Solidification Behavior and Hot Cracking Susceptibility of High Manganese Steel Weld Metals
… other cryogenic materials (9Ni steel, Invar, 304 SS, etc.) which are commonly used during the construction of liquefied natural gas (LNG) tanks. The proposed steel alloys contain Mn levels in the range of 20 to 28 wt% and C additions on the order of 0.4 wt%. Although austenite stability is …
-
Evaluation of the Effect of Tungsten and Boron Additions on the Microstructure and Solidification Cracking Susceptibility of Fe-Mn-C Filler Metals
… the Single-Sensor Differential Thermal Analysis (SS-DTA™) technique. Metallurgical characterization was carried out using both optical microscopy, and scanning electron microscopy. The objective of this study was to determine the optimum range of tungsten and boron additions within the …
-
Analysis of Nickel Aluminum Bronze Weld Metal Microstructure and Mechanical Response as a Function of Cooling Rate
… bronze (NAB) is a copper-based alloy used across a range of industries, including marine, aerospace, architecture, offshore oil and gas, and petrochemical sectors. Traditionally, large NAB components have been fabricated via casting; however, the industry is steadily shifting toward additive …
-
Weldability Evaluation in Autogenous Welds of Alloys 230, 800H, and 825
… to solidification cracking and stress relief cracking in Alloys 800H, 825, and 230. To evaluate the solidification behavior and solidification cracking susceptibility in these alloys, the Cast Pin Tear Test (CPTT), thermodynamic simulations with Thermo-Calc, and the technique of …
-
An investigation of reheat cracking in the weld heat affected zone of type 347 stainless steel
… for many alloys such as the stabilized stainless steels: Types 321 and 347 and Cr-Mo-V steels as well as Ni-base superalloys termed “strain-age cracking”. Cracking occurs during PWHT at the HAZ. Many investigations have been conducted on the RHC with still no comprehensive theory to explain …
-
Intermediate temperature grain boundary embrittlement in nickel-base weld metals
… and single sensor differential thermal analysis (SS-DTA) to develop a better understanding of how carbide precipitation affects grain boundary locking and the mechanism for DDC. Macroscopic grain boundary locking occurs in alloys that form intragranular precipitates at the end of solidification. …
-
Development of a Coating Formulation Procedure for Ni-base Shielded Metal Arc Electrodes with Varying Core Wire Composition
… as well as flexibility in the manufacturing process. Nickel base welding consumables often require specialized chemical compositions which are more stringent than the requirements for the base material on which they are welded. To complicate this problem further, the core wire chemistry often has …
-
Physical Simulation of Friction Stir Processed TI-5Al-1Sn-1Zr-1V-0.8Mo
<p>Friction stir processing (FSP) can be employed to modify the grain size and microstructure of a material. In titanium alloys, the refined microstructure achieved during processing can improve the mechanical properties, such as yield stress and fatigue crack initiation resistance. Documenting the …
-
Development of Predictive Formulae for the A1 Temperature in Creep Strength Enhanced Ferritic Steels
… steels P91 and P92 are extensively used in fossil supercritical power plants due to their improved creep strength at elevated temperatures. Loss of creep strength and/or toughness may occur in CSEF steel welds due to formation of fresh martensite, ferrite, or retained austenite during welding …
-
Characterization of the Response to Tempering and Development of Predictive Formula for A1 Temperature in Grade 91 Weld Metal
… resistance, even at high temperatures. Recent issues have developed however, in which premature failure due to creep can shorten the life of the steel. This is often attributed to improper post weld heat treatments in which the A1 temperature of the steel is exceeded, causing creep strength and …
-
Girth Welding of Internally Clad API 5L Grade X65 Pipes using Low Alloy Steel Filler Metal
… of alloy 625 overlays on high-strength steel (HSS) has been reported in works pertaining to the oil and gas, petrochemical, and power generation industries. Extensive investigations have been conducted analyzing microstructural and compositional gradients along the fusion boundary and transition …
-
Optimal Composition Window of Type 410 Welding Consumables and Base Metals for Hydro-processing Applications
… the petrochemical industry, martensitic stainless steels are primarily selected over the more expensive austenitic stainless steels for their increased hardenability and resistance to halide stress corrosion cracking. Recently, unexpected high hardness and a loss of toughness has been …
-
Microstructural Evolution and Mechanical Properties in Simulated Heat Affected Zone Regions of Grade 91 Steel Welds
… single sensor differential thermal analysis (SS-DTA) and in-situ XRD measurements were used to determine the phase transformations at occur during simulation of weld thermal histories. From these measurements, ferrite was shown to form on cooling from peak temperatures within the ICHAZ …
-
Phase Transformation Behavior and Hydrogen Cracking Susceptibility in Grade T23 and T24 Steel Welds
Cracking in water walls of newly built fossil power plants using Grade T23 and T24 steels has halted service. The cause for this cracking is still undetermined, and one possible mechanism is hydrogen assisted cracking (HAC). The goal of this research was to compare the susceptibility to HAC in …