Global ETD Search

Search theses and dissertations gathered from participating repositories worldwide. Every result links back to the library that holds it. No account is needed.

Results 1 to 9 of 9 for “"Overageing"”

  1. CYCLIC OVERAGEING PRE-WELD HEAT TREATMENT FOR NICKEL-BASED SUPERALLOY (RENE 80)

    … alloys. ln this project, the effects of cyclic overageing pre-weld heat treatment scheme proposed by Lim [U.S. Patent No. 5,509,980 (1996) ] on the ductility and weldability improvement of Rene 80 nickel-based superalloy are investigated. Room temperature tensile tests, fractographic studies, …

    nus Repository record for CYCLIC OVERAGEING PRE-WELD HEAT TREATMENT FOR NICKEL-BASED SUPERALLOY (RENE 80) (opens in a new tab)

  2. Ανάπτυξη και χαρακτηρισμός με τεχνικές ηλεκτρονικής μικροσκοπίας υπερκραμάτων νικελίου

    … were performed by subjecting Haynes® 282® to overageing treatments for 100, 500, and 1000 hours at 788°C; the standard second ageing step's temperature, which also falls in the alloy’s operating temperature range. At the same time, the modification of the solution step of SFHT was examined, …

    greece Repository record for Ανάπτυξη και χαρακτηρισμός με τεχνικές ηλεκτρονικής μικροσκοπίας υπερκραμάτων νικελίου (opens in a new tab)

  3. Toughness-strength relationships in high strength 7xxx aluminium alloys

    … the increase in toughness with increased overageing is accompanied by a change in fracture mode from predominantly intergranular/transgranular shear failure to coarse voiding. A fracture toughness model was derived based on the microstructurally dependent work hardening factor, …

    soton Repository record for Toughness-strength relationships in high strength 7xxx aluminium alloys (opens in a new tab)

  4. POST-WELD HEAT TREATMENT CRACKING IN RENE 80 AND EFFECT OF PRE-WELD HEAT TREATMENT

    … of PWHT cracks in the material. After the cyclic overageing pre-weld heat treatment, the microstructure becomes coarser, more stable and homogenous, which gives rise to higher ductility of the base metal and narrower mushy zone and HAZ during welding. All these contribute collectively to reducing …

    nus Repository record for POST-WELD HEAT TREATMENT CRACKING IN RENE 80 AND EFFECT OF PRE-WELD HEAT TREATMENT (opens in a new tab)

  5. Microstructural Evolution and Mechanical Properties of a Medium Manganese Transformation Induced Plasticity Third Generation Advanced High Strength Steel

    … consisting of intercritical annealing and overageing stages compatible with the continuous galvanizing process were investigated in terms of their effects on the microstructure and the mechanical properties from the as-received, tempered martensite (TM) microstructure and a fully …

    mcmaster Repository record for Microstructural Evolution and Mechanical Properties of a Medium Manganese Transformation Induced Plasticity Third Generation Advanced High Strength Steel (opens in a new tab)

  6. Phase stability, constitution and precipitation effects in Fe-Ni-Cr alloys.

    … in the temperature region 400°-500°C. Overageing of the alpha' precipitates after 1000 hours at 500°G was accompanied by the precipitation of a rod like austenite. The elements 2%Mo, 1%Nb, 1/4%Ti and 1% and 2%Si were added totwo Fe-Ni-Cr base alloys. One alloy was an austenitic …

    sheffield-hallam Repository record for Phase stability, constitution and precipitation effects in Fe-Ni-Cr alloys. (opens in a new tab)

  7. Heat treatment optimization and mechanical characterization of a Nickel-based superalloy obtained via hot isostatic pressing (HIPping)

    … order to enhance mechanical properties, avoiding overageing and indicating the best combination of time and temperature to be used to maximize γ’ precipitation. Three optimized recipes were obtained which were verified through tensile and creep tests giving very similar properties one to each …

    poli-torino Repository record for Heat treatment optimization and mechanical characterization of a Nickel-based superalloy obtained via hot isostatic pressing (HIPping) (opens in a new tab)

  8. Crack growth in alloy 709 at high temperatures under fatigue, creep and dwell-fatigue loads

    … At a temperature of 650°C, it is found that overageing does not degrade creep crack growth resistance. Also, a significant improvement in creep crack growth behaviour is confirmed in Alloy 709, compared with 316H. When using the C*-integral to characterise creep crack growth resistance which …

    birmingham Repository record for Crack growth in alloy 709 at high temperatures under fatigue, creep and dwell-fatigue loads (opens in a new tab)

  9. Vieillissement en service d'alliages d’aluminium à durcissement structural : évolution microstructurale et propriétés mécaniques associées

    Les carters et couvercles des boîtes de transmission de puissance des turboréacteurs aéronautiques sont principalement fabriqués à partir d’alliages d’aluminium durcis par précipitation. L'une des exigences critiques en matière de conception est leur résistance au vieillissement thermique pendant …

    star-france Repository record for Vieillissement en service d'alliages d’aluminium à durcissement structural : évolution microstructurale et propriétés mécaniques associées (opens in a new tab) Restricted access