Global ETD Search

Search theses and dissertations gathered from participating repositories worldwide. Every result links back to the library that holds it. No account is needed.

Results

Showing 1 to 2 of 2 for “"ODS superalloy"”.

  1. Development of Ni-based Oxide Dispersion Strengthened (ODS) powder particles for Metal Additive Manufacturing (AM) Applications

    … or nickel-based Oxide Dispersion Strengthened (ODS) powders, with nanocrystalline microstructure, cannot be produced with the atomization process because of the high temperature of yttrium (III) oxide (Y2O3, 2425 °C) compared to iron (Fe, 1538 °C), nickel (Ni, 1668 °C), chromium (Cr, 1907 °C) …

    wvu Repository record for Development of Ni-based Oxide Dispersion Strengthened (ODS) powder particles for Metal Additive Manufacturing (AM) Applications (opens in a new tab)