Global ETD Search

Search theses and dissertations gathered from participating repositories worldwide. Every result links back to the library that holds it. No account is needed.

Results

Showing 1 to 20 of 96 for “"Nickel based superalloy"”.

  1. Fiber laser welding of nickel-based superalloy Inconel 718

    Inconel 718 (IN 718) is widely used in applications, such as aircraft and power turbine components. Recently, fiber laser welding has become an attractive joining technique in industry for fabrication and repair of service-damaged components. However, a major limitation in the laser welding of IN …

    manitoba Repository record for Fiber laser welding of nickel-based superalloy Inconel 718 (opens in a new tab)

  2. Molecular Dynamics Study of Creep Deformation in Nickel-based Superalloy

    … employs molecular dynamics simulations of Ni-based superalloy to investigate the creep behavior under uniaxial compression test. Dislocation dynamics is analyzed for the nickel-based single crystal superalloy with the presence of void and with varying the distribution of gamma-prime phase The …

    mo-state Repository record for Molecular Dynamics Study of Creep Deformation in Nickel-based Superalloy (opens in a new tab)

  3. The microstructure and properties of powder HIPped nickel-based superalloy CM247LC

    The response of powder of the Nickel-based superalloy CM247LC to a range of Hot Isostatic Pressing (HIPping) conditions and post-HIP heat treatments has been investigated as a preliminary step in the assessment of net shape HIPping as a possible process-route for component production. A HIPping …

    birmingham Repository record for The microstructure and properties of powder HIPped nickel-based superalloy CM247LC (opens in a new tab)

  4. Thermo-mechanical fatigue crack growth modeling of a nickel-based superalloy

    … development of this model was a polycrystalline superalloy, Inconel 100 (IN-100). The first step in creating a reliable model was to define the first order effects that influence TMF crack growth in a typical engine spectrum. Load interaction effects were determined to be major contributors to …

    gatech Repository record for Thermo-mechanical fatigue crack growth modeling of a nickel-based superalloy (opens in a new tab)

  5. Corrosion Behavior of Additively Manufactured Alloy 625, A Nickel Based Superalloy

    … research concerning corrosion behavior of wire-based methods. Most of the existing studies have predominantly focused on powder-based methods, leaving wire-based techniques relatively underexplored. This disparity in research attention highlights the need for additional corrosion research …

    arizona-thes Repository record for Corrosion Behavior of Additively Manufactured Alloy 625, A Nickel Based Superalloy (opens in a new tab)

  6. CYCLIC OVERAGEING PRE-WELD HEAT TREATMENT FOR NICKEL-BASED SUPERALLOY (RENE 80)

    … made of gamma prime precipitation strengthened nickel-based superalloys which have many desirable mechanical properties. However, the perennial conflict between strength and ductility makes low ductility and hence poor weldability a consequence of such precipitation strengthened alloys. ln this …

    nus Repository record for CYCLIC OVERAGEING PRE-WELD HEAT TREATMENT FOR NICKEL-BASED SUPERALLOY (RENE 80) (opens in a new tab)

  7. High-resolution characterisation of strengthening effects in nickel-based superalloy Alloy 718

    … a polycrystalline, precipitation-strengthened nickel-based superalloy. High-temperature strength, creep resistance and corrosion resistance allow operational temperatures of 650 °C for service cycles of several 100,000 h under high mechanical workloads. Conventional processing of Alloy 718 …

    unsw Repository record for High-resolution characterisation of strengthening effects in nickel-based superalloy Alloy 718 (opens in a new tab)

  8. Characterization of gamma prime precipitates in a powder metallurgy nickel-based superalloy

    Nickel-based superalloys see wide use in applications requiring high strengths at high temperatures, notably in the blades of gas turbines. An important contributor to this superior high-temperature strength is the presence of Gamma Prime precipitates. This project characterizes the behaviour of a …

    manitoba Repository record for Characterization of gamma prime precipitates in a powder metallurgy nickel-based superalloy (opens in a new tab)

  9. CHARACTERIZATION OF 3D PRINT NICKEL BASED SUPERALLOY FOR OIL AND GAS DRILLING APPLICATIONS

    In this thesis, the research works are being divided into two parts. First part of the work will detail the variation and adjustment of selective laser melting parameters to achieve the lowest possible porosity. Two different characterization techniques consist of Archimedes method and X-ray …

    nus Repository record for CHARACTERIZATION OF 3D PRINT NICKEL BASED SUPERALLOY FOR OIL AND GAS DRILLING APPLICATIONS (opens in a new tab)

  10. Residual stress assessment for shot peened nickel based superalloy by eddy current technique

    … for conductivity characterization of shot peened nickel based alloys. A model-based, eddy current inversion method is presented and applied to the SHFEC data obtained from a series of shot peened nickel based alloys to determine the depth profiles of actual conductivity up to 400 mum below the …

    iastate Repository record for Residual stress assessment for shot peened nickel based superalloy by eddy current technique (opens in a new tab)

  11. Recrystallisation and ?? precipitation during industrial open die forging of the nickel based superalloy AD730

    Ni-based superalloys are used in very challenging operating conditions in jet turbine engines. In order to withstand these challenging operating conditions, and be used in safety critical parts such as turbine discs, the microstructure of such alloys must be well controlled. Much of this control is …

    strathclyde Repository record for Recrystallisation and ?? precipitation during industrial open die forging of the nickel based superalloy AD730 (opens in a new tab)

  12. High-Temperature Oxidation, Fluoride-Ion Cleaning, and Activated Diffusion Brazing of Nickel-Based Superalloy GTD111

    … has resulted in the continual modification of nickel-based superalloys to provide better high-temperature strength and corrosion resistance for components such as hot-section turbine blades. Thermal-Mechanical Fatigue (TMF) cracking, accelerated by the oxidation that forms as a result of the …

    waterloo Repository record for High-Temperature Oxidation, Fluoride-Ion Cleaning, and Activated Diffusion Brazing of Nickel-Based Superalloy GTD111 (opens in a new tab)

  13. Parametric Investigation and Optimization for Inconel 718 Nickel-Based Superalloy in Laser Powder Bed Fusion

    … to decrease with increasing laser scan speed. Based on the measurement of cellular structures and Rosenthal models, cooling rate in LPBF was estimated to be in the order of 10^5 - 10^7 K/s.

    ucf Repository record for Parametric Investigation and Optimization for Inconel 718 Nickel-Based Superalloy in Laser Powder Bed Fusion (opens in a new tab)

  14. An investigation of defects in the nickel-based superalloy IN738LC fabricated by laser powder bed fusion

    Nickel-based superalloy Inconel 738 LC (IN738LC) can be used for the components in aero-engine due to its excellent high-temperature mechanical properties and oxidation/corrosion resistance. However, this alloy is difficult to be processed due to a high level of defects by laser powder bed fusion …

    birmingham Repository record for An investigation of defects in the nickel-based superalloy IN738LC fabricated by laser powder bed fusion (opens in a new tab)

  15. Microstructural Development of Inconel 625 Nickel-Based Superalloy as Function of Laser Powder Bed Fusion Parameters

    Additive manufacturing (AM) allows fabrication of complex components with features that are impractical or impossible to achieve through conventional methods. Selective laser melting (SLM) powder bed fusion AM technology was selected for this study on Inconel 625, a widely utilized high-temperature …

    ucf Repository record for Microstructural Development of Inconel 625 Nickel-Based Superalloy as Function of Laser Powder Bed Fusion Parameters (opens in a new tab)

  16. Fatigue Crack Growth Behaviour of Cobalt-based and Nickel-based Superalloy Processed by Selective Laser Melting

    The production of cobalt-based and nickel-based superalloys via Selective Laser Melting (SLM) has been successfully applied in low-mass production, particularly in producing components/equipment for the spacecraft and medical industries. SLM technique allows complex and customised parts to be …

    auckland-tech Repository record for Fatigue Crack Growth Behaviour of Cobalt-based and Nickel-based Superalloy Processed by Selective Laser Melting (opens in a new tab)

  17. Parent Material Surface Deposits Origin in Finish Turning Operations of the Powder Processed Nickel Based Superalloy RR1000

    … denoted as pick-up, on finish turned advanced nickel based superalloy RR1000 has been investigated. Three types of pick-up were defined: streaks of chip residue producing relatively low surface roughness changes, minor pick-up deposits ranging in length from 10-100 μm, and major pick-up …

    whiterose Repository record for Parent Material Surface Deposits Origin in Finish Turning Operations of the Powder Processed Nickel Based Superalloy RR1000 (opens in a new tab)

  18. Heat treatment optimization and mechanical characterization of a Nickel-based superalloy obtained via hot isostatic pressing (HIPping)

    … the consolidated Astroloy. Another LRU of INSTM, based at Politecnico di Milano (I), was involved in the project for their unique expertise on Fstigue Crack Growth tests and analysis. The Aubert & Duval (Fr) company was the other major partner of the project and provided the HIP process, methods …

    poli-torino Repository record for Heat treatment optimization and mechanical characterization of a Nickel-based superalloy obtained via hot isostatic pressing (HIPping) (opens in a new tab)

Page 1 of 5