Global ETD Search

Search theses and dissertations gathered from participating repositories worldwide. Every result links back to the library that holds it. No account is needed.

Results

Showing 1 to 15 of 15 for “"Slow strain rate test"”.

  1. Environment-Induced Degradations in a Target Structural Material for Transmutation Applications

    … temperature. The results of constant load SCC testing using smooth specimens showed no failure in the neutral solution but a threshold stress of 97 ksi was observed in the 90°C acidic environment. SCC testing by the slow-strain-rate test method indicate that the time-to-failure, true failure …

    unlv Repository record for Environment-Induced Degradations in a Target Structural Material for Transmutation Applications (opens in a new tab) Download PDF for Environment-Induced Degradations in a Target Structural Material for Transmutation Applications (opens in a new tab)

  2. Hydrogen Effects on X80 Steel Mechanical Properties Measured by Tensile and Impact Testing

    … of hydrogen charging current density and tensile strain rate on the mechanical properties of X80 pipeline steel were investigated by slow strain rate test (SSRT), Charpy impact test, and scanning electron microscopy (SEM) in this thesis. The results show that both the ultimate tensile strength and …

    usf Repository record for Hydrogen Effects on X80 Steel Mechanical Properties Measured by Tensile and Impact Testing (opens in a new tab)

  3. Efeito do tratamento térmico de revenimento na fragilização pelo hidrogênio do aço 9% Ni em água do mar sintética e tiossulfato de sódio

    … seawater and sodium thiosulfate (Na2S2O3). The Slow Strain Rate Test (SSRT) results showed the effect of the environment in the toughness, elongation and rupture time in comparison with the result in the air at the same deformation rate, evidencing the embrittlement process of the 9% Ni steel. …

    brazil-uerj Repository record for Efeito do tratamento térmico de revenimento na fragilização pelo hidrogênio do aço 9% Ni em água do mar sintética e tiossulfato de sódio (opens in a new tab)

  4. The Effect of Hydrogen Sulfide on Hydrogen Permeation in High-strength Low-alloy Carbon Steel C110

    … that the hydrogen permeation process is accelerated by increasing H2S concentration, decreasing pH, and decreasing NaCl concentration. H2S improves the hydrogen permeation level either by accelerating the hydrogen reduction reaction or by catalyzing the hydrogen absorption. A hydrogen …

    tamu Repository record for The Effect of Hydrogen Sulfide on Hydrogen Permeation in High-strength Low-alloy Carbon Steel C110 (opens in a new tab)

  5. Hydrogen-Induced Damage in Additively Manufactured (AM) 316LN Stainless Steel and Glass-Fiber Reinforced Polypropylene for Hydrogen Transport

    … microscopy (SEM), optical microscopy (OM), and strain rate testing (SRT) to assess the damage to materials when hydrogen is introduced into their structure. In contrast, due to their non-conductive nature glass fiber-reinforced (GFRPP) composites, with 30% reinforcement each, were exposed to a …

    tamu Repository record for Hydrogen-Induced Damage in Additively Manufactured (AM) 316LN Stainless Steel and Glass-Fiber Reinforced Polypropylene for Hydrogen Transport (opens in a new tab) Embargoed until 2028-05-01

  6. Hydrogen-Induced Damage in Additively Manufactured (AM) 316LN Stainless Steel and Glass-Fiber Reinforced Polypropylene for Hydrogen Transport

    … microscopy (SEM), optical microscopy (OM), and strain rate testing (SRT) to assess the damage to materials when hydrogen is introduced into their structure. In contrast, due to their non-conductive nature glass fiber-reinforced (GFRPP) composites, with 30% reinforcement each, were exposed to a …

    tamu Repository record for Hydrogen-Induced Damage in Additively Manufactured (AM) 316LN Stainless Steel and Glass-Fiber Reinforced Polypropylene for Hydrogen Transport (opens in a new tab) Embargoed until 2028-05-01

  7. The tensile properties and toughness of microstructures relevant to the HAZ of X80 linepipe steel girth welds

    … the heat treated samples tensile and Kahn tear test specimens were made for testing at ambient, -20⁰C, and -60⁰C. The highest strength microstructure proved to be the finest, lower bainitic microstructure, while the lowest strength microstructure was the coarsest, upper bainitic sample …

    ubc Repository record for The tensile properties and toughness of microstructures relevant to the HAZ of X80 linepipe steel girth welds (opens in a new tab) Download PDF for The tensile properties and toughness of microstructures relevant to the HAZ of X80 linepipe steel girth welds (opens in a new tab)

  8. STRESS CORROSION CRACKING OF SELECTED AUSTENITIC AND DUPLEX STAINLESS STEELS IN POTASH BRINE ENVIRONMENT

    … UNS S32550) in relation to SCC damage in a saturated potash brine solution. The electrochemical corrosion behavior of these alloys in a chloride environment and their strain rate sensitivities were also investigated. SCC experiments were performed using the slow strain rate test technique …

    sask Repository record for STRESS CORROSION CRACKING OF SELECTED AUSTENITIC AND DUPLEX STAINLESS STEELS IN POTASH BRINE ENVIRONMENT (opens in a new tab)

  9. Effect of various deformation processes on the corrosion behavior of casing and tubing carbon steels in sweet environment, The

    … poorly in a corrosive environment in the slow strain rate test. The ductile material exhibited the highest loss in strength and highest susceptibility to stress corrosion cracking in a CO2-containing environment. The loss in strength declined with cold-rolling, which can be ascribed to the …

    colo-mines Repository record for Effect of various deformation processes on the corrosion behavior of casing and tubing carbon steels in sweet environment, The (opens in a new tab)

  10. Avaliação da influência do entalhe em corpos de prova ensaiados a baixa taxa de deformação em meio etanol

    O aumento de demanda por combustíveis menos poluentes e de fontes renováveis faz com que o Etanol se destaque como uma alternativa as fontes convencionais de energia. O crescente aumento no consumo deste produto, para os próximos anos, exigirá meios de transporte e estocagem eficientes e seguros, …

    brazil-ufrgs Repository record for Avaliação da influência do entalhe em corpos de prova ensaiados a baixa taxa de deformação em meio etanol (opens in a new tab)

  11. THE EFFECT OF GRAIN SIZE ON THE MECHANICAL PROPERTIES OF PIPELINE STEELS UNDER DIFFERENT ENVIRONMENTS

    … grain size was the primary variable, several tests were conducted in various media, including an electrochemical corrosion test, hydrogen permeation test, hydrogen-induced cracking (HIC) test, and slow strain rate test (SSRT). Following these tests, the microstructures of both untested and …

    sask Repository record for THE EFFECT OF GRAIN SIZE ON THE MECHANICAL PROPERTIES OF PIPELINE STEELS UNDER DIFFERENT ENVIRONMENTS (opens in a new tab)

  12. Stress corrosion cracking of X65 pipeline steel in fuel grade ethanol environments

    … accomplish this, a systematic study was done to test effects of FGE feedstock and common contaminants and constituents such as water, chloride, dissolved oxygen, and organic acids on SCC behavior of an X65 pipeline steel. Slow strain rate tests (SSRT) were employed to evaluate and compare …

    gatech Repository record for Stress corrosion cracking of X65 pipeline steel in fuel grade ethanol environments (opens in a new tab)

  13. A Novel Biodegradable Fe-35wt.%Mn Alloy Produced via Powder Metallurgy

    … However, as a fully dense alloy, the degradation rate was still not satisfactory. In this doctoral project, the Fe-35wt.%Mn alloys were produced via several PM routes. This research employed three different starting powders, which were blended elemental (BE), mechanically milled (MMed) and BE …

    auckland-ms Repository record for A Novel Biodegradable Fe-35wt.%Mn Alloy Produced via Powder Metallurgy (opens in a new tab)

  14. Effect of Thermal Ageing on the Corrosion and Stress Corrosion Cracking of Type 310S Stainless Steel in Supercritical Water

    … Potentiokinetic Reactivation (DL-EPR) testing, of three heat-treated materials studied is: SA ~ TT << S. The ranking reflects the controlling role played by Cr-depleted zones, which were only observed in the S material. The absence of a Cr-depleted zone accompanying the σ phase grain …

    mcmaster Repository record for Effect of Thermal Ageing on the Corrosion and Stress Corrosion Cracking of Type 310S Stainless Steel in Supercritical Water (opens in a new tab)

  15. Effect of Thermal Ageing on the Corrosion and Stress Corrosion Cracking of Type 310S Stainless Steel in Supercritical Water

    … Potentiokinetic Reactivation (DL-EPR) testing, of three heat-treated materials studied is: SA ~ TT << S. The ranking reflects the controlling role played by Cr-depleted zones, which were only observed in the S material. The absence of a Cr-depleted zone accompanying the σ phase grain …

    mcmaster Repository record for Effect of Thermal Ageing on the Corrosion and Stress Corrosion Cracking of Type 310S Stainless Steel in Supercritical Water (opens in a new tab)