Global ETD Search

Search theses and dissertations gathered from participating repositories worldwide. Every result links back to the library that holds it. No account is needed.

Results

Showing 1 to 20 of 22 for “"Outdoor weathering"”.

  1. Effect on water absorpion and outdoor weathering on emerging polymer interlayers

    … polymer interlayer materials, will behave after weathering action. It is known that weathering action has a significant impact on polymer interlayer materials, and previous studies have evaluated certain aspects of weathering such as temperature, humidity, and UV radiation. The purpose of this …

    missouri Repository record for Effect on water absorpion and outdoor weathering on emerging polymer interlayers (opens in a new tab)

  2. An Evaluation of Acrylic Resin, Ethyl Silicate, and Methyltrimethoxysilane Treatment at San Antonio Missions National Historic Park, San Antonio, Texas

    … stone conservation treatment after 17 years of outdoor weathering. It is rare for a conservator to return to a site and assess her/his treatment and even rarer to monitor a treatment periodically over time. The conservation project under review was performed in 1993-94 and was documented step by …

    penn Repository record for An Evaluation of Acrylic Resin, Ethyl Silicate, and Methyltrimethoxysilane Treatment at San Antonio Missions National Historic Park, San Antonio, Texas (opens in a new tab)

  3. Detection and potential impacts of nanomaterials released from building materials in the natural weathering environment

    … and cement. Since building materials are in the outdoor environment, incorporated (nano)-particles may be released into the environment and have unforeseen consequences. Outdoor weathering experiments were performed on two building materials, micronized copper azole (MCA) treated lumber and …

    colo-mines Repository record for Detection and potential impacts of nanomaterials released from building materials in the natural weathering environment (opens in a new tab)

  4. Effects of HALSs and Nano-ZnO Worked as UV Stabilizers of Polypropylene

    This work reports the outdoor weathering performance of ultraviolet (UV)-stabilized polypropylene (PP) products (using PP resins from Encore Wire). Different hindered amine light stabilizers (HALSs) and nano-ZnO were used to stabilize PP-film-based formulations that were exposed under UV light for …

    unt Repository record for Effects of HALSs and Nano-ZnO Worked as UV Stabilizers of Polypropylene (opens in a new tab)

  5. Mechanisms for the Formation and Degradation of Microplastic : Results from Accelerated Weathering Studies

    … polymer systems via accelerated-controlled weathering. The first paper investigates amorphous polystyrene (PS) as tensile bars and particles, exposed to accelerated weathering for 3200 hours (two years of outdoor weathering). Samples were taken at 13 time intervals and changes in molecular …

    bayreuth Repository record for Mechanisms for the Formation and Degradation of Microplastic : Results from Accelerated Weathering Studies (opens in a new tab)

  6. The role of trees in reducing the urban heat island effect on the New Jersey Institute of Technology campus, Newark, NJ

    … indicate that the material is well suited for an outdoor environment with mass losses of less than 0.08% after five months of outdoor weathering and less than 0.5% after 54 freeze/thaw cycles. Further research should include a complete life cycle analysis to quantify the environmental benefits and …

    njit Repository record for The role of trees in reducing the urban heat island effect on the New Jersey Institute of Technology campus, Newark, NJ (opens in a new tab)

  7. Laboratory evaluation of moisture performance of weather resistive barriers

    … also used to evaluate effect of penetrations, outdoor weathering, and contribution of detergent dissolved in the interstitial water. Subsequent to the material testing, an assembly testing provided a comparative evaluation of such effects as penetrations or additives in a stucco layer. Proposed …

    concordia

  8. Weather resistive barriers in stucco cladding systems

    … or deposited on WRB surfaces. Neither four-month outdoor weathering nor laboratory mechanical stretching showed a significant effect in WRB performance when measured with typical test methods. This is because in most cases vapour transmission is a dominant phase of the transport. On the other …

    concordia

  9. Digital technology used in the application of colour measurement and colour formulation of skin in maxillofacial prosthetics

    … in darkness, exposed to accelerated ageing and outdoor weathering. Test groups included non-pigmented, individually pigmented samples and Caucasian skin tone coloured specimens. Investigations further involved the use of UV-light absorbers and silicone surface sealants to improve the colour …

    kings Repository record for Digital technology used in the application of colour measurement and colour formulation of skin in maxillofacial prosthetics (opens in a new tab)

  10. Investigation of Pretreatment Primer Performance by Electrochemical Techniques and Environmental Weathering

    … cells, neutral salt spray, humidity and under outdoor weathering conditions in Bohus Malmön, Sweden (BM) were characterised using EIS. Impedance modulus, |Z|, indicates the overall performance of the system, and phase angles were indicative of the presence of corrosion product. The total …

    sheffield-hallam Repository record for Investigation of Pretreatment Primer Performance by Electrochemical Techniques and Environmental Weathering (opens in a new tab)

  11. Radicals Transforming Organic Matter: Implications for Non-Pyrogenic Black Carbon and Nitrogen Formation, Molecular Dynamics in Tropical Soils, and Lignin Valorization

    … long-term iron-exposed wood subjected to natural outdoor weathering reveal progressive aromatic condensation, nitrogen incorporation, and heterocyclic nitrogen formation in the absence of fire. These findings demonstrate that non-pyrogenic pathways can contribute to global reservoirs of condensed …

    odu Repository record for Radicals Transforming Organic Matter: Implications for Non-Pyrogenic Black Carbon and Nitrogen Formation, Molecular Dynamics in Tropical Soils, and Lignin Valorization (opens in a new tab)

  12. Durability of building envelope materials

    … done based on ASTM C1589, Standard Practice for Outdoor Weathering of Construction Seals and Sealants Procedure C, and important trends are presented after observation and data analysis of the gathered information. Important takeaways from water-repellent testing are listed considering the …

    texas Repository record for Durability of building envelope materials (opens in a new tab)

  13. A study of environmental exposure on structural adhesively bonded austenitic stainless steel.

    … Environmental exposure included natural outdoor weathering and a high humidity environment coupled with the application of an applied load. It was noted that to further appraise more durable pre-treatments used prior to bonding different testing configurations was required. Perforated …

    sheffield-hallam Repository record for A study of environmental exposure on structural adhesively bonded austenitic stainless steel. (opens in a new tab)

  14. Degradation studies on recycled Polyethylene terephthalate

    … on the properties under natural and artificial weathering. The real-time outdoor weathering exposures provide the most accurate results but, they are very slow and manufacturers cannot afford to wait in order to see if a new or improved product formulation is really an improvement. So, …

    london-metro Repository record for Degradation studies on recycled Polyethylene terephthalate (opens in a new tab)

  15. CHARACTERIZING DEGRADATION OF NANO-ENABLED MATERIALS AND ENGINEERED NANOMATERIAL RELEASE FOLLOWING NATURAL AND ARTIFICIAL WEATHERING

    … release following either accelerated or natural weathering is described herein. To that end, this body of work had two primary focuses: a) Determine how the initial nanoparticle content within a polymer nanocomposite impacted said nanocomposite’s photodegradation following accelerated weathering; …

    jhu Repository record for CHARACTERIZING DEGRADATION OF NANO-ENABLED MATERIALS AND ENGINEERED NANOMATERIAL RELEASE FOLLOWING NATURAL AND ARTIFICIAL WEATHERING (opens in a new tab)

  16. Natural Kenaf Fiber Reinforced Composites as Engineered Structural Materials

    … than synthetic fiber composites, a series of weathering and environmental tests were conducted on the kenaf fiber composites. The environmental conditions studied include real-time outdoor weathering, elevated temperatures, immersion in different pH solutions, and UV exposure. In all of these …

    wvu Repository record for Natural Kenaf Fiber Reinforced Composites as Engineered Structural Materials (opens in a new tab)

  17. DEVELOPMENT OF ALGAL RESISTANT SURFACE COATING FOR EXTERNAL WALL OF BUILDINGS IN THE TROPICS WITH PARTICULAR REFERENCE TO THE BUILDINGS AND ENVIRONMENTAL CONDITIONS IN SINGAPORE

    … paint was validated through two series of outdoor weathering tests to screen the durability of the paint film against mechanical breakdown and against algal growth. Environment of the two test sites complement each other for the two weathering test. In the field One of the most difficult …

    nus Repository record for DEVELOPMENT OF ALGAL RESISTANT SURFACE COATING FOR EXTERNAL WALL OF BUILDINGS IN THE TROPICS WITH PARTICULAR REFERENCE TO THE BUILDINGS AND ENVIRONMENTAL CONDITIONS IN SINGAPORE (opens in a new tab)

  18. Cross-Laminated Timber made of Unmodified and Thermally Modified Yellow-Poplar Lumber

    … reduced diffusion by an average of 77%. Outdoor weathering over one year showed no delamination in the 5-layer hybrid CLT, while control YP CLT exhibited significant delamination on the surface and thickness; minor surface checks on TMW were attributed to lower elasticity. These results …

    vt Repository record for Cross-Laminated Timber made of Unmodified and Thermally Modified Yellow-Poplar Lumber (opens in a new tab)

  19. Silicone nanofilaments as functional coatings: properties, applications and modifications

    … basic conditions. Both natural and artificial weathering tests showed promising results for an outdoor application of the coating. The superhydrophobic and anti reflective properties were retained for at least one year of outdoor weathering. Under artificial weathering conditions the coating …

    zurich Repository record for Silicone nanofilaments as functional coatings: properties, applications and modifications (opens in a new tab)

Page 1 of 2