Global ETD Search

Search theses and dissertations gathered from participating repositories worldwide. Every result links back to the library that holds it. No account is needed.

Results

Showing 1 to 19 of 19 for “"Spherical nanoindentation"”.

  1. Stored energy maps in deformed metals using spherical nanoindentation

    … length scales. Recently, remarkable advances in nanoindentation data analysis techniques have been made which now make it possible to obtain quantitative information about the local mechanical properties of constituent individual grains in polycrystalline metallic samples. In this work, a novel …

    gatech Repository record for Stored energy maps in deformed metals using spherical nanoindentation (opens in a new tab)

  2. Spherical nanoindentation protocols for extracting microscale mechanical properties in viscoelastic materials

    Nanoindentation has a high load resolution, depth sensing capabilities, and can be used to characterize the local mechanical behavior in material systems with heterogeneous microstructures. Recently nanoindentation has been used to extract useful stress-strain curves, primarily in hard materials …

    gatech Repository record for Spherical nanoindentation protocols for extracting microscale mechanical properties in viscoelastic materials (opens in a new tab)

  3. Determination of the Yield Stress of Borosilicate Glasses by Means of Spherical Nanoindentation

    … by means of a novel methodology involving spherical nanoindentation. A theoretical description of this new method is provided alongside corroboration with uniaxial compression tests. The practical effect of water interaction during mechanical surface preparation of the glasses on measuring …

    utk-theses Repository record for Determination of the Yield Stress of Borosilicate Glasses by Means of Spherical Nanoindentation (opens in a new tab)

  4. Quantitative methods for inferring process-structure-property relations in machining

    … properties are inferred from a combination of spherical nanoindentation experiments and a novel Bayesian nanoindentation inverse solution. The process-structure-property linkages are established for OFHC Cu using a coupled nonparametric regression model and a robust method for inverting the …

    gatech Repository record for Quantitative methods for inferring process-structure-property relations in machining (opens in a new tab)

  5. Understanding irradiation embrittlement of reactor pressure vessel steels using micromechanical methods and atom probe tomography

    … to irradiation conditions and alloy composition. Spherical nanoindentation was applied as a near non-destructive technique to correlate nanostructural changes with mechanical property alterations. APT techniques for extracting grain boundary misorientation from APT data were compared to ensure an …

    oxford Restricted access

  6. Micro-mechanical investigations of irradiation tolerance in nanostructured ferritic alloys processed into thin-walled tubing

    … this work shows the use of sharp indentation, spherical nanoindentation, micro-pillar compression, and micro-tensile testing techniques. The first part of the dissertation explores the different techniques on varied material systems. The second part applies these characterization methods to one …

    unr Repository record for Micro-mechanical investigations of irradiation tolerance in nanostructured ferritic alloys processed into thin-walled tubing (opens in a new tab)

  7. Hierarchical and high throughput mechanical characterization of titanium alloys using spherical indentation stress-strain curves

    Recent work has shown the capability of spherical nanoindentation to capture local structure-property relationships in polycrystalline cubic metals by measuring indentation stiffness and yield strength from stress-strain curves as a function of the local microstructure in the indentation zone. …

    gatech Repository record for Hierarchical and high throughput mechanical characterization of titanium alloys using spherical indentation stress-strain curves (opens in a new tab)

  8. Crystal plasticity finite element simulations using discrete Fourier transforms

    … a recently developed data analysis approach for spherical nanoindentation and Orientation Imaging Microscopy (OIM) have been used to extract the critical resolved shear stress of the ferrite phase in dual phase steels. This new methodology offers a novel efficient tool for the extraction of …

    gatech Repository record for Crystal plasticity finite element simulations using discrete Fourier transforms (opens in a new tab)

  9. Rapid evaluation of cyclic performance using small-volume metal samples through spherical indentation

    … of intrinsic material properties. First, novel spherical microindentation protocols are developed on wrought Ti-6Al-4V (Ti64) samples then extended to laser powder bed fusion processed Inconel 718 (IN718) samples. In these studies, repeatable load-displacement loops are successfully converted …

    gatech Repository record for Rapid evaluation of cyclic performance using small-volume metal samples through spherical indentation (opens in a new tab)

  10. The role of grain boundaries in plastic deformation

    … grain boundaries. We perform room-temperature spherical and Berkovich nanoindentation tests on low- and high- angle grain boundaries. We observe that in the high-angle grain boundary sample, the interface acts as a site of microplasticity and as a barrier to incoming dislocations. The low-angle …

    oxford Repository record for The role of grain boundaries in plastic deformation (opens in a new tab)

  11. Mechanisms for White Etching Matter formation under rolling contact loading

    … properties of WEM have also been measured using spherical nanoindentation. The characterization shows that the WEM is elastically soft with a low yield strength and exhibits a low shear resistance. This low shear resistance behavior and reduced yield strength can explain the widespread dispersion …

    gatech Repository record for Mechanisms for White Etching Matter formation under rolling contact loading (opens in a new tab)

  12. High throughput prototyping and multiscale indentation characterization of metallic alloys

    … micro-pillar compression, micro- bending, and nanoindentation. Among these, spherical nanoindentation is the most efficient and most reliable one. This high throughput mechanical protocol is capable of capturing local mechanical responses at different length scales in polycrystalline metals in …

    gatech Repository record for High throughput prototyping and multiscale indentation characterization of metallic alloys (opens in a new tab)

  13. MICROMECHANICS AND MICROSTRUCTURE OF IMPACT-INDUCED BONDING IN METALS

    … microprojectile impact test (LIPIT) and spherical nanoindentation was developed to quantify the phonon-drag regime and to calibrate a physically-based constitutive model for particle impact predictions. Well-controlled, isolated bonded particles were produced using LIPIT, followed by …

    cornell Repository record for MICROMECHANICS AND MICROSTRUCTURE OF IMPACT-INDUCED BONDING IN METALS (opens in a new tab)

  14. Micromechanical testing of irradiated tungsten for fusion

    … 1.67 dpa at 900 °C.</p> <p>Constant strain rate spherical nanoindentation experiments using 5 μm and 10 μm radius tips were executed at 3.2x10-3 s-1, 3.2x10-4 s-1 and 3.2x10-5 s-1 to produce indentation stress-strain curves. The unirradiated sample showed an absence of work hardening and large …

    oxford Repository record for Micromechanical testing of irradiated tungsten for fusion (opens in a new tab)

  15. Micromechanical investigations of the remarkable damage tolerance in tooth-enamel of Hadrosaurid dinosaurs

    … with the small-scale testing techniques like spherical nanoindentation (sub µm to 10s of µm volume- achieved by changing indenter radius) and more specialized in-situ micropillar compression testing (few µm to 10s of µm volume – achieved by changing pillar dimensions). These tests were …

    iastate Repository record for Micromechanical investigations of the remarkable damage tolerance in tooth-enamel of Hadrosaurid dinosaurs (opens in a new tab)

  16. Tribo-Mechanical Investigation of the Functional Components used in Flexible Energy Harvesting Devices

    … films was explored using microtensile testing, spherical nanoindentation, controlled mechanical buckling, stress corrosion cracking, and shear-contact reciprocating wear. The electro-mechanical performance and reliability of functional ZnO films and nanostructures were also studied. ZnO was …

    wvu Repository record for Tribo-Mechanical Investigation of the Functional Components used in Flexible Energy Harvesting Devices (opens in a new tab)

  17. High-throughput assessment of mechanical behavior of pharmaceutical molecular crystals for accelerated drug manufacturing

    … product design and manufacturing optimization. Nanoindentation emerges as a transformative high-throughput, non-destructive technique uniquely suited for probing the mechanical properties of materials at nano- and micro-scales. This methodology offers unprecedented capability to test small …

    umn Repository record for High-throughput assessment of mechanical behavior of pharmaceutical molecular crystals for accelerated drug manufacturing (opens in a new tab)

  18. Contact deformation of carbon coatings: mechanisms and coating design.

    … mechanical properties was undertaken using nanoindentation and nano-scratch tests. The same techniques were used to induce fracture within the coatings to allow subsequent analysis of the fracture mechanism. These were ascertained with the assistance of cross-sectional imaging of indents …

    unsw Repository record for Contact deformation of carbon coatings: mechanisms and coating design. (opens in a new tab)

  19. Extraction of elastic-plastic material properties from spherical indentation stress-strain measurements and finite element simulations

    … curves measured using recently developed spherical indentation protocols. More specifically, protocols are developed to extract the homogenized (bulk) properties (e.g., uniaxial yield strength and hardening rate) at the macroscale. At the microscale, new protocols are formulated to extract …

    gatech Repository record for Extraction of elastic-plastic material properties from spherical indentation stress-strain measurements and finite element simulations (opens in a new tab)