Global ETD Search

Search theses and dissertations gathered from participating repositories worldwide. Every result links back to the library that holds it. No account is needed.

Results

Showing 1 to 19 of 19 for “"Reactive Wetting"”.

  1. The role of surface topology on reactive wetting of SAC305 solder on Ag substrates

    Physical removal of material via grit paper is the most common method of preparing surfaces for soldering. Most researchers have shown that increased roughness improves solder spreading; however, what isn't fully known is which exact feature or features create the positive outcome. This research …

    whiterose Download PDF for The role of surface topology on reactive wetting of SAC305 solder on Ag substrates (opens in a new tab)

  2. Selective Oxidation and Reactive Wetting of 2Mn-Si Steels During Continuous Hot-Dip Galvanizing

    … annealing time, on the selective oxidation and reactive wetting of Fe-0.1C-2Mn-1.3Si (wt.%) and Fe-0.1C-2Mn-1.7Si (wt.%) advanced high strength steels during continuous galvanizing was investigated. The effect of the addition of 0.05 wt.% Sn on the selective oxidation and reactive wetting of the …

    mcmaster Repository record for Selective Oxidation and Reactive Wetting of 2Mn-Si Steels During Continuous Hot-Dip Galvanizing (opens in a new tab)

  3. Parallel molecular dynamics simulations of dynamics of oxidation and reactive wetting in metal/ceramic systems

    … of a flat aluminum (111) surface and the reactive wetting of the aluminum (Al) droplet on a flat alumina (α-Al2O3) surface are investigated by using parallel molecular-dynamics simulations with dynamic charge transfer among atoms on a microscopic length scale. The interatomic potential, …

    lsu-thes Repository record for Parallel molecular dynamics simulations of dynamics of oxidation and reactive wetting in metal/ceramic systems (opens in a new tab)

  4. EFFECT OF Sb-MICRO ADDITIONS ON THE OXIDATION KINETICS AND REACTIVE WETTING OF ADVANCED HIGH-STRENGTH STEELS

    … the substrate surface can negatively impact reactive wetting, coating adhesion, and overall coating quality. In this study, the selective oxidation kinetics and reactive wetting of a series of Fe-(2-10)Mn-(0.00/0.01/0.03)Sb (at. pct) were determined and a model was proposed for analyzing …

    mcmaster Repository record for EFFECT OF Sb-MICRO ADDITIONS ON THE OXIDATION KINETICS AND REACTIVE WETTING OF ADVANCED HIGH-STRENGTH STEELS (opens in a new tab)

  5. The effect of Sn microalloying on the selective oxidation kinetics and reactive wetting of advanced high strength steels

    … N2-H2-H2O process atmosphere are detrimental to reactive wetting. Microalloying with 0.01 and 0.03 at.% Sn was evaluated as strategy to decrease selective oxidation kinetics and enhance reactive wetting of Fe-(6-10)Mn (at.%) alloys. During annealing, Sn segregated to grain boundaries, metal/oxide …

    mcmaster Repository record for The effect of Sn microalloying on the selective oxidation kinetics and reactive wetting of advanced high strength steels (opens in a new tab)

  6. SELECTIVE OXIDATION AND REACTIVE WETTING OF FE-0.1C-6MN-2SI-xSN ADVANCED HIGH STRENGTH STEELS DURING CONTINUOUS HOT-DIP GALVANIZING

    … surface by these oxides is detrimental to reactive wetting, good coating adhesion and integrity. Simulated galvanizing treatments were conducted on two prototype Fe-0.1C-6Mn-2Si (wt pct) 3G steels; one as the reference steel and the other with 0.05 wt pct Sn added to the composition. The …

    mcmaster Repository record for SELECTIVE OXIDATION AND REACTIVE WETTING OF FE-0.1C-6MN-2SI-xSN ADVANCED HIGH STRENGTH STEELS DURING CONTINUOUS HOT-DIP GALVANIZING (opens in a new tab)

  7. Selective oxidation and reactive wetting of an Fe-0.15C-5.5Mn-1.17Si-1Al advanced high strength steel (AHSS) during hot-dip galvanizing

    … annealing time, on the selective oxidation and reactive wetting of an Fe-0.15C-5.56Mn-1.17Si-1Al (wt%) prototype 3G AHSS during intercritical annealing as well as continuous galvanizing. Simulated annealing and galvanizing were conducted on the prototype Fe-0.15C-5.56Mn-0117Si-1Al (wt%) 3G …

    mcmaster Repository record for Selective oxidation and reactive wetting of an Fe-0.15C-5.5Mn-1.17Si-1Al advanced high strength steel (AHSS) during hot-dip galvanizing (opens in a new tab)

  8. Coating of High Strength Steels with a Zn-1.6Al-1.6Mg Bath

    … contri- bution, the selective oxidation and reactive wetting of a series of C-Mn AHSS were determined with the objective of providing a quantitative description of this pro- cess. The process atmosphere pO2 was varied using dew points of −50◦C, −30◦C and −5◦C. The surface oxide chemistry and …

    mcmaster Repository record for Coating of High Strength Steels with a Zn-1.6Al-1.6Mg Bath (opens in a new tab)

  9. Mechanical Property Development and Galvanizing of a Medium-Mn Third-Generation Advanced High Strength Steel

    … alloying elements during annealing can prevent reactive wetting of the substrate by the galvanizing bath. The conflicting objectives of achieving the desired mechanical properties and high-quality galvanized coatings were addressed in this work on a prototype 0.15C-5.6Mn-1.9Al-1.1Si (wt%) steel. …

    mcmaster Repository record for Mechanical Property Development and Galvanizing of a Medium-Mn Third-Generation Advanced High Strength Steel (opens in a new tab)

  10. Understanding hydrogen permeation through molten metal alloy membranes

    … membrane apparatus were challenged due to poor wetting of the top candidates identified on quartz. In order to investigate this, wetting of copper-bismuth alloys to porous substrates was evaluated. Non-reactive wetting of Cu₀.₀₃Bi₀.₉₇ and Cu₀.₀₃Sn₀.₉₇ to porous quartz substrate exhibited contact …

    ubc Repository record for Understanding hydrogen permeation through molten metal alloy membranes (opens in a new tab) Download PDF for Understanding hydrogen permeation through molten metal alloy membranes (opens in a new tab)

  11. Kinetics of corrosion and dross build-up in molten Zn-Al systems.

    … (3) clarify the reactive wetting behaviors of both metallic and composite materials in contact with molten Zn/Al alloy; (4) develop and apply electrochemical methods as effective research tools for the study of in-situ behavior of molten metal instant corrosion …

    wvu Repository record for Kinetics of corrosion and dross build-up in molten Zn-Al systems. (opens in a new tab)

  12. Mechanical Property Development, Selective Oxidation, and Galvanizing of Medium-Mn Third Generation Advanced High Strength Steel

    … high-quality galvanized coatings via enhanced reactive wetting. It was found that the starting microstructure, intercritical annealing (IA) time/temperature, and Sn micro-alloying had a significant effect on the retained austenite volume fraction and stability and, thereby, the mechanical …

    mcmaster Repository record for Mechanical Property Development, Selective Oxidation, and Galvanizing of Medium-Mn Third Generation Advanced High Strength Steel (opens in a new tab)

  13. SHORT-TERM FORMATION KINETICS OF THE CONTINUOUS GALVANIZING INTERFACIAL LAYER ON MN-CONTAINING STEELS

    … line annealing atmospheres. This can deteriorate reactive wetting by the liquid Zn(Al,Fe) alloy during galvanizing and prevent the formation of a well developed Fe-Al interfacial layer at the coating/substrate interface, resulting in poor zinc coating adherence and formability. However, despite Mn …

    mcmaster Repository record for SHORT-TERM FORMATION KINETICS OF THE CONTINUOUS GALVANIZING INTERFACIAL LAYER ON MN-CONTAINING STEELS (opens in a new tab)

  14. Galvanization of Al-Si Trip-Assisted Steels

    … oxygen partial pressure on oxidation and reactive wetting during galvanizing was determined for four TRIP-assisted steels having varied Si and Al contents. Three different process atmospheres were studied for each alloy: a -53 °C dew point (dp) or-50 °C dp with N2 -20% H2 , a -30 °C dp …

    mcmaster Repository record for Galvanization of Al-Si Trip-Assisted Steels (opens in a new tab)

  15. Surface modification of ceramic and metallic alloy substrates by laser raster-scanning

    … from 350 to 500 J/cm2 . In Process (b), complete reactive wetting of carbon-carbon composite cylinders surface was achieved by laser melting a Si-Cr-Hf-C slurry. Coatings showed good thermal stability at 1000ºC in argon, and, when tested in air, a percent weight reduction rate of -6.5 wt.%/hr was …

    texas Repository record for Surface modification of ceramic and metallic alloy substrates by laser raster-scanning (opens in a new tab)

  16. Effect of surface condition on resistance spot welding of advanced high strength steel

    … to the Zn pool via the enhancement of the reactive wetting. The presence of these internal oxides has shown to shift the weld lobe to higher currents, increasing the time required to generate an acceptable weld. Study of weld development showed that surface melting is responsible for this …

    waterloo Repository record for Effect of surface condition on resistance spot welding of advanced high strength steel (opens in a new tab)

  17. Thermo-Mechanical Characterization and Interfacial Thermal Resistance Studies of Chemically Modified Carbon Nanotube Thermal Interface Material - Experimental and Mechanistic Approaches

    … into eutectic gallium indium liquid metal (LM) wetting matrix. Thermal conductivity data from Infrared microscopy tool reveals the dependence of experimental factors such as matrix types, TIM contacting interfaces, orientation of CNTs and wetting of CNTs in the matrix on the thermal behavior of …

    arizona-thes Repository record for Thermo-Mechanical Characterization and Interfacial Thermal Resistance Studies of Chemically Modified Carbon Nanotube Thermal Interface Material - Experimental and Mechanistic Approaches (opens in a new tab)

  18. High-temperature interactions of molten Ti-Al, Ni-Al and Ni-B alloys with TiB2 ceramic

    … reaktiven Benetzen (engl. dissolutive, reactive wetting) auf der Ni-reichen Seite zu einem nicht-reaktiven Benetzen auf der Al-reichen Seite. Die Ergebnisse deuten darauf hin, dass der Ni-Gehalt in Ni-Al Legierungen eine Hauptursache für die Veränderungen der Substratauflösung und der …

    qucosa-diss