Results 1 to 20 of 23 for “"Slurry erosion"”
-
Experimental Testing of an Electrical Submersible Pump Undergoing Abrasive Slurry Erosion
… flow, tandem compression type pump. Although the erosion of the pump diffuser and impeller stages are significant, the ESP study shows that the most sever failure is due to components that affect the pump’s rotor dynamics such as radial bearings and impeller seals when eroded with 100 mesh sand. …
-
Comprehensive study of the abrasive wear and slurry erosion behavior of an expanded system of high chromium cast iron and microstructural modification for enhanced wear resistance
… environments, where resistances to abrasion, erosion and erosion-corrosion are required. For instance, machinery and facilities used in mining and extraction in Alberta’s oil sands suffer from erosion and erosion-corrosion caused by silica-containing slurries, which create challenges for the …
-
A Preliminary Study of Slurry Pipeline Erosion Using a Toroid Wear Tester
Wear-related reliability issues, especially slurry erosion has become one of the principal concerns for the process industries that use slurry pipelines for coarse particle transport. The study and development of an appropriate wear model for slurry pipelines is, therefore, essential from the …
-
Three Phase Erosion Testing and Vibration Analysis of an Electrical Submersible Pump
… ESP equipment is facing a crucial problem of slurry erosion which may affect life and cost significantly. The wear caused by slurry erosion may bring the issue such as unbalanced side loads, severe vibration and decreased pressure head. Eventually, this phenomenon will lead to a complete …
-
Erosive wear mechanisms of rubber pump lining materials in minerals processing applications
Erosive slurry wear occurs extensively throughout minerals processing equipment for slurry transport applications. Wear resistant materials are designed to prolong the life of equipment used to transport the slurry such as pumps, hoses, grinders, conveyor belts, screens, etc. In this study, the …
-
Advanced surface engineering : evaluation of SprayStir
… MMC surfaces that demonstrated superior erosion performance than that of unreinforced substrate alloy. Throughout this study, SprayStir was applied to several coating and substrate combinations, and their respective erosion performance established through slurry erosion testing. The …
-
The tribological and wear properties of carbon-graphite composites
… using abrasive wear, dry sliding wear, particle erosion, slurry erosion, cavitation erosion and the corresponding wear rates have been related to the bulk properties of the different materials. In all tests; hardness, elastic modulus, porosity and the presence of fillers were found to influence …
-
Novel enhancement of HVOF thermal sprayed nanostructured WC-12Co / inconel-625 coatings for tribocorrosion applications
… affect coating performance, especially in erosion and corrosion preventive applications. The coating layer therefore must be enhanced with a view to reducing microstructural defects and thereby prolonging the coating’s service life. This research is aimed at examining the effect of using a …
-
Dependence of Wear and Corrosion Properties on the Electron Work Function
… thus the better performance in solid-particle erosion, slurry erosion and acid-medium corrosion tests. In sliding wear and neutral-medium corrosion tests, this correlation between EWF and material’s performance was concealed due to the influence of oxdiation. Using the relationship between EWF …
-
Investigating Sold Particle Erosion of Pipeline Material
… myriad of erosive conditions. The occurrence of erosion on a material surface is influenced by a considerable number of factors. Research has found that the impact of each contributing parameter varies based on the conditions. As such the field of erosion studies has been heavily reliant on …
-
A tribological study of a detonation gun coating of tungsten carbide for use in a subsea gate valve
… analysis has pointed to three-body abrasion, erosion and adhesion being the dominant failure modes and therefore, a suite of tribo-test methods have been developed to replicate them These are namely reciprocating diamond-on-flat, slurry erosion and reciprocating pin-on-plate tests. The …
-
Nitrocarbonetação eletrolítica à plasma em aço SAE 1045 : análise de mecanismos de desgaste por erosão-corrosão em meio aquoso – slurry
… desenvolvido e denominado Electrochemical Slurry Erosion Wear Test (ESEWT). Revestimentos Nitrocarburizados por Saturação Eletrolítica de Plasma (PEN/C) são obtidos por um processo de nitretação ou carbonitretação a plasma hidrostático de baixa temperatura e têm sido propostos para aumentar …
-
Flow Fields and Particle Trajectories in Abrasive Slurry-jet Micro-machining of Sintered Ceramics and Metallic-layered Structures
… difficult to machine them economically. Abrasive slurry-jet micro-machining (ASJM), in which a target is eroded by the impingement of a micro-jet of water containing fine abrasive particles, is a low-cost alternative for micro-machining of sintered ceramic materials without tool wear and thermal …
-
Erosion-corrosion of carbon steel and duplex stainless steel elbows in potash brine-sand slurry
… internal walls of these pipes are prone to erosion-corrosion damage, which can lead to product leakage and eventual failure of the piping system. The purpose of this research is to evaluate the performance of AISI 1018 carbon steel and AISI 2205 duplex stainless steel elbows to …
-
A particle erosion model of monocrystalline silicon for high heat flux microchannel heat exchangers
… exceed 20 m/s the potential for particle erosion becomes a significant reliability threat. While numerous particle erosion models exist, seldom are the velocities, particle sizes, materials and testing times in alignment with those present in embedded cooling systems. This research fills …
-
Revestimentos de WC-10CO-4CR obtidos por aspersão térmica (HVOF) sobre aço inoxidável martensítico visando melhorar a resistência à corrosão e a erosão
A geração de energia elétrica através de usinas hidrelétricas é ainda a maior fonte geradora de energia elétrica no Brasil, responsável por aproximadamente 59 % de toda a energia produzida. Neste contexto, são importantes alguns cuidados na manutenção destes grandes empreendimentos. Com isso, …
-
Investigation of Erosive Flow Injected Through Apertures into a Narrow Annulus
… solid particulates using liquids, forming a slurry. Those slurries conveyed in conduits generate erosion caused by particulate impingements on the walls. The erosive action of slurry may significantly reduce the service life of processing equipment, even at slow transport velocities. The …
-
Estudo comparativo do desgaste erosivo do tipo lama, do aço inox martensitíco AISI 410 com os revestimentos carbeto de tungstênio 86WC-10Co4Cr, obtido por HVOF e o elastômero PUR comercial
Na indústria hidrometalúrgica, diversos materiais são utilizados para a construção dos equipamentos, a fim de satisfazer as necessidades dos processos que estão sujeitos, tendo em conta a importância deles em condições complexas, tais como erosão e a corrosão. Neste trabalho é avaliado o …
-
Abrasive Wear Assessment of X70 Steel and Polyurethane Coupons on a Modified Dry/Sand Rubber Wheel Apparatus
… were conducted on X-70 steel to isolate erosion effects under wet conditions. Wear mechanisms in the materials under study were assessed through scanning electron microscopy analysis. In general, wear mechanisms such as cracking, pluck-out and indentations were observed with more or less …