  1. Metal-Mold Reactions in CMSX-4 Single Crystal Superalloy Castings

    … are often found on the surface of as-cast CMSX-4 single-crystal alloy parts. These layers cannot be removed prior to solution heat treatment of cast parts because of the sensitivity of the single-crystal castings to recrystallization (RX) defect formation. Removal of the reaction layer after …

    unr Repository record for Metal-Mold Reactions in CMSX-4 Single Crystal Superalloy Castings (opens in a new tab)

  2. MHigh temperature oxidation behaviour of the single crystal superalloy CMSX-10

    … achieve higher efficiency. The compositions of superalloys used in the critical components of engines are changing to improve their high temperature capabilities. Historically, efforts in improving the performance of superalloys, in general, have been focused only on the mechanical properties; …

    ubc Repository record for MHigh temperature oxidation behaviour of the single crystal superalloy CMSX-10 (opens in a new tab) Download PDF for MHigh temperature oxidation behaviour of the single crystal superalloy CMSX-10 (opens in a new tab)

  3. Study of back-diffusion in the nickel-base single crystal superalloy RR-2100

    Nickel-base superalloys have been an topic of active research for over five decades and the findings from various researchers worldwide have had a direct impact not only on different areas of materials science but also on applications thereof, in particular the aircraft industry, i.e. the …

    ubc Repository record for Study of back-diffusion in the nickel-base single crystal superalloy RR-2100 (opens in a new tab) Download PDF for Study of back-diffusion in the nickel-base single crystal superalloy RR-2100 (opens in a new tab)

  4. Characterization and modeling of thermo-mechanical fatigue crack growth in a single crystal superalloy

    … the thermo-mechanical fatigue crack behavior in single crystal superalloys is crucial to accurately evaluate component life to ensure reliable operations without blade fracture through the use of "retirement for cause" (RFC). This research was conducted on PWA1484, a single crystal superalloy …

    gatech Repository record for Characterization and modeling of thermo-mechanical fatigue crack growth in a single crystal superalloy (opens in a new tab)

  5. Void Growth and Collapse in a Creeping Single Crystal

    … In particular, the understanding of creep in single crystal superalloy turbine blades is of importance for designing more reliable and fuel efficient aircraft engines. Creep tests on single crystal superalloy specimens have shown greater creep strain rates for thinner specimens than predicted …

    unt Repository record for Void Growth and Collapse in a Creeping Single Crystal (opens in a new tab)

  6. Molecular Dynamics Study of Creep Deformation in Nickel-based Superalloy

    … molecular dynamics simulations of Ni-based superalloy to investigate the creep behavior under uniaxial compression test. Dislocation dynamics is analyzed for the nickel-based single crystal superalloy with the presence of void and with varying the distribution of gamma-prime phase The …

    mo-state Repository record for Molecular Dynamics Study of Creep Deformation in Nickel-based Superalloy (opens in a new tab)

  7. Thermomechanical fatigue crack formation in a single crystal Ni-base superalloy

    … determination model for the second generation single crystal superalloy PWA 1484 experiencing out-of-phase thermomechanical fatigue (TMF). The life model was developed as a result of a combination of critical mechanical tests, dominant damage characterization and utilization of well-established …

    gatech Repository record for Thermomechanical fatigue crack formation in a single crystal Ni-base superalloy (opens in a new tab)

  8. Effects of specimen geometry and coating on the thermo-mechanical fatigue of PWA 1484 superalloy

    The single crystal superalloy PWA 1484 is used in hot section turbine blade applications due to its performance at high temperatures. In practice, the turbine blades are often coated in order to protect them from environmental degradation. However, under repeated cyclic loading, the coating may …

    gatech Repository record for Effects of specimen geometry and coating on the thermo-mechanical fatigue of PWA 1484 superalloy (opens in a new tab)

  9. Creep and fatigue of a single crystal nickel base superalloy

    The introduction of single crystal casting techniques has led to the development of existing nickel-base superalloys to produce materials with optimum mechanical properties in the single crystal condition. As single crystals are known to be anisotropic, a study is needed to determine the general …

    aston Download PDF for Creep and fatigue of a single crystal nickel base superalloy (opens in a new tab)

  10. Effect of anisotropy on the mechanical testing of Ni-based single-crystal superalloys

    … extent to which this can be achieved. Ni-based single-crystal superalloys, renowned for retaining their high yield strengths at extreme temperatures, have been created to break these boundaries. In this thesis, we investigate the mechanical properties of the Ni-based single-crystal superalloy …

    oxford Repository record for Effect of anisotropy on the mechanical testing of Ni-based single-crystal superalloys (opens in a new tab)

  11. Fracture studies in superalloys

    … <p>The crack propagation characteristics of a single crystal superalloy have been investigated at various temperatures and frequencies. Determination of the fatigue crack propagation rates was combined with the measurement of crack tip plastic zone sizes and observation of the deformation …

    oxford Repository record for Fracture studies in superalloys (opens in a new tab)

  12. Instabilities on High Temperature Isothermal Creep Performance in Ni-Based Single Crystal Superalloys

    Nickel-based singe crystal superalloys are a class of metallic materials with a combination of high-temperature strength, toughness, and resistance to degradation in oxidizing environments, which makes them great candidates for aircraft engine turbine blades that operate at temperatures beyond 1000 …

    tamu Repository record for Instabilities on High Temperature Isothermal Creep Performance in Ni-Based Single Crystal Superalloys (opens in a new tab)

  13. Segregation-assisted creep in nickel-based superalloys: experiments, theory and modelling

    … 850°C is assuming greater importance in Ni-based superalloys. This is because the design operating temperature of the combustion cycle is increasing as the new generations turbofan engines become more efficient. The temperature at the rim of turbine disks and the root of turbine blades can be in …

    oxford Repository record for Segregation-assisted creep in nickel-based superalloys: experiments, theory and modelling (opens in a new tab)

  14. Development of In-situ Nanocrystalline NiCoCrAlTaY Coatings by Cold Spray on a Single-Crystal Nickel-base Superalloy for Gas Turbine Applications

    … research is to characterize CS deposition on a single-crystal nickel-base superalloy and to develop low-cost/high-performance NiCoCrAlTaY coatings using the CS technique. Several individual studies were carried out with each having a specific focus towards achieving the general research …

    ottawa-retro Repository record for Development of In-situ Nanocrystalline NiCoCrAlTaY Coatings by Cold Spray on a Single-Crystal Nickel-base Superalloy for Gas Turbine Applications (opens in a new tab)

  15. Dislocation Microstructure and Surface Roughness Evolution in Single and Multi-phase Microcrystals

    … the evolution of complex dislocation networks in crystals having arbitrary microstructures and initial defect distributions, and under different loading conditions. In this thesis, a DDD framework has been developed and utilized to investigate the evolution of dislocation microstructures and …

    jhu Repository record for Dislocation Microstructure and Surface Roughness Evolution in Single and Multi-phase Microcrystals (opens in a new tab)

  16. Microstructural Instabilities in Nickel-based Single Crystal Superalloys

    Single crystal superalloys, mostly Nickel-based, have been, so far, the material of choice for high-temperature applications, such as gas turbine blades. Single crystalline turbine blades are usually cast in the direction, providing the best combination of properties. While misorientations up to …

    tamu Repository record for Microstructural Instabilities in Nickel-based Single Crystal Superalloys (opens in a new tab)