Conservation of Polyester-urethane Magnetic Audio Tapes and Discrimination of Textile Fiber Dyes Using Spectroscopy and Chemometrics
… techniques and chemometrics. Conservation of polyester urethane magnetic audio tapes has become a major challenge since they are susceptible to degradation via hydrolysis. The world’s modern cultural history is vastly recorded in this media, and now conservationists need a non-destructive …
-
New strategies for conservation of cultural heritage under climate change conditions
… of southern Europe. The performance of a novel polyester-urethane cutin-based coating for bronze was evaluated via laboratory ageing simulating rain exposure (stagnant and run-off), and temperature/relative humidity/UV cycles. A multi-analytical approach allowed to assess corrosion processes and …
-
Non-Destructive Determination of Magnetic Audio Tape Degradation for Various Tape Chemistries Using Spectroscopy and Chemometrics
… the majority of these tapes were made with a polyester urethane (PEU) binder, which has shown to degrade through hydrolysis of the ester component, called sticky shed syndrome (SSS). As the name implies, degraded tapes will stick and shed onto player guides and heads during playback. This can …
-
Spectroscopy and Chemometrics for Cultural Heritage and Forensics: Conservation of Magnetic Tape by Identifying Degraded Polymer Signatures; and Characterizing the Chemiluminescent Reaction of Luminol with Blood
… medium. A majority of magnetic tapes contain polyester urethane (PEU) binders, which are known to degrade via hydrolysis, making the retrieval of recorded data difficult and at times impossible. Degraded tapes are currently identified through visual inspection followed by playback on vintage …
-
The compressive response of open-cell foams
… class of foams. The experiments are conducted on polyester urethane open-cell foams of several cell sizes. They include: measurement of the compressive response of the foams, characterization of the foam microstructure, and measurement of the mechanical properties of foam ligaments. It was found …
-
Steric and Anchimeric Effects on the Hydrolysis of Oligoesters and their Influence on End-Use Polyurethane Coatings
<p>Polyesters are used in a wide range of industries due to the breadth of formulation and the good balance of end properties and cost. However, the performance of polyesters is affected by the sensitivity of ester groups towards water. Based on this setback, the objective of this dissertation was …
-
Materials and clinical aspects of orthodontic treatment with aligners
… two different aligner companies, Clear Aligner (polyester) and Invisalign(polyester-urethane) for a two-week period. The acidity, changes in the chemical composition and changes in Martens Hardness (HM), elastic modulus (EIT), elastic index (nIT) and relaxation (RIT) were studied. Finally, …
-
Development of functional biopolymers with controlled architecture
… oligomères ont été utilisés pour préparer des polyesters amides fonctionnalisés acrylates ou mercaptans. Dans une approche parallèle, du PCL multi acrylate a été préparé avec succès par copolymérisation par ouverture de cycle de méthacrylate de glycidyle avec du caprolactone. Des copolymères …