Global ETD Search

Search theses and dissertations gathered from participating repositories worldwide. Every result links back to the library that holds it. No account is needed.

Results 1 to 20 of 39 for “"Plastic zone size"”

  1. The effect of the mixed mode ratio on the plastic zone size and shape and the J-integral

    … an edge crack in order to assess the resulting plastic zone size and shape, and to evaluate the J-integral. The theoretical approach allows the determination of the displacement, strain and stress field at every point around the crack tip for any mixed-mode loading condition. This permits, by …

    ttu Repository record for The effect of the mixed mode ratio on the plastic zone size and shape and the J-integral (opens in a new tab)

  2. Small fatigue crack growth in high strength aluminium alloys

    … pattern (SAECP) method was used to measure the plastic zone size (PZS) and shape of small fatigue cracks. A novel experiment enabling PZS measurements on growing small fatigue cracks was developed to investigate the development of plastic zone size and shape with crack growth and the relation …

    the-open-u Repository record for Small fatigue crack growth in high strength aluminium alloys (opens in a new tab)

  3. Modified Dugdale Model

    A precise determination of the influence of plastic yielding on the deformation and failure at a crack tip is needed for accurate predictions of the behavior of cracked bodies under static load large enough to cause fracture, and subcritical repetitive loads which cause fatigue. The catastrophic …

    sdstate Repository record for Modified Dugdale Model (opens in a new tab)

  4. Charpy Impact Testing of Twinning Induced Plasticity and Transformation Induced Plasticity High Entropy Alloys

    … resistance. Even more recently, twinning induced plasticity (TWIP) and transformation induced plasticity (TRIP) non-equiatomic high entropy alloys have been engineered, promising increased strength and ductility as compared to their equiatomic counterparts. However, impact and fracture resistance …

    unt Repository record for Charpy Impact Testing of Twinning Induced Plasticity and Transformation Induced Plasticity High Entropy Alloys (opens in a new tab)

  5. Influence of specimen geometry on fatigue crack growth rates in cast and forged Ti- and Ni-based alloys

    … faster than cracks in C(T) specimens, the plastic zone size in Kb and C(T) specimens was evaluated through numerical simulations using the finite element method. Further, the grain sizes in cast Ti-64 and IN-718 specimens were measured. The measured grain sizes were found to be …

    chalmers Repository record for Influence of specimen geometry on fatigue crack growth rates in cast and forged Ti- and Ni-based alloys (opens in a new tab)

  6. The application of the Dugdale model to an orthotropic plate

    … and displacements along the crack and elastic plastic interface were found. The effect of orthotropy on several isotropic properties was found to be a multiplicative factor which is a function of the state of orthotropy. The yield stress is assumed to follow a von Mises' yield criterion which …

    vt Repository record for The application of the Dugdale model to an orthotropic plate (opens in a new tab)

  7. The Effect of Phase Transformation on The Fatigue Crack Growth Rate of Austenitic Stainless Steels Tested in Argon and Hydrogen Atmospheres

    … were also measured using various techniques. The plastic zone size of some specimens was determined by using a microhardness tester and electron channeling data. The residual stress around the crack tip was measured using strain gages. The volume fraction of martensite was determined by measuring …

    uiuc Repository record for The Effect of Phase Transformation on The Fatigue Crack Growth Rate of Austenitic Stainless Steels Tested in Argon and Hydrogen Atmospheres (opens in a new tab)

  8. Modelling of combined roughness and plasticity induced closure effects in high strength Al-alloys

    <p>An investigation of plasticity induced crack closure (PICC) and roughness induced crack closure (RIC C) behaviour using finite element (FE) methods is presented for cracks subjected to small scale yielding (SSY) conditions. For constant amplitude (CA) undeflected cracks have been examined under …

    soton Repository record for Modelling of combined roughness and plasticity induced closure effects in high strength Al-alloys (opens in a new tab)

  9. APPLICATION OF THE LASER SPECKLE TECHNIQUE IN THE STUDIES OF CRACKS AND NOTCHES IN PLATES

    … in three areas: Crack tip and notch root plastic zone size measurements, crack initiation detection and strain measurement in polypropylene. In this work, the changes in speckle patterns as a result of plasticity and fatigue damage are studied by using a newly defined parameter called the …

    nus Repository record for APPLICATION OF THE LASER SPECKLE TECHNIQUE IN THE STUDIES OF CRACKS AND NOTCHES IN PLATES (opens in a new tab)

  10. Fatigue damage accumulation in nickel base superalloys.

    … bend tests. Substantial differences in grain size and structure occurred across the section of the disc. Fatigue damage occurred primarily as a result of persistent slip band formation, cell formation, Orowan looping and precipitate shearing. A small number of grains exhibited dislocation …

    whiterose Repository record for Fatigue damage accumulation in nickel base superalloys. (opens in a new tab)

  11. Corrosion and high-temperature deformation characteristics of a target structural material for transmutation applications

    … at elevated temperatures due to increased plasticity. The results of SSR testing, in the 90°C acidic solution, indicate that the failure stress was increased but the ductility was reduced to some extent at longer tempering times. The CPP results indicate that the critical potentials …

    unlv Repository record for Corrosion and high-temperature deformation characteristics of a target structural material for transmutation applications (opens in a new tab)

  12. Effect of heat treatment on deformation and corrosion behavior of Type 422 stainless steel

    … parameters were enhanced due to increased plastic flow at elevated temperatures. The results of stress corrosion cracking tests performed by slow strain rate technique in the 90°C acidic solution revealed higher failure stress and reduced ductility to some extent for specimens tempered …

    unlv Repository record for Effect of heat treatment on deformation and corrosion behavior of Type 422 stainless steel (opens in a new tab)

  13. The effect of stress ratio, maximum stress, stress amplitude and yield strength of materials on fatigue crack closure of 2024 aluminum and 4130 steel

    … be concluded that crack closure is a function of plastic zone size at the tip of a growing fatigue crack. Crack closure is a plane stress phenomenon, but it also exists in plane strain condition.

    missouri Repository record for The effect of stress ratio, maximum stress, stress amplitude and yield strength of materials on fatigue crack closure of 2024 aluminum and 4130 steel (opens in a new tab)

  14. The influence of the environment on the plastic zone of a propagating fatigue crack tip in aluminum and steel

    … used in an effort to measure changes in bulk plasticity due to changes in environment at the tip of a propagating fatigue crack. The study was done to determine if there are changes in the residual stresses in the plastically deformed region as a function of the two environments which were …

    missouri Repository record for The influence of the environment on the plastic zone of a propagating fatigue crack tip in aluminum and steel (opens in a new tab)

  15. Small Scale Fracture Toughness Testing

    … plane strain, is independent of the geometry and plastic zone size. Further the development of a simple single specimen J-integral test method is done during this work. In terms of the data obtained both the minimum C.O.D.i values and the Jlc values increase with increasing ductility of the …

    mcmaster Repository record for Small Scale Fracture Toughness Testing (opens in a new tab)

  16. The Ductile-Brittle Fracture Transition: A Comparison of Macro and Microscopic Observation on Compact Tension Specimens

    … inch and 1.00 inch. Load-COD data and gross plastic flow measurements are compared to scanning electron microscopy (SEM) fracture surface analysis in order to correlate macroscopic observations of the ductile-brittle transition on a macroscopic scale with microscopic data permit the validity …

    ut-knoxville Repository record for The Ductile-Brittle Fracture Transition: A Comparison of Macro and Microscopic Observation on Compact Tension Specimens (opens in a new tab)

  17. Microstructure for Enhanced Plasticity and Toughness

    … of various microstructural factors like grain size, texture, constituent particles, precipitates on crack initiation and propagation. Tensile properties were evaluated by mini-tensile tests. Crack growth in WE43 sheets was also affected by mechanics and digital image correlation (DIC) was …

    unt Repository record for Microstructure for Enhanced Plasticity and Toughness (opens in a new tab)

  18. INVESTIGATION OF FATIGUE CRACK BEHAVIOR ON NEAR THRESHOLD REGION OF AISI 4340 STEELS FOR DIFFERENT HEAT TREATMENT CONDITIONS

    … limit evaluation for components with small crack size. Determining long crack threshold value as a design criterion is not a new research topic; even so, some anomalies arising from different test methods in the literature make this subject suitable for investigation. The fatigue crack growth …

    metu Repository record for INVESTIGATION OF FATIGUE CRACK BEHAVIOR ON NEAR THRESHOLD REGION OF AISI 4340 STEELS FOR DIFFERENT HEAT TREATMENT CONDITIONS (opens in a new tab)

  19. Mechanistic Failure Criterion for Unidirectional and Random Fibre Polymer Composites

    … interfacial debonding and effects of the plastic zone size. In random fibre composite the criterion also includes the effect of fibre orientation and fibre pull-out energy. The pull-out energy was calculated with the help of a finite element model. Several experiments were performed to …

    uwo Repository record for Mechanistic Failure Criterion for Unidirectional and Random Fibre Polymer Composites (opens in a new tab)

  20. Fatigue crack growth of ultra fine grained aluminium

    … analysis in the crack tip process zone and outside the crack region to study fatigue induced changes and also provide a detailed analysis of crack path. A combination of intergranular and transgranular crack growth was reported at the fatigue threshold. Grain boundary sliding is a …

    unsw Repository record for Fatigue crack growth of ultra fine grained aluminium (opens in a new tab)

Page 1 of 2