Global ETD Search

Search theses and dissertations gathered from participating repositories worldwide. Every result links back to the library that holds it. No account is needed.

Results 1 to 12 of 12 for “"Oxides formation"”

  1. Modeling of the nitrogen oxides formation process applicable to several diesel combustion modes

    Como consecuencia de las exigentes legislaciones medioambientales actualmente en vigor, como las Euro Emission Standards en Europa, los investigadores e ingenieros se ven forzados a "re-desarrollar" el proceso de combustión diésel para hacerlo menos contaminante. Uno de los principales …

    upv Repository record for Modeling of the nitrogen oxides formation process applicable to several diesel combustion modes (opens in a new tab)

  2. Mecanismos da formação da superfície heterogênea no aço inoxidável ferrítico 439

    … the mechanisms is understanding the transformations of the surface during the production process. The work was carried out through observations, understanding the phenomena of hot oxidation and removal of oxides layers by chemical pickling, relating science to industrial practice. The …

    brazil-ufmg Repository record for Mecanismos da formação da superfície heterogênea no aço inoxidável ferrítico 439 (opens in a new tab)

  3. Steam oxidation of advanced high temperature resistant alloys for ultra-supercritical applications

    … scale morphology. In case of T23, it triggers formation of micro-layered inner oxide, whereas for T92 it promotes the formation of an outer haematite layer. For austenitic steels, the faster steam flow increases the formation of initially protective oxide scales, but also accelerates the growth …

    cranfield Repository record for Steam oxidation of advanced high temperature resistant alloys for ultra-supercritical applications (opens in a new tab)

  4. Welding of cast A359/SiC/10p metal matrix composites

    … interface between the weld and the base MMC. Oxides formation was controlled along the weld joint. Low heat inputs provided higher weld strengths and better weld integrity. It was found that the weld strengths were approximately 85% of the parent material strength. The weld region had higher …

    tamu Repository record for Welding of cast A359/SiC/10p metal matrix composites (opens in a new tab)

  5. Analysis of Differential Corrosion on High-Silicon Steel Laminations

    … on unprocessed lamination surfaces to form iron oxides. Formation of red oxide (Fe203) was at a maximum for 900°F, 60 minutes. At 1100°F, 60 minutes, the laminations tended to form black oxide (Fe304) which is more resistant to further corrosion. These results suggest that the direct attack of …

    wku-diss Repository record for Analysis of Differential Corrosion on High-Silicon Steel Laminations (opens in a new tab)

  6. Síntese e caracterização de nanopartículas de vidro bioativo contendo Ca e Mn e incorporação em hidrogéis injetáveis de Pluronic® F127

    … structure was verified, as well as the manganese oxides formation according to the Mn concentration used. In vitro results showed controlled ion release capacity and bioactivity in physiological medium. Cellular assays showed a manganese dose-dependent effect on cell viability and alkaline …

    brazil-ufmg Repository record for Síntese e caracterização de nanopartículas de vidro bioativo contendo Ca e Mn e incorporação em hidrogéis injetáveis de Pluronic® F127 (opens in a new tab)

  7. Metal Dusting of Heat-Resistant Alloys

    … caused less carbon deposition and more oxides formation on the alloy surfaces leading to a reduction in the attack aggressiveness. UCX© exhibited the highest resistance to metal dusting whilst HP suffered the severest attack. The presence of high concentrations of chromium at the surface …

    cambridge Repository record for Metal Dusting of Heat-Resistant Alloys (opens in a new tab)

  8. Desenvolvimento de procedimentos para análise inorgânica de biodiesel usando técnicas espectroanalíticas

    … added to the plasma, probably due to the highest formation of oxides. However, despite oxides formation best accuracies were reached when employing oxygen gas.

    brazil-ufscar Repository record for Desenvolvimento de procedimentos para análise inorgânica de biodiesel usando técnicas espectroanalíticas (opens in a new tab)

  9. Effect of corroded reinforcement in RC structures: from cracking to bond performance

    … layer between steel and concrete because of the oxides formation; therefore, bond between the materiala changes. In the present dissertation, steel reinforcement corrosion and its mechanical implications were studied; in particular, the investigation was developed both experimentally and …

    poli-torino Repository record for Effect of corroded reinforcement in RC structures: from cracking to bond performance (opens in a new tab)

  10. Exploring microbial mechanisms in arsenic adsorption and desorption in iron-manganese binary oxides

    … onto and from iron-manganese (Fe-Mn) binary oxides formed through both biological and abiotic processes. Indeed, iron and manganese oxides often co-exist in the environment, and the roles of these binary phases in trace metal cycling are currently under-investigated. Fe-Mn binary oxides might …

    oxford Repository record for Exploring microbial mechanisms in arsenic adsorption and desorption in iron-manganese binary oxides (opens in a new tab)

  11. Mineralogy and geochemistry of iron-oxides in the Olympic Dam IOCG-deposit and adjacent prospects, South Australia

    … in the genetic conditions. Analysis of Fe-oxides, bridging scales of observation from deposit down to the nanoscale, highlights different formation conditions within deposits and prospects from the ~1.6 Ga Olympic Dam district, South Australia. In addition, Fe-oxides from the ~5.3-1.6 Ma El …

    adelaide Repository record for Mineralogy and geochemistry of iron-oxides in the Olympic Dam IOCG-deposit and adjacent prospects, South Australia (opens in a new tab)

  12. Etude en fretting usure sous hautes températures d'un contact Waspaloy/René125 : formation et stabilité des "glaze layers"

    … qu’à partir de 400°C, l’interface génère la formation d’une glaze layer lubrifiante qui réduit considérablement la cinétique de l’usure. En fixant la température à 700°C (température de l’application industrielle), nous avons étudié la stabilité de ces couches protectrices vis-à-vis de la …