Global ETD Search
Search theses and dissertations gathered from participating repositories worldwide. Every result links back to the library that holds it. No account is needed.
Results 1 to 9 of 9 for “"PWSCC"”
-
Preferential Intergranular Oxidation and Stress Corrosion Cracking of Alloy X-750 in CO-CO2 Gas Mixtures
… to primary water stress corrosion cracking (PWSCC) in both pressurized water reactors (PWR) and boiling water reactors (BWR). Currently, preferential intergranular oxidation (PIO) is the most accepted mechanism for PWSCC, where the primary water environment (~300 °C hydrogenated water) …
-
Effectiveness of Surveillance Sampling Strategies for Detecting Steam Generator Tube Degradation
… primary water stress corrosion cracking (PWSCC) of steam generator (SG) tubes as an example degradation mechanism. An empirical model for PWSCC crack growth is adopted to simulate crack growth over a 40-year operating lifetime. Surveillance and maintenance strategies similar to those …
-
A probabilistic fracture mechanics model for the tubing degradation of the Koeberg steam generators
… 600) to primary water stress corrosion cracking (PWSCC) has been a major concern to the nuclear industry since 1971, when this phenomenon was first observed outside the laboratory. Since the susceptibility of Inconel 600 to PWSCC in pure water was first established as a certainty, various …
-
Predicting the Crack Response for a Pipe with a Complex Crack
… by primary water stress corrosion cracking (PWSCC). A coded solution for a single material with a weld was developed that gives an accurate maximum load and crack driving force prediction for a pipe with a through wall crack (TWC), called LBBEng. To support the analysis of a CC, …
-
Stress Corrosion Cracking of Ni-Fe-Cr Alloys Relevant to Nuclear Power Plants
… plants. The mechanism of primary water SCC (PWSCC) was studied in Alloys 600, 690, 800 and Alloy 82 dissimilar metal welds using the internal oxidation model as a guide. Initial experiments were carried out in a 480 °C hydrogenated steam environment considered to simulate high temperature …
-
Weldability Evaluation of High-Cr Ni-Base Filler Metals using the Cast Pin Tear Test
… by primary water stress corrosion cracking (PWSCC). These alloys provide optimum resistance to PWSCC in nuclear power plant cooling systems. However some of these nickel alloys present weldability challenges including susceptibility to solidification cracking and ductility dip cracking. There …
-
Macrostructure and Micro chemistry Analysis on Stress Corrosion Cracking(SCC) of Alloy 690
… of primary water stress corrosion cracking (PWSCC). The alloy 690 was chosen as the material of interest for this study because of its relevance in current application in nuclear industries and application on different structural component at extreme environmental conditions. An integrated …
-
Effect of thermal ageing on Alloys 690 and 52 in pressurized water reactor applications
… primary water stress corrosion cracking (PWSCC) resistance of PWR components, such as the steam generator for Alloy 690 and the reactor pressure vessel (RPV) safe-end dissimilar metal weld (DMW) for Alloy 52. In addition, it is known that post-weld heat treatment (PWHT) affects narrow …
-
APPLICABILITY OF COLD METAL TRANSFER FOR REPAIR OF DISSIMILAR METAL WELDS IN STAINLESS STEEL PIPING IN NUCLEAR POWER PLANTS
… from primary water stress corrosion cracking (PWSCC) requires welds to be repaired using structural weld overlays (SWOLs) on the outer pipe diameter to prevent through-thickness breaches. In recent years the nuclear power industry has faced challenges with hot cracking when depositing SWOLs …