while applying thermal and mechanical impact – tensile and creep loading at 800◦C. This is because the turbine component in jet propulsion or power generation …

    oxford Repository record for In situ diagnostics of damage accumulation in Ni-based superalloy (opens in a new tab)

  3. Processing-Structure-Property Relationships in Ni-based Superalloy René 41

    The cast and wrought Nickel based superalloy René 41 combines excellent strength, toughness, and corrosion properties. Its mechanical properties outperform all similar competitor aerospace alloys such as Waspaloy and Haynes 282. However, processing of René 41 remains challenging due to cracking and …

    unsw Repository record for Processing-Structure-Property Relationships in Ni-based Superalloy René 41 (opens in a new tab)

  4. Tertiary Creep Damage Modeling Of A Transversely Isotropic Ni-based Superalloy

    Anisotropic tertiary creep damage formulations have become an increasingly important prediction technique for high temperature components due to drives in the gas turbine industry for increased combustion chamber exit pressures, temperature, and the use of anisotropic materials such as metal matrix …

    ucf Repository record for Tertiary Creep Damage Modeling Of A Transversely Isotropic Ni-based Superalloy (opens in a new tab)

  5. The Role of Slip System Activation on Ni-Based Superalloy High Temperature Fatigue

    Nickel-based superalloys are used extensively in the aviation industry, particularly in aircraft engine components. These materials are desirable due to their high strength, resistance to creep, corrosive environment, and high temperature. It has been well documented that material fatigue is …

    embry-riddle Repository record for The Role of Slip System Activation on Ni-Based Superalloy High Temperature Fatigue (opens in a new tab)

  6. Radiation Damage Effect on Mechanical Properties and Microstructure of X-750 Ni-based Superalloy

    Inconel X-750 is an age-hardened Ni-based superalloy with high mechanical strength and creep resistance. The X-750 alloy is extensively used in the cores of reactors, such as spacers in CANada Deuterium Uranium (CANDU) fuel channels. The recent mechanical tests on the ex-service Inconel X-750 …

    queens Repository record for Radiation Damage Effect on Mechanical Properties and Microstructure of X-750 Ni-based Superalloy (opens in a new tab)

  7. Linear friction welding of AD730™ Ni-based superalloy to additively manufactured Inconel 718

    … emerging solid-state welding technology for joining of blades to disks (blisks) or repairing turbine disks in gas turbines and air engines. In recent years, LFW has also been applied to the assembly of components made of Nickel (Ni)-based superalloys, as well as in many other engineering …

    ets-quebec Download PDF for Linear friction welding of AD730™ Ni-based superalloy to additively manufactured Inconel 718 (opens in a new tab)

  8. Tracking meta-dynamic recrystallization in a Ni-based superalloy using timeresolved synchrotron X-ray diffraction

    … high operating temperatures while maintaining metallurgical stability. The nickel-based superalloy Haynes 282 has emerged as a promising material for use in aero-engine applications. Recrystallization plays a critical role in determining the final microstructure and, consequently, the …

    chalmers Repository record for Tracking meta-dynamic recrystallization in a Ni-based superalloy using timeresolved synchrotron X-ray diffraction (opens in a new tab)

  9. Evolution of microstructure and mechanical properties during linear friction welding of AD730 TM Ni-based superalloy

    … is an emerging manufacturing technology for joining of blades to disks or repairing turbine disks in gas turbines and jet engines. LFW has already been applied to Ti alloys for compressor (i.e. low temperature) operation applications but not to high temperature components. Thus, many challenges …

    ets-quebec Download PDF for Evolution of microstructure and mechanical properties during linear friction welding of AD730 TM Ni-based superalloy (opens in a new tab)

  10. UNDERSTANDING PROCESSING-MICROSTRUCTURE-PROPERTY RELATIONSHIPS AND THE ASSOCIATED DEFORMATION MECHANISMS IN ATI 718PLUS NI-BASED SUPERALLOY

    A superalloy is a multi-metal alloy system that exhibits a good combination of high-temperature properties, such as resistance to thermal creep deformation, oxidation, and corrosion and has a service temperature often above 0.7 times the absolute melting temperature. Alloy ATI 718Plus is a …

    msu Repository record for UNDERSTANDING PROCESSING-MICROSTRUCTURE-PROPERTY RELATIONSHIPS AND THE ASSOCIATED DEFORMATION MECHANISMS IN ATI 718PLUS NI-BASED SUPERALLOY (opens in a new tab)

  11. Fabrication of Hard-to-Process Ni-Based Superalloy Thin-Wall Parts Made by Laser Powder Bed Fusion

    Thin-wall part fabrication is significant for aerospace, automotive, and thermal applications, which require complex metallic features hard to manufacture using conventional manufacturing processes. Laser powder bed fusion (LPBF) additive manufacturing (AM) technique enables the construction of …

    waterloo Repository record for Fabrication of Hard-to-Process Ni-Based Superalloy Thin-Wall Parts Made by Laser Powder Bed Fusion (opens in a new tab)

  12. Influences of microstructure and oxidation processes on fatigue failure mechanisms in advanced turbine disc Ni-based superalloy

    Most in-service Ni-based turbine disc alloys have a bi-modal or tri-modal <i>γ</i>ʹ size distribution, where primary <i>γ</i>ʹ size (or presence) is linked to the duration and temperature of the solution heat treatment (e.g. super or sub-solvus) whilst secondary <i>γ</i>ʹ and tertiary <i>γ</i>ʹ …

    soton Download PDF for Influences of microstructure and oxidation processes on fatigue failure mechanisms in advanced turbine disc Ni-based superalloy (opens in a new tab)

  13. Porosity closure during hot isostatic pressing of additively manufactured Ni-based superalloy IN718 produced by LPBF and EBM

    Inconel 718 is a precipitation hardened Ni-based superalloy for aerospace applications where corrosion, creep and fatigue resistance are required. Additive manufacturing (AM) enables production of new designs of weight-optimised components with features not possible with traditional manufacturing …

    chalmers Repository record for Porosity closure during hot isostatic pressing of additively manufactured Ni-based superalloy IN718 produced by LPBF and EBM (opens in a new tab)

  14. Tool Wear and Workpiece Surface Integrity during Ni-Based Superalloy Machining with Multi-layer CVD Alumina Coated Carbides

    Ni-based superalloys are used in the most hostile engineering environments, including the hottest stages of aeroengines. The exceptional high-temperature performance of these alloys presents significant challenges during machining; substantial heat and high stresses are generated that impact the …

    whiterose Download PDF for Tool Wear and Workpiece Surface Integrity during Ni-Based Superalloy Machining with Multi-layer CVD Alumina Coated Carbides (opens in a new tab)

  15. Effects of C and B microalloying additions on the microstructure and processability of René 41 Ni-based superalloy

    René 41 is a cast and wrought Ni-based superalloy with high yield strength and stress-rupture properties contrasted with poor processability. The aim of this thesis is to systematically investigate the influence of C and B microalloying additions on processability of René 41. The first approach is …

    unsw Repository record for Effects of C and B microalloying additions on the microstructure and processability of René 41 Ni-based superalloy (opens in a new tab)

  16. Study of fatigue crack initiation and propagation mechanisms in an advanced Ni-based superalloy: effects of microstructures and oxidation

    … (CG) and fine grained (FG) LSHR alloys by uninterrupted and interrupted three-point bending with a replication procedure at room temperature, 650 and 725 oC in air and vacuum under a sine waveform (20Hz) and/or 1-1-1-1 trapezoidal waveform to investigate fatigue crack initiation and early …

    soton Download PDF for Study of fatigue crack initiation and propagation mechanisms in an advanced Ni-based superalloy: effects of microstructures and oxidation (opens in a new tab)

  17. The oxidation damage of Ni-based superalloy, RR1000, with different surface modifications and the role of oxidation in fatigue crack initiation

    … The chromia external scale growth rate is significantly greater than pure chromia on chromium and the enhancement is attributed to the increased ionic transport caused by doping of the chromia layer with Ti. This effect is still seen regardless of surface condition prior to oxidation. Oxides, …

    birmingham Download PDF for The oxidation damage of Ni-based superalloy, RR1000, with different surface modifications and the role of oxidation in fatigue crack initiation (opens in a new tab)

  18. Modes and Progression of Tool Deterioration and Their Effects on Cutting Force During End Milling of 718Plus Ni-based Superalloy Using Cemented WC-CO Tools

    … force (F) during milling of difficult-to-cut Ni-based superalloys is important for the improvement of machinability of the alloys. It also serves to clarify whether and how an F-based method for monitoring tool deterioration is possible. This understanding is however far from sufficient, as is …

    auckland-tech Repository record for Modes and Progression of Tool Deterioration and Their Effects on Cutting Force During End Milling of 718Plus Ni-based Superalloy Using Cemented WC-CO Tools (opens in a new tab)

  19. Understanding the deformation mechanisms in Ni-based superalloys with using crystal plasticity finite element method

    “Ni-based superalloy is considered as a good candidate due to its excellent resistance to elevated temperature deformation for long term period application. Understanding the deformation and failure mechanisms of Ni-Based superalloys is very helpful for providing design guidelines for processing …

    must-thes Repository record for Understanding the deformation mechanisms in Ni-based superalloys with using crystal plasticity finite element method (opens in a new tab)

  20. Thermophysical property measurements at high temperatures for liquid metal alloys and gadolinium oxide-doped uranium dioxide samples

    New techniques for obtaining various thermophysical properties, i.e., densities and incremental enthalpies of selected materials at high temperatures have been developed with emphasis on the utilization of levitation technique and drop calorimetry. The density of liquid copper has been evaluated at …

    rice Repository record for Thermophysical property measurements at high temperatures for liquid metal alloys and gadolinium oxide-doped uranium dioxide samples (opens in a new tab)

Page 1 of 3