Global ETD Search

Search theses and dissertations gathered from participating repositories worldwide. Every result links back to the library that holds it. No account is needed.

Results 1 to 11 of 11 for “"Seam weld"”

  1. The Susceptibility of Electric Resistance Welded Line Pipe to Selective Seam Weld Corrosion

    Selective seam weld corrosion (SSWC) is a localized corrosion phenomenon and an integrity threat to pipelines consisting of electric resistance welded (ERW) line pipe. Due to the typical morphology of SSWC, the corrosion anomalies associated with the mechanism are difficult to detect with currently …

    ohiolink Repository record for The Susceptibility of Electric Resistance Welded Line Pipe to Selective Seam Weld Corrosion (opens in a new tab)

  2. Effect of Bridge Geometry on Seam Weld Microstructures in AA6xxx Aluminum Porthole Die Extrusions

    … the influence of die geometry (bridge shape and welding chamber height), extrusion process parameters (ram speed) on the weld seam formation of the extrudate and its tensile properties in the natural aged (T4) and artificially aged (T5 and T6) conditions. In addition, a mathematical model was …

    waterloo Repository record for Effect of Bridge Geometry on Seam Weld Microstructures in AA6xxx Aluminum Porthole Die Extrusions (opens in a new tab)

  3. Burst Pressure Prediction for Pipelines with Selective Seam Weld Corrosion Using Experimental Validation, Finite Element Analysis, and Physics-Guided Modeling

    Selective Seam Weld Corrosion (SSWC) is a localized corrosion mechanism that preferentially attacks the seam weld region of pipelines and often produces narrow groove-like or wedge-shaped defects. Unlike general metal-loss corrosion, SSWC can behave as a notch-like feature, where the defect vertex …

    houston Repository record for Burst Pressure Prediction for Pipelines with Selective Seam Weld Corrosion Using Experimental Validation, Finite Element Analysis, and Physics-Guided Modeling (opens in a new tab) Embargoed until 2028-08-01

  4. Weld Seam Properties of TRIP 690 tubes

    Production of seam welded, and roll formed tubes have been a core part of hydroformed automotive structural components. With the emergence of Advanced High Strength Steels (AHSS), most automotive companies are shifting from conventional steels to AHSS for vehicle light weighting considerations. …

    guelph Repository record for Weld Seam Properties of TRIP 690 tubes (opens in a new tab)

  5. Prediction and control of residual stresses and distortion in HY-130 thick pipe weldments

    … techniques for computer simulation of the welding process, an experiment is designed and carried out in which seam and girth weld are produced on a high strength steel cylinder. Fabrication of the HY-130 cylinder, selection of welding parameters for the seam and girth welds, and the …

    nps Repository record for Prediction and control of residual stresses and distortion in HY-130 thick pipe weldments (opens in a new tab)

  6. Tube equal channel angular extrusion as a novel severe plastic deformation technique for Mg-3Al-1Zn alloy and pure niobium

    … tube manufacturing processes involve either a seamless tube production method using high temperature extrusion which results in a large, non-uniform grain size or production of tubes that are seam welded after extrusion through a porthole or spider die. Welded regions are often the weak part of …

    tamu Repository record for Tube equal channel angular extrusion as a novel severe plastic deformation technique for Mg-3Al-1Zn alloy and pure niobium (opens in a new tab)

  7. Instrumented impact testing and its application to the study of acicular ferrite steels

    … Tests also revealed that sites near the seam weld of the pipe made with that semi-killed steel had experienced sufficient pipe-forming strain and thermal energy from the welding process to exhibit strain age effects. The fully killed acicular ferrite steel did not strain age; its strength …

    ubc Repository record for Instrumented impact testing and its application to the study of acicular ferrite steels (opens in a new tab)

  8. Effect of graphitization on the static mechanical properties of service exposed ASTM A516 Gr. 65 steam pipe metal

    … on three graphitized service exposed steam pipe weldment samples and on a newly welded and post weld heat treated sample with graphitized service exposed steam pipe material. Macro samples were removed from each of the samples at two positions and these were evaluated with regard to graphite …

    nmmu Repository record for Effect of graphitization on the static mechanical properties of service exposed ASTM A516 Gr. 65 steam pipe metal (opens in a new tab)

  9. Transmission laser micro-welding of preheated glass substrates

    … of the respective application. Laser glass welding is a technique for joining surfaces without using an intermediate layer. Generally, the technology can be used to weld a transparent material to a transparent or non-transparent material such as glass-to-glass, glass-to-ceramic and …

    ksu Repository record for Transmission laser micro-welding of preheated glass substrates (opens in a new tab)

  10. Caractérisation rapide des propriétés à la fatigue à grand nombre de cycle des assemblages métalliques soudés de type automobile : vers une nouvelle approche basée sur des mesures thermométriques

    Malgré plusieurs décennies d'études expérimentales et numériques sur la tenue en fatigue d'assemblages soudés, cette problématique demeure une préoccupation principale de l'industrie automobile. En effet, de nombreux composants aux géométries complexes (e.g. berceaux) sont obtenus à partir de …

    star-france Repository record for Caractérisation rapide des propriétés à la fatigue à grand nombre de cycle des assemblages métalliques soudés de type automobile : vers une nouvelle approche basée sur des mesures thermométriques (opens in a new tab)

  11. DEVELOPING A DESIGN METHODOLOGY FOR REINFORCING CRACK-LIKE DEFECTS IN THE LONGITUDINAL ELECTRONIC RESISTANCE WELDED SEAMS OF TRANSMISSION PIPELINES

    … 1920 and 1970 were typically constructed using a welding process known as electronic resistance welding, or ERW. At the time, this welding process was susceptible to multiple quality control problems which created small inclusions and flaws at the longitudinal weld seam at the time of manufacture. …

    tamu Repository record for DEVELOPING A DESIGN METHODOLOGY FOR REINFORCING CRACK-LIKE DEFECTS IN THE LONGITUDINAL ELECTRONIC RESISTANCE WELDED SEAMS OF TRANSMISSION PIPELINES (opens in a new tab)