Global ETD Search
Search theses and dissertations gathered from participating repositories worldwide. Every result links back to the library that holds it. No account is needed.
Results
Showing 1 to 20 of 62 for “"Portlandite"”.
-
Understanding Pozzolanic Reactivity: Dissolution Kinetics of Silica Fume and Portlandite
… primarily acts by replacing calcium hydroxide (portlandite) with additional calcium silica hydrate gel, the dissolution kinetics both of SFs and of calcium hydroxide are interrogated using conductance measurements. This research identifies the influence of SFs' chemical composition and physical …
-
Thermodynamics of mixing in the system whitlockite-fluorite-portlandite-hydrophyllite and the applications to silicic magmatism
Thermodynamics of mixing for solids and liquids in the anhydrous apatite system Ca$\sb3$(PO$\sb4)\sb2$ - CaF$\sb2$ - Ca(OH)$\sb2$ - CaCl$\sb2$ are quantified using mathematical modeling of new and existing experimental data. These data apply to apatite experiments or to understanding natural …
-
Characterization and quantification of crystalline and amorphous phase assemblage in ternary binders during hydration
… in the ternary diagram OPC‒CAC‒CsHx. C‒S‒H, portlandite, ettringite and AFm phases stand as main hydration products in the OPC‒rich combinations. C‒S‒H accounts for ~70% of the X‒ray amorphous fraction. In the CAC‒CsHx rich combinations ettringite along with AH3, monosulphoaluminate, …
-
Gaining higher salt scaling resistance with slag concretes
… in these blends. Consequently, the amount of portlandite as well as the Ca/Si ratio in the C-A-S-H chains decrease as slag replacement increase. It has been reported that addition of slag to concrete has a two-faceted outcome regarding its resistance against deicing salts. Slag improves …
-
Influence de la carbonatation sur la microstructure, la minéralogie et la lixiviation du cuivre pour les matériaux traités par stabilisation/solidification avec ou sans bentonite
… de ciment S/S à cause de l'appauvrissement en portlandite, qui a un effet tampon important pour résister aux attaques acides. Les résultats de microtomographie à rayons X (CT scan) montrent que la porosité diminue après la carbonatation accélérée et induite pour un matériau composé à 100 % de …
-
A Method to Determine Lime Demand for Soil Stabilization Using Soluble Calcium Ions and Zeta Potential Measurements
… at which the pH reaches the saturation pH of portlandite is regarded as the optimum lime dosage. This protocol although widely adopted does not provide insights about the type of the pozzolanic products, the stabilization potential of a soil, or the benefit/ill-effects of over liming. Inspired …
-
Effect of phosphorus and fluorine compounds from phosphogypsum on the hydration of major mineral phases in portland clinker : C3S and C3A
… up to 13.06 hours. TGA and XRD confirm delayed portlandite formation. In C3A hydration, orthorhombic C3A hydrates faster than cubic C3A, with PG substitution delaying the hydration peak. While P2O5 had a minimal effect on peak timing, it reduced total heat release. Additionally, F⁻ significantly …
-
Σύνθεση ζεολίθου από ελληνικές ιπτάμενες τέφρες παρουσία υδατικών διαλυμάτων Η2Ο2
… lime decreased to 0-3 wt% (from 4-14 wt%) and portlandite decreased to 0-6 wt% (from 13 wt%), while the initial content of calcite increased to 8-26 wt% (from 6-19 wt%).Anhydrite (CaSO4), a constituent of the initial fly ashes, is partially consumed leading to the formation of gypsum …
-
Impacts of Water and Saline Brine Flow on Fractured Wellbore Cement
… to nitrogen, attributable to the dissolution of portlandite which reduces the stiffness of the cement adjacent to the fracture surface and allows for additional closure of the fracture. During flow of saline brine, the hydraulic aperture progressively decreased and eventually approached that …
-
Étude de la carbonatation des granulats de béton recyclé altéré par la réaction alcali-silice
… physico-chimiques majeures (consommation de portlandite et formation de carbonates de calcium), conduisant à une densification microstructurale avec une diminution de la porosité et de l’absorption d’eau et une augmentation de la densité. Ces modifications influencent fortement le …
-
Calcium Carbonate Formation in Energy-Related Subsurface Environments and Engineered Systems
… related to the formation of a wide and weak portlandite-depleted zone in the cement matrix immediately inside of the carbonated layer. The effects of 0.05 M of sulfate ions were also examined. Interestingly, the additional sulfate ions were found to mitigate CO2 attack by forming a more …
-
An assessment of carbon dioxide removal potential from stormwater ponds using concrete-based materials
… driven by their alkaline nature and high portlandite (Ca(OH)2) content. However, the mechanistic understanding of how specific parameters including mass, surface area, and degradation of calcium silicate hydrate (C-S-H) phases collectively control carbonation kinetics and CO2 uptake under …
-
Otimização de formulação de pastas de cimento contendo bentonita para aplicação em poços petrolíferos com baixo gradiente de fratura
… that there was the presence of etringite, portlandite, calcium silicate and quartz. It was also observed that the images obtained by scanning electron microscopy (SEM) the paste of 13,5 lb/gal with 4 % bentonite showed notoriously the presence of ettringite needles, as well as the steps of …
-
An Isotopic and Mineralogical Investigation of Concrete Decay
… phases present in cement pastes, in particular portlandite, can have random or preferred orientations at the cement paste to aggregate interface. The micro-mineralogy of the cement paste to aggregate bond interface in concretes is texturally complex and concrete mixing techniques can effect the …
-
Raman spectroscopy for characterizing and determining the pozzolanic reactivity of fly ashes
… hydroxides showed the gradual spatial growth of portlandite in the studied areas of the samples. The growth rate and concentration of portlandite in different fly ash-cement-water mixes was correlated to the reactivity of the given fly ashes. While a clear connection wasnot established, several …
-
Elucidating the Fresh and Hardened Properties of Limestone Calcined Clay Cements through Data Analytics
… Analytical measures (e.g., changes in portlandite and bound water contents over time) show how microstructural development translates to compressive strength and surface resistivity development. For instance, LC3 mortar strength over 28 days of hydration can be accurately predicted not …
-
Municipal solid waste incineration (MSWI) ashes for greener concrete
… to activate RISE BA (bottom ash) and STENA BA. Portlandite did not act as a good enough activator. The experiment results from the solution test showed that 𝑁𝑎𝑂𝐻 and 𝐾𝑂𝐻 activators added in order to reach a 𝑝𝐻 of 14, were able to activate RISE BA in addition to SLAG. However, STENA BA were still …
-
Spectroscopic Investigation of Cement Hydrate Phases and Their Chloride Binding Properties
… surface properties of the individual hydrates. Portlandite and AFm surfaces have high affinity for chloride due to their positive zeta-potentials. For C-S-H samples, the chloride binding capacity increases with increasing C/S ratio due to increased numbers of surface Ca-OH sites and decreased …
-
Experimental Investigation on the Behavior and Performance of Modified Cement Mortar made with Fly Ash, Hydrated Lime and Spent Garnet for Co2 Uptake: Influence of Carbonation Age
… samples, with a significant reduction in portlandite peaks in the mixes with HL, suggesting extensive carbonation. The results indicate that incorporating FA, HL, and SG not only uptake higher amount of CO2 but also enhances concrete performance, making it a viable solution for sustainable …
-
Reactions In the Microannulus of a Wellbore System with Produced Water from The Permian Basin
… show the predominate solids of bulk cement are, portlandite [Ca(OH)2], CaH4Si2O7 and brownmillerite [Ca2(Fe1.45Al0.55)O7]. The weight % content of these predominant solids remained unchanged, and the weight % content of periclase [MgO] increased with increasing reaction time. Flow measurements …