Global ETD Search
Search theses and dissertations gathered from participating repositories worldwide. Every result links back to the library that holds it. No account is needed.
Results 1 to 14 of 14 for “"Parabolic law"”
-
Analyses of isothermal solidification kinetics during transient liquid phase bonding of silver with aluminium and copper filler metals
… The results show that a deviation from the parabolic law occurred during the isothermal solidification process, at all the selected bonding temperatures. This deviation from the parabolic law cannot be explained by the existing concepts suggested in the literature. In this research work, …
-
Ion assisted deposition of multicomponent thin films
… found that growth of the PbTiO₃ phase obeyed the parabolic law and the effective activation energy was estimated to be 108 kJ/mole. It is believed that the mechanism of this reaction was dominated by grain boundary diffusion of the participating cations.
-
Anisotropy effects in the critical field of superconducting tin-indium alloys
… are found to reduce the deviation from the parabolic law, h = 1 - t2. The observations are explained by theoretical predictions of Clem for which the meansquared anisotropy in pure tin is taken to be (a2) = .014 ± .001.
-
ΚΙΝΗΤΙΚΗ ΤΗΣ ΕΚΡΟΦΗΣΕΩΣ ΦΩΣΦΟΡΟΥ ΑΠΟ ΤΕΣΣΕΡΑ ΕΛΛΗΝΙΚΑ ΕΔΑΦΗ. Η ΔΙΑΧΥΣΗ ΣΑΝ ΚΑΘΟΡΙΣΤΙΚΟ ΣΤΑΔΙΟ ΤΗΣ ΤΑΧΥΤΗΤΟΣ
… USED KINETIC EQUATIONS INCLUDING FUNCTIONAL RATE LAWS (ZERO, FIRST AND SECOND ORDER, AS WELL AS RESOLUTION OF THE KINETIC CURVE INTO THREE EXPONENTIALEXPRESSIONS) THE PARABOLIC LAW AND THE BANGHAM AND THE ELOVICH EQUATIONS, WERETESTED WITH OUR DATA AND FOUND INADEQUATE, WITH THE LAST TWO SHOWING …
-
The transition from internal oxidation to external oxidation is silver-zinc alloys
… a light microscope, and was observed to obey the parabolic law. A model based on volume diffusion control of oxygen has been proposed for the velocity of the internal ZnO precipitates.</p> <p>The Ag-12.9 wt % Zn alloy was observed to form an internal ZnO scale in combination with an external ZnO …
-
Mechanism of siliconizing of molybdenum and tantalum by vapor deposition
… fused quartz helix balance, generally follows a parabolic law, y = k t1/2, where y = weight gain, t = time, and k = rate constant. The activation energy is estimated at 21.6 k cal/mole for siliconizing of molybdenum. Deposition rate is greatly reduced at the later stage of the diffusion …
-
Influência da adição de cério na microestrutura e comportamento de oxidação de aços inoxidáveis Fe-Mn-Si-Cr-Ni com efeito de memória de forma
… to the oxidation resistance. The restrict parabolic law is only observed for alloys containing 0.18 and 0.42 wt.% of Ce. The oxide layer formed after 120 h of oxidation is composed of Mn oxides, promoting the depletion of this element below the oxide and phase transformation from austenite …
-
The Linear Growth Rates of Pentaerythritol Crystals
… growth rate was kinetically controlled having a parabolic law over most of the range of conditions studied with an activation energy of 8.47 Kcal/mol. The effect of di-Pe was generally that it caused a slight reduction in the growth rate except at certain critical concentrations where the effect …
-
Rate of Diffusion-controlled Adsorption Processes
… for unsteady state diffusion derived from Fick's law for spheres usually, ignoring the amount adsorbed and the shape of the adsorption isotherm. These inappropriate equations result in calculated diffusivities that are too low and activation energies that are too large. </p> <p> Numerical. …
-
Oxidation resistance of Ti-Al intermetallic alloys and protection by ceramic coating
… extent the oxide layers grew according to a parabolic law. The kinetic rate constants and the activation energies were calculated. These kinetic parameters allowed to assess a rank of oxidation resistance, which can be correlated with the composition of the alloys. In order to improve the …
-
Modélisation de la tribocorrosion d'aciers inoxydables dans l'eau à haute pression et haute température
… The oxidation kinetic was found to follow a parabolic law (diffusion controlled oxide growth). Rubbing resulted in repeated scratching of the surface leading to a thinning of the oxide film and thus to an enhanced anodic oxidation. A quantitative model of the electrochemical response of …
-
Thermal Upgrading of Nickeliferous Pyrrhotite Tailings for Nickel Recovery
… sulfidization by Pyrr were found to follow a parabolic law, which indicates that the rate-controlling step is the diffusion of Fe cations within the newly formed sulfide. Three mechanisms of the ferronickel alloy formation resulting from the interaction between the metallic iron and the …
-
Corrosion Assessment and Mechanisms of Materials in Advanced Thermal Energy Production Systems
… C. The oxidation kinetics of DSS 2205 follows parabolic law. O2 and H2O act as oxidants while SO2 and HCl are the pitting inducers. In general, DSS 2205 is a suitable candidate for the construction of flue gas components. High-temperature s-CO2 Brayton cycle has been recognized as a promising …
-
Valorisation des coques de noix de palmiste dans la construction des routes à faible trafic
La production de l’huile de palme génère plusieurs déchets dont les coques de noix de palmistes (CNP). Face à l’épuisement des ressources naturelles, utilisables en technique routière, la valorisation des déchets agricoles comme les coques de noix de palmiste constitue une solution alternative …