Global ETD Search

Search theses and dissertations gathered from participating repositories worldwide. Every result links back to the library that holds it. No account is needed.

Results 1 to 20 of 60 for “"Slow Crack Growth"”

  1. An Assessment of Slow Crack Growth in Leucite-Reinforced Ceramics

    Purpose: To assess the slow crack growth parameters of a leucite-reinforced dental ceramic under constant stress rate condition and determine the influence of the environment and surface finish on the resulting parameters. Materials & methods: 130 ceramic plates (Pro-CAD, Ivoclar Vivadent, Schaan, …

    ohiolink Repository record for An Assessment of Slow Crack Growth in Leucite-Reinforced Ceramics (opens in a new tab)

  2. Slow crack growth and associated plastic deformation in linear medium-density polyethylene

    Since the introduction of polyethylene (PE) pipe for use in natural gas distribution about twenty years ago, nearly one billion feet of various grades have been installed in North America. Now more than 80% of all pipe installed for natural gas distribution is made of PE, and this percentage is …

    uiuc Repository record for Slow crack growth and associated plastic deformation in linear medium-density polyethylene (opens in a new tab)

  3. Hydrogen Transport and Hydrogen Embrittlement in Stainless Steels (Diffusion, Permeation, Solubility, Slow Crack Growth)

    … the kinetics of gaseous hydrogen-induced slow crack growth (SCG) in metastable austenitic stainless steels, hydrogen permeation and/or cracking velocity were measured and compared for three types of stainless steels. These included austenitic, ferritic, and duplex ((gamma)/(alpha)) alloys. …

    uiuc Repository record for Hydrogen Transport and Hydrogen Embrittlement in Stainless Steels (Diffusion, Permeation, Solubility, Slow Crack Growth) (opens in a new tab)

  4. Studium vztahu mezi vnitřní strukturou HDPE a odolností vůči rychlosti šíření trhliny SCG (Slow Crack Growth)

    Diplomová práce se zabývá vztahy mezi vnitřní strukturou a odolností proti křehkému lomu mechanismem pomalého růstu trhliny (SCG) v HDPE. V teoretické části jsou shrnuty doposud známé poznatky o přípravě PE a vztahu mezi vnitřní strukturou a odolností proti šíření SCG. V experimentální části byly …

    brno-tech Repository record for Studium vztahu mezi vnitřní strukturou HDPE a odolností vůči rychlosti šíření trhliny SCG (Slow Crack Growth) (opens in a new tab)

  5. Studium vztahu mezi podmínkami testu FNCT (Full Notched Creep) a rychlostí šíření trhliny SCG (Slow Crack Growth) pro hodnocení odolnosti HDPE vůči růstu trhlin

    Teoretická časť predstavuje súhrn materiálových a testovacích parametrov ovplyvňujúcich priebeh SCG a následne aj dĺžku trvania FNCT testu. Experimentálna časť sa zameriava na modifikáciu podmienok FNCT testu s cieľom maximálneho zníženia času do lomu skúšaného materiálu. Pre vybrané 4 druhy …

    brno-tech Repository record for Studium vztahu mezi podmínkami testu FNCT (Full Notched Creep) a rychlostí šíření trhliny SCG (Slow Crack Growth) pro hodnocení odolnosti HDPE vůči růstu trhlin (opens in a new tab)

  6. Static fatigue of graphite

    Subcritical crack growth has been studied in two different grades of a fine-grained isotropic graphite and in pyrolytic graphite. The double torsion technique was used. Room temperature tests revealed a stress intensity-crack velocity behaviour similar to the third stage of crack growth in …

    ubc Repository record for Static fatigue of graphite (opens in a new tab)

  7. High temperature fatigue and creep deformation behavior under static and cyclic loading in ceramics containing a viscous grain boundary phase

    … At high stresses, fracture was dictated by slow growth of a single dominant flaw along the grain boundaries; at low stresses fracture occurred due to the nucleation, growth and linkage of multiple macrocracks. In the stress range used in the fatigue experiments, fracture under cyclic loading …

    uiuc Repository record for High temperature fatigue and creep deformation behavior under static and cyclic loading in ceramics containing a viscous grain boundary phase (opens in a new tab)

  8. Effects of Post-Treatment Abrasion on Dynamic Fatigue of Chemically Strengthened Glass

    … rate on strengths were also plotted, and the slow crack growth constant (n) was determined for each combination of ion exchange time and post-abrasion. Results indicate that the surface stresses induced by chemical strengthening reduces effects of stress-induced slow crack growth. However, …

    alfred Repository record for Effects of Post-Treatment Abrasion on Dynamic Fatigue of Chemically Strengthened Glass (opens in a new tab)

  9. Investigation of the work hardening characteristics and fracture toughness of low alloy steels

    … the true work hardening rate decreased. Critical crack opening displacement (C.O.D.) values were deterlnined for all the alloys over the temperature range. The critical event was defined as the onset of slow crack growth, or fast fracture, whichever occurred first. Onset of slow crack growth was …

    strathclyde Repository record for Investigation of the work hardening characteristics and fracture toughness of low alloy steels (opens in a new tab)

  10. Evaluation of the Mechanical Properties of Solid Oxide Fuel Cell Materials

    … investigation, the strength distribution and Slow Crack Growth (SCG) behavior of a dense MMA manifold material and porous MMA tube material were evaluated via 4-point flexural testing at temperatures of 20°C, 50°C, and 850°C under wide range of environmental conditions involving exposure to …

    washington Repository record for Evaluation of the Mechanical Properties of Solid Oxide Fuel Cell Materials (opens in a new tab)

  11. An assessment of the fracture toughness of two cast and wrought stainless steels

    The crack-tip displacement concept has been applied to austenitic steels at 25°C and in the temperature range 400-800°C. The measurement of a maximum load crack-tip displacement in a notch bend test, provided a good indication of fracture-toughness since it included a portion of slot: crack-growth. …

    brunel Repository record for An assessment of the fracture toughness of two cast and wrought stainless steels (opens in a new tab)

Page 1 of 3