Global ETD Search

Search theses and dissertations gathered from participating repositories worldwide. Every result links back to the library that holds it. No account is needed.

Results 1 to 19 of 19 for “"Steam oxidation"”

  1. Steam oxidation of shot peened austenitic stainless steel

    … vacuum, deoxygenated atmospheric pressure steam and deoxygenated 70bar steam. The microstructural changes and oxide morphologies of the shot peened material were observed with SEM, TEM, microhardness testing and TKD mapping. An estimate of the lifetime of the shot peened microstructure in …

    birmingham Repository record for Steam oxidation of shot peened austenitic stainless steel (opens in a new tab)

  2. Steam Oxidation Resistance of Shot Peened Austenitic Stainless Steel Superheater Tubes

    Steam-side oxidation and the resultant exfoliation of iron-based scales cause unplanned shutdowns at coal-fired power generation facilities. Exfoliation mitigation is currently limited to frequent unit cycling to minimize the volume of exfoliated scale and upgrading a plant with a “blow down” …

    ohiolink Repository record for Steam Oxidation Resistance of Shot Peened Austenitic Stainless Steel Superheater Tubes (opens in a new tab)

  3. Cyclic steam oxidation of a steel for biomass power plant application

    … these conditions, the alloy will experience oxidation which greatly affects the lifetime of the materials. The increased likelihood of more cyclic operating conditions means a greater level of understanding of the oxidation and spallation behaviour of these alloys is required. High …

    birmingham Repository record for Cyclic steam oxidation of a steel for biomass power plant application (opens in a new tab)

  4. Steam oxidation of advanced high temperature resistant alloys for ultra-supercritical applications

    Steam oxidation of heat exchanger tubing is of growing interest as increasing the efficiencies of conventional pulverised fuel fired power plants requires higher steam temperatures and pressures. These new, more severe steam conditions result in faster steam oxidation reactions, which can …

    cranfield Repository record for Steam oxidation of advanced high temperature resistant alloys for ultra-supercritical applications (opens in a new tab)

  5. Steam oxidation of heat exchanger materials for the new generation of power plants.

    … efficiencies can be improved by increasing steam working temperatures and pressures inside power plants. However, these more severe working conditions can accelerate degradation phenomena, for example, by steam oxidation. To assess the simulate steam oxidation processes at the elevated …

    cranfield Repository record for Steam oxidation of heat exchanger materials for the new generation of power plants. (opens in a new tab)

  6. Surface Characterization of Accident Tolerant Fuel Claddings Candidates After Prolonged Exposure to Steam Oxidation

    … after extended exposure to a high-temperature steam environment. The surfaces of the materials were studied to determine the impact of the flowing steam on the material’s oxidation. The results showed that both proposed cladding materials exhibited improved oxidation characteristics compared to …

    vcu Repository record for Surface Characterization of Accident Tolerant Fuel Claddings Candidates After Prolonged Exposure to Steam Oxidation (opens in a new tab)

  7. The effect of steam treatment and precipitation hardening on the mechanical properties and wear resistance of sintered iron and iron-copper alloys

    Steam treatments reduce porosity(1) of sintered iron and sintered iron-base alloy products and provide them with increased compressive strength, hardness, resistance to wear and corrosion. The aims of the present investigation were: (a) to examine the influence of copper content and process …

    brunel Repository record for The effect of steam treatment and precipitation hardening on the mechanical properties and wear resistance of sintered iron and iron-copper alloys (opens in a new tab)

  8. Fe<sub>2</sub>O<sub>3</sub>-based Oxygen Carriers for Gaseous and Solid-Fueled Chemical Looping Processes

    … reactor sizing, and decreased capital costs. The steam to H<sub>2</sub> conversion efficiency of Fe<sub>2</sub>O<sub>3</sub> based oxygen carriers using Al<sub>2</sub>O<sub>3</sub>, MgAl<sub>2</sub>O<sub>4</sub> and TiO<sub>2</sub> as support materials is investigated in a fixed bed for chemical …

    ohiolink Repository record for Fe<sub>2</sub>O<sub>3</sub>-based Oxygen Carriers for Gaseous and Solid-Fueled Chemical Looping Processes (opens in a new tab)

  9. The application of plasma assisted chemical vapour deposition of ZrC onto a Zr-alloy substrate

    … zirconium alloy, as fuel rod cladding exposed to steam oxidation produces explosive hydrogen. Thus, the improvement against oxidation of Zr alloy fuel cladding by coatings, such as, silicon carbide (SiC) and zirconium carbide (ZrC) has become an area of interest. This study investigated available …

    nwu-za Repository record for The application of plasma assisted chemical vapour deposition of ZrC onto a Zr-alloy substrate (opens in a new tab)

  10. Estimation of coping time in pressurized water reactors for accident tolerant fuel claddings

    … claddings. In this work, high-temperature steam oxidation characteristics of potential ATF claddings, monolayer iron-chromium-aluminum (FeCrAl) and Cr-coated Zircaloy, are experimentally investigated. Specifically, this work investigates the high-temperature oxidation characteristics of …

    mit Repository record for Estimation of coping time in pressurized water reactors for accident tolerant fuel claddings (opens in a new tab)

  11. Safety of light water reactor fuel with silicon carbide cladding

    … and simulation. High temperature (1100°C~1500°C) steam oxidation experiments demonstrated that the oxidation of monolithic SiC is about three orders of magnitude slower than that of zirconium alloys, and with a weaker impact on mechanical strength. This, along with the presence of the …

    mit Repository record for Safety of light water reactor fuel with silicon carbide cladding (opens in a new tab)

  12. Evaluation of multilayer silicon carbide composite cladding under loss of coolant accident conditions

    … is investigated after exposure to 1,400°C steam and after quenching from 1,200°C into either 100°C or 90°C atmospheric-pressure water. The samples consist of two-layer SiC, with an inner SiC/SiC CMC layer and an outer monolith SiC layer. The relationship between mechanical performance and …

    mit Repository record for Evaluation of multilayer silicon carbide composite cladding under loss of coolant accident conditions (opens in a new tab)

  13. Exploração de ciclos redox de óxido de cério para produção de hidrogénio a partir de gás de síntese

    … by a reducing syngas stream, followed by the oxidation of the reduced Ceria with steam, resulting in hydrogen production. The main objective was to assess the thermodynamic viability of this process by identifying the temperature and composition conditions that maximise the overall energy …

    coimbro Repository record for Exploração de ciclos redox de óxido de cério para produção de hidrogénio a partir de gás de síntese (opens in a new tab)

  14. Synthesis and high-temperature oxidation of ternary carbide coatings on zirconium-based alloy cladding

    … rapid exothermic reaction with high-temperature steam associated with hydrogen generation in accident scenarios motivate the requisite to develop enhanced accident tolerant fuel (ATF) claddings. One reasonable solution to improve the accident tolerance of the zirconium alloy cladding in …

    karlsruhe-diss Repository record for Synthesis and high-temperature oxidation of ternary carbide coatings on zirconium-based alloy cladding (opens in a new tab)

  15. Deposition of Zirconium Carbide onto a substrate

    … the lack of resistance of the zirconium alloy to steam oxidation. Zirconium alloys have been known to oxidise and produce hydrogen in a steam environment which can explode as in the case of Fukushima. To avoid oxidation at high temperatures by steam, the use of a corrosion resistant coating has …

    nwu-za Repository record for Deposition of Zirconium Carbide onto a substrate (opens in a new tab)

  16. Modeling the Effect of Thermal Oxidation on the Pore Structure of Artificial Graphite

    … materials is loss of graphite due to thermal oxidation reactions with air or steam. Oxidation is insidious since it enlarges the inherent pores, which rapidly degrades microstructure and properties. Artificial graphites vary in their initial pore microstructure, yet the currently used 2D …

    ohiolink Repository record for Modeling the Effect of Thermal Oxidation on the Pore Structure of Artificial Graphite (opens in a new tab)

  17. CORROSION AND HYDROGEN RESISTANT MODIFIED ZIRLO SURFACES FOR NUCLEAR FUEL CLADDING

    … zirconium alloy fuel rods react with hot steam resulting in the release of hydrogen. High temperatures increase the oxidation rate and hence the hydrogen production rate which in turn increase the risk of a hydrogen gas explosion such as what is surmised to have happened in the 2011 …

    nmmu Repository record for CORROSION AND HYDROGEN RESISTANT MODIFIED ZIRLO SURFACES FOR NUCLEAR FUEL CLADDING (opens in a new tab)

  18. Hydruration secondaire et fragilisation d'une gaine M5(Framatome) après sollicitation de type APRP

    L'hydruration secondaire, qui fait référence à une prise massive d'hydrogène par la gaine combustible due à l'oxydation à haute température de la surface interne de la gaine, peut survenir pendant un transitoire APRP (Accident de Perte de Réfrigérant Primaire), en cas d'éclatement de gaine …

    star-france Repository record for Hydruration secondaire et fragilisation d'une gaine M5(Framatome) après sollicitation de type APRP (opens in a new tab)