Global ETD Search

Search theses and dissertations gathered from participating repositories worldwide. Every result links back to the library that holds it. No account is needed.

Results

Showing 1 to 9 of 9 for “"Stainless steel -- Testing"”.

  1. A Shear Bondstrength Evaluation of Five Orthodontic Light-Cured Adhesives

    … The brackets were individually bonded to knurled stainless steel testing rings via the respective adhesives. Each bracket was sheared from the testing ring using an Instron machine. For each adhesive a 2, 5, 10, and 20 second cure-time, and an immediate, 5 minute, 20 minute, and 24 hour shear test …

    loma-linda Repository record for A Shear Bondstrength Evaluation of Five Orthodontic Light-Cured Adhesives (opens in a new tab)

  2. The fatigue-crack growth and fracture characteristics of a precipitation-hardened semiaustenitic stainless steel

    … static-strength data on PH15-7Mo (TH 1050) stainless steel are presented in this thesis. In addition, the capability of McEvily and Illg's crack-growth analysis and Kuhn and Figge's residual strength analysis to correlate the test data has been investigated. Axial-load fatigue-crack …

    vt Repository record for The fatigue-crack growth and fracture characteristics of a precipitation-hardened semiaustenitic stainless steel (opens in a new tab)

  3. The effects of nitrogen concentration between 0.27 per cent and 1.30 per cent on internal friction peaks in 304L stainless steel

    … percent on the internal friction peaks in 304L stainless steel. The amplitude of the internal friction peak associated with the stress-induced diffusion of interstitial nitrogen increased as a linear function of the nitrogen content. The activation energy of diffusion was found to decrease with …

    vt Repository record for The effects of nitrogen concentration between 0.27 per cent and 1.30 per cent on internal friction peaks in 304L stainless steel (opens in a new tab)

  4. Impact fracture of austenitic stainless steels

    … material selection is imperative. Austenitic stainless steels may be a likely choice for hydrogen service because their behavior in high pressure hydrogen ranges from no apparent damage to relevant, but generally small ductility loss (13). Because of this Variation in behavior, a single …

    vt Repository record for Impact fracture of austenitic stainless steels (opens in a new tab)

  5. Cellular Corrosion of CoCrMo Total Knee Implants: Understanding Underlying Mechanisms Through Retrieval Analysis and Simulated Inflammatory Conditions

    … Nitride coated implants. After failing normality testing, Mann Whitney Rank Sum tests were utilized to determine any significant differences.In a separate experiment, IC-21 ATCC peritoneal macrophages were cultured with growth medium of RPMI 1640 with 10% fetal bovine serum (FBS), L-glutamine, and …

    tenn-hsc Repository record for Cellular Corrosion of CoCrMo Total Knee Implants: Understanding Underlying Mechanisms Through Retrieval Analysis and Simulated Inflammatory Conditions (opens in a new tab)