Electrochemical Studies of Molten Salt Corrosion
… in acidic media. At 350 °C, the fundamental parting limit (55-60 at.% of the less-noble element in aqueous solutions) decreased to 44 at.% due to the high surface mobility of elemental Ni. At 350 °C, the parting limit further decreased to a value of approximately 32 at.% Fe when elemental Ni …
-
The formation and evolution of bi-continuous porous structures : mechanisms and applications
… solid solution. The process displays a parting limit and coarsening similar to electrochemical dealloying. In Chapter 3, we demonstrate that the electrochemical reduction of a ZnO anode, the charging process in alkaline Zn batteries, is also a process of percolation dissolution toward …
-
Structural Transformations Of Multimetallic Nanoparticles
… alloy NPs with Cu atomic fractions above the parting limit. The electrochemically active surface area and the specific activity of the dealloyed nanoframes can be systematically tuned to achieve the optimal electrocatalytic activity. Both the stability and the activity of the dealloyed Au …
-
Exploring De-alloying in Fe-Ni-Cr Alloys and its Relationship to Stress Corrosion Cracking in Nuclear High Temperature Water Environments
… LN content below which de-alloying stops (the parting limit). In Fe-Ni-Cr engineering alloys de-alloying may be responsible for Cl-SCC, although this has not been proven explicitly. Initial indications show that de-alloying causes SCC in hot, caustic environments. In some cases, Ni enrichment …