  1. Stress-diffusion interaction during oxide scale growth on metallic alloys

    … alloy is placed in an oxygen environment, oxide scale may be formed on the metal surface. The continuous growth of such oxide scale is enabled by the diffusion of various ionic species in the scale layer primarily driven by the gradient of chemical potentials of these ionic species. In …

    gatech Repository record for Stress-diffusion interaction during oxide scale growth on metallic alloys (opens in a new tab)

  2. Computational models of particle size effects on brittle oxide scale erosion

    … of a continuous surface layer of essentially oxide scale for further oxidation resistance. Erosion of these machine parts by the small solid particle entrained in the liquid or gaseous working environment is a serious problem in many industrial applications. Numerous experiments have been …

    wvu Repository record for Computational models of particle size effects on brittle oxide scale erosion (opens in a new tab)

  3. Growth and structure of nickel oxide scale formed on polycrystalline nickel

    … this thesis the growth and structure of nickel oxide scales formed on polycrystalline nickel during continuous oxidation and oxidation interrupted by vacuum anneals at 800° and PO₂ = 400 Torr were studied. The morphological development of nickel oxide formed commencing with early stages of …

    mcmaster Repository record for Growth and structure of nickel oxide scale formed on polycrystalline nickel (opens in a new tab)

  4. Critical Parameters Controlling Oxide Scale Formation and Hydro-Descaling Efficiency During Steelmaking

    … resulting in the formation of multilayer oxide scales on the steel surface. These scales interact with mold-flux residues originating from the casting process (CC). The morphology, chemistry, and adhesion of oxide scale strongly influence its removability during high-pressure hydraulic …

    must-thes Repository record for Critical Parameters Controlling Oxide Scale Formation and Hydro-Descaling Efficiency During Steelmaking (opens in a new tab)

  5. High-Temperature Oxide Scale Evolution of a Non-Stoichiometric Complex Concentrated Alloy Coating

    … to assess the chemistry and performance of oxide scales cultivated on Al10Co25Cr8Fe15Ni36Ti6 at% coatings. Coatings were developed via high rate unbalanced direct current magnetron sputtering. Optimal processing conditions were selected to promote the growth of thick, dense films on CMSX-8 …

    alabama Repository record for High-Temperature Oxide Scale Evolution of a Non-Stoichiometric Complex Concentrated Alloy Coating (opens in a new tab)

  6. Identification of the Mechanism of Oxide Scale Fracture, and its Correlation with Strain Using Acoustic Emission.

    Thermally formed oxides scales can protect metals from aggressive environments at high temperatures. However the barrier function is destroyed when the oxide fails. Therefore a new 4-point bend test technique has been developed to measure the failure strains and to study the failure mechanisms of …

    southwales Repository record for Identification of the Mechanism of Oxide Scale Fracture, and its Correlation with Strain Using Acoustic Emission. (opens in a new tab) Download PDF for Identification of the Mechanism of Oxide Scale Fracture, and its Correlation with Strain Using Acoustic Emission. (opens in a new tab)

  7. Modeling and simulation of stress-induced non-uniform oxide scale growth during high-temperature oxidation of metallic alloys.

    … rely on the development of a protective oxide scale to sustain the long-term aggressive exposition. However, the oxide scale growth is most of the time coupled with stress and morphological developments limiting its lifetime and then jeopardizing the metallic component reliability. In …

    gatech Repository record for Modeling and simulation of stress-induced non-uniform oxide scale growth during high-temperature oxidation of metallic alloys. (opens in a new tab)

  8. Effect of Ni-content on oxide scale microstructure of FeCr model alloys after breakaway corrosion at 600°C

    … in an aggressive environment to investigate the oxide microstructure after breakaway corrosion. Furthermore, an oxide thickness was chosen as a target for all alloys to facilitate the comparison of oxide microstructure. The conditions of exposure were 5% O2, 95% N2 with a 1 mg/cm2 K2CO3 deposit …

    chalmers Repository record for Effect of Ni-content on oxide scale microstructure of FeCr model alloys after breakaway corrosion at 600°C (opens in a new tab)

  9. Modelling of oxide failure in hot metal forming operations

    Oxide scale can affect many aspects of hot metal forming operations, such as heat transfer, friction and the final surface finish of the rolled product. Surface oxide scale is always present on the steel slab and sometimes on cold rolls. Therefore, the study of the thermo-mechanical behaviour of …

    whiterose Download PDF for Modelling of oxide failure in hot metal forming operations (opens in a new tab)

  10. Ni/Ce as a Cobalt-Free Coating Alternative for SOEC Interconnects

    … widely used as interconnect materials in solid oxide electrolysis cells (SOECs), but oxide-scale growth and chromium evaporation can reduce their durability. Although Co-based coatings effectively suppress chromium volatilisation, concerns regarding cobalt supply, cost, and sustainability …

    chalmers Repository record for Ni/Ce as a Cobalt-Free Coating Alternative for SOEC Interconnects (opens in a new tab)

  11. Performance Evaluation of Candidate Materials For Solid Oxide Cell Interconnects

    … suggesting better protective properties of the oxide scale formed on the surface of Crofer 22 APU. The findings highlight that Crofer 22 APU, due to its protective oxide scale, is the most promising candidate for SOFC interconnects under the tested conditions. Furthermore, the possibility of …

    chalmers Repository record for Performance Evaluation of Candidate Materials For Solid Oxide Cell Interconnects (opens in a new tab)

  12. Nickel-iron-based metallic inert anodes for aluminium electrolysis

    … can be reduced by applying a protective metal oxide scale. Unfortunately, the behaviour of the scale during electrolysis is not well understood. In the present study, the behaviour of nickel-iron-based anodes having thermally grown protective oxide scales was investigated. Oxidised binary …

    unsw Repository record for Nickel-iron-based metallic inert anodes for aluminium electrolysis (opens in a new tab)

  13. Corrosion Behaviour of Fe-Cr and Ni-Cr Alloys in O2, H2O and H2O+O2 gases at 700°C

    … Fe-Cr and Ni-Cr alloys and to understand the oxide scale formation in high and low pO2 atmospheres. In this work, model Fe-Cr (0, 5, 10, 20 and 30wt%) and Ni-Cr (0, 5, 10, 20 and 30wt%) alloys were reacted at 700°C in Ar-20%O2, Ar-20%O2-20%H2O and Ar-20%H2O, respectively. For pure iron, the …

    unsw Repository record for Corrosion Behaviour of Fe-Cr and Ni-Cr Alloys in O2, H2O and H2O+O2 gases at 700°C (opens in a new tab)

  14. Oxide Scales Behaviour During Descaling and Hot Rolling

    … studies completed on the effect of the secondary scales and the influence of the primary scales has been unnoticed. The aim of this research was to study the behaviour of oxide scales during the descaling and hot rolling of two steel grades, particularly the influence of primary scales. In this …

    whiterose Download PDF for Oxide Scales Behaviour During Descaling and Hot Rolling (opens in a new tab)

  15. The Oxidation of Fe-Mn Alloys in Carbon Dioxide-Carbon Monoxide Atmospheres at 1000°C

    … contents up to 60 w/o exposed to carbon dioxide-carbon monoxide atmospheres at 1000°C have been determined as a function of gas composition by a gravimetric technique. The experimental conditions were chosen in order that the product of the reaction between metal and oxidizing atmosphere …

    mcmaster Repository record for The Oxidation of Fe-Mn Alloys in Carbon Dioxide-Carbon Monoxide Atmospheres at 1000°C (opens in a new tab)

  16. A microstructural investigation of Fe-oxides for developing high-temperature corrosion lifetime prediction models

    … study was to investigate the microstructure of oxide scales formed in environments relevant to biomass- and waste boilers used for superheater appli cations. It also investigated how KCl can a!ect both the corrosion kinetics and mi crostructure, specifically the characteristics of oxide grain …

    chalmers Repository record for A microstructural investigation of Fe-oxides for developing high-temperature corrosion lifetime prediction models (opens in a new tab)

  17. Processing-Microstructure-Properties Relationships in Additively Manufactured Zrb2-Sic Ceramics

    … (AM) with CO2. The oxidation kinetics and scale microstructures were compared for ZrB2-SiC made by hot pressing (HP) and by AM coupled with PS. All specimens exhibited parabolic oxidation kinetics. The difference in oxidation behavior becomes evident at temperatures of 1100-1400°C …

    must-thes Repository record for Processing-Microstructure-Properties Relationships in Additively Manufactured Zrb2-Sic Ceramics (opens in a new tab)

  18. New strategies to understand oxidation processes of high temperature materials

    … oxidation tests provided insight into the oxide scales formed on the alloys, and long-term tests characterized the oxygen consumption rate up until complete oxidation. Comparison of the results from these tests helped understand how the alloy composition affects the oxide scale formed, and …

    umn Repository record for New strategies to understand oxidation processes of high temperature materials (opens in a new tab)

  19. Feasibility of using MAX phase materials in molten salt reactors

    … At 850°C, the sample exposed to LKE formed an oxide scale containing lithium aluminate and lithium titanate which underwent pitting corrosion, whereas the sample exposed to KME formed a stable magnesium aluminate scale by diffusion of aluminium from the underlying MAX phase. The samples of …

    whiterose Download PDF for Feasibility of using MAX phase materials in molten salt reactors (opens in a new tab)