Global ETD Search

Search theses and dissertations gathered from participating repositories worldwide. Every result links back to the library that holds it. No account is needed.

Results 1 to 20 of 22 for “"Sour environments"”

  1. Galvanic Interactions in Sweet and Sour Environments

    Corrosion of carbon steel exposed to aqueous environments containing dissolved carbon dioxide (CO2) and hydrogen sulfide (H2S) is responsible for many failures of equipment and pipelines in the oil and gas industry. Corrosion product films, e.g., iron carbonate (FeCO3) and iron sulfide (FexSy), …

    ohiolink Repository record for Galvanic Interactions in Sweet and Sour Environments (opens in a new tab)

  2. Initiation and Propagation of Localized Corrosion of Mild Steel in Marginally Sour Environments

    … of pitting failure of mild steel in marginally sour environments was performed with the objective of understanding and predicting the occurrence of localized corrosion. While localized corrosion can happen due to a variety of reasons, recent work has shown that mild steel was particularly …

    ohiolink Repository record for Initiation and Propagation of Localized Corrosion of Mild Steel in Marginally Sour Environments (opens in a new tab)

  3. Sulfide Stress Cracking Susceptibility of Low Alloy Steels for Casing Application in Sour Environments

    Sulfide stress cracking (SSC) resistance of casing steels with different alloying chemistries (i.e. Ti-B and Mn-Cr-Mo) was evaluated using constant load tensile test and slow strain rate test in NACE-TM0177 environment. SSC resistance in terms of RAH2S/RAair and time to failure was found to …

    alberta Repository record for Sulfide Stress Cracking Susceptibility of Low Alloy Steels for Casing Application in Sour Environments (opens in a new tab)

  4. Microstructure Optimization to Prevent Hydrogen-Induced Cracking of API X70 Pipeline Steels in Sour Environments

    … days, by increasing the demand for oil and gas resources, the failure of pipeline steels has become one of the crucial topics in the oil and gas transportation industry. The failure of pipeline steels is divided into two major categories: stress corrosion cracking (SCC) and hydrogen assistant …

    sask Repository record for Microstructure Optimization to Prevent Hydrogen-Induced Cracking of API X70 Pipeline Steels in Sour Environments (opens in a new tab)

  5. Effect of welding parameters on the susceptibility to hydrogen cracking in line pipe steels in sour environments

    … of welded steels used in petroleum lines under sour petroleum environments was investigated. The testing environment in NACE TM0284-2003 standard was used in order to simulate sour petroleum environment. In order to investigate behavior of welding parameters, used in pipe production, on HIC, …

    metu Repository record for Effect of welding parameters on the susceptibility to hydrogen cracking in line pipe steels in sour environments (opens in a new tab)

  6. Influência do tamanho de grão austenítico na resistência à corrosão sob tensão de aços para aplicação sour service

    … steels on sulfide stress corrosion cracking in sour environments with high H2S content. The base of the work will be two steels with a range of carbon equal a 0,24 and 0,34% containing chromium, molybdenum, vanadium, niobium and titanium. It wasvaried the heat treatment conditions to obtain …

    brazil-ufmg Repository record for Influência do tamanho de grão austenítico na resistência à corrosão sob tensão de aços para aplicação sour service (opens in a new tab)

  7. Top of the Line Corrosion in CO<sub>2</sub>/H<sub>2</sub>S Environments

    Top of the line (TLC) corrosion in sour (H<sub>2</sub>S) environments has not been well understood until now, since most reported TLC research has focused on sweet (CO<sub>2</sub>) conditions, with various models developed to predict corrosion rates and related phenomena in sweet systems. This has …

    ohiolink Repository record for Top of the Line Corrosion in CO<sub>2</sub>/H<sub>2</sub>S Environments (opens in a new tab)

  8. Electrochemical Degradation Behavior of Supermartensitic and Additively Manufactured Stainless Steels in CO2 and H2S Saturated Salt Brines for Oil and Gas Applications

    … and high corrosion resistance in moderately sour environments. However, discrepancies between their expected service limits and actual performance, especially in regions where failures were anticipated but did not occur, suggest a potential for false positive assessments of material …

    tamu Repository record for Electrochemical Degradation Behavior of Supermartensitic and Additively Manufactured Stainless Steels in CO2 and H2S Saturated Salt Brines for Oil and Gas Applications (opens in a new tab) Embargoed until 2026-12-01

  9. Mechanism and Modeling of Galvanic Corrosion Between Mild Steel and Iron Sulfidesin Acidic Solutions

    Sour hydrocarbon reservoirs, containing H2S gas, are receiving increasing attention due to the growing demand for energy. Although uniform corrosion is not a significant obstacle for oil and gas companies in sour environments, the major challenge in this field is prevention of localized corrosion …

    ohiolink Repository record for Mechanism and Modeling of Galvanic Corrosion Between Mild Steel and Iron Sulfidesin Acidic Solutions (opens in a new tab)

  10. Indicadores de patentes para o monitoramento tecnológico em aços para dutos utilizados em transporte de hidrocarbonetos

    … challenges such as low temperatures and acid environments demands innovative products and processes that, consequently, require research and development of new materials and processes. This study aimed to analyze the technological development of steel for hydrocarbons pipelines through the …

    brazil-ufscar Repository record for Indicadores de patentes para o monitoramento tecnológico em aços para dutos utilizados em transporte de hidrocarbonetos (opens in a new tab)

  11. Electrochemical study and corrosion modeling of chromium alloy steels exposed to sulfide containing environment

    … a metal or metal alloy and its environment in sour systems (H₂S dominant) has progressively become a greater concern to the oil and gas industry as a result of production from increasingly sour environments. In this study, the effects of the principal H₂S corrosion product, iron sulfide, on the …

    newfoundland Repository record for Electrochemical study and corrosion modeling of chromium alloy steels exposed to sulfide containing environment (opens in a new tab)

  12. Investigation of Localized Corrosion of Carbon Steel in H2S Environments

    … the localized corrosion of carbon steel, in sour systems (H2S dominant) has progressively become a greater concern to the oil and gas industry as a result of production from increasingly sour environments. In this study, the effects of chloride ion concentration on the localized H2S corrosion …

    ohiolink Repository record for Investigation of Localized Corrosion of Carbon Steel in H2S Environments (opens in a new tab)

  13. Evaluation of EDTA and GLDA Corrosion on S13Cr-110 Metal Alloy at High Temperature and High Pressure With and Without Salt

    … at high temperatures (>200°F) in more corrosive environments, both stimulation fluids and well tubing metallurgies have changed. Traditional well stimulation fluids such as HCl have been replaced by chelating agents such as ethylene diamine tetra-acetic acid (EDTA). In offshore environments, …

    tamu Repository record for Evaluation of EDTA and GLDA Corrosion on S13Cr-110 Metal Alloy at High Temperature and High Pressure With and Without Salt (opens in a new tab)

  14. Estudo da difusibilidade e solubilidade do hidrogênio no aço inoxidável bifásico martensítico-ferrítico

    … demands materials capable of performing in sour environments with low pH, presence of chlorides, pressure of H2S and protonic hydrogen. They must be resistant to corrosion and embrittlement by hydrogen. The ferritic-martensitic stainless steel was developed from the supermartensitic steel, …

    brazil-uerj Repository record for Estudo da difusibilidade e solubilidade do hidrogênio no aço inoxidável bifásico martensítico-ferrítico (opens in a new tab)

  15. Caracterização avançada de aços microligados de baixo Mn e alto Nb aplicados em tubos sour service visando aumento do desempenho de tenacidade

    … pipelines for transportation of oil and gas in sour environments, where the presence of hydrogen leads to premature failures of these structures. On the other hand, the low carbon equivalent value, usually found in this type of steel, demands that the hot rolling and accelerated cooling process …

    brazil-ufmg Repository record for Caracterização avançada de aços microligados de baixo Mn e alto Nb aplicados em tubos sour service visando aumento do desempenho de tenacidade (opens in a new tab)

  16. Investigation of hydrogen induced cracking susceptibility of API 5L X65 pipeline steels

    … low temperatures, microbial attack, acidic or sour environments etc. These conditions can trigger different failure mechanisms such as corrosion, embrittlement and cracking. The hydrogen induced cracking (HIC) phenomenon often affects pipelines exposed to sour and acidic environments. It …

    sask Repository record for Investigation of hydrogen induced cracking susceptibility of API 5L X65 pipeline steels (opens in a new tab)

  17. Kinetics and microstructural analysis of fatigue fracture progress in weld joints of duplex stainless steel grade 2205

    … behaviour of the fusion zone in both air and sour environments has been interested and investigated within the damage tolerant design framework. A comparative analysis basis methodology was employed during investigations; beside hybrid plasma-gas metal arc welding, gas metal arc welding and …

    metu Repository record for Kinetics and microstructural analysis of fatigue fracture progress in weld joints of duplex stainless steel grade 2205 (opens in a new tab)

  18. Pitting corrosion behaviour of CRAs in CO2 and CO2/H2S-containing environments using cyclic polarisation technique

    … stresses associated with these aggressive environments, including high H2S content. An understanding of the operating performance for these materials under demanding conditions has to be determined in order to reduce failures, improve corrosion performance and maintain structural integrity. …

    whiterose Repository record for Pitting corrosion behaviour of CRAs in CO2 and CO2/H2S-containing environments using cyclic polarisation technique (opens in a new tab)

  19. Degradation of OCTG Steel in SAGD Application

    … The corrosion mechanism of OCTG steel in the sour environment consisting of H2S and CO2 was fully understood but the performance of the coated (Ni-P coating) and uncoated OCTG steel in a real SAGD operation was not evaluated till now. So in this study, at the first, the coated (electroless …

    alberta Repository record for Degradation of OCTG Steel in SAGD Application (opens in a new tab)

  20. Sulphide Stress Cracking in X80 Pipeline Steel Welds

    … gas pipelines if they are used for severe sour service applications, where severe sour is defined as SSC region 3 in the NACE standard MR0175/ISO 15156, as the range where H2S partial pressure exceeds 1 kPa, and below a pH of 3.5, and above 100 kPa and below a pH of 5.5. Thus, it is very …

    waterloo Repository record for Sulphide Stress Cracking in X80 Pipeline Steel Welds (opens in a new tab)