Global ETD Search
Search theses and dissertations gathered from participating repositories worldwide. Every result links back to the library that holds it. No account is needed.
Results
Showing 1 to 20 of 35 for “"Stellite"”.
-
Corrosion Behaviour of High-Carbon High-Molybdenum Stellite Alloys in Amine Environment
Stellite alloys are cobalt-based alloys which display exceptional mechanical properties, wear and corrosion resistance owing to its unique chemical compositions. Stellite 6, which is used for hardfacing of valve trim components within control valves in boiler feedwater systems, have failed in …
-
Improvement in Metal-on-Metal Bearing of Hip Implants with Advanced Stellite Alloys
CoCrMo alloy Stellite 21 has been used as hip implant material decades. However, its limited metal-on-metal bearing has resulted in loosening in hip implants. Three advanced alloys, Stellite 720, Stellite 21 with increased 10 wt%Cr (named modified Stellite 21) and Stellite 21 with additional 0.4 ~ …
-
Experimental and Modeling Study of Sliding Wear Performance for Selected Molybdenum Stellite Alloys
… of wear performance of molybdenum-containing Stellite alloys. Wear testing conditions are pin-on-disc type using a tungsten carbide ball against the Stellite alloys in dry-sliding mode at ambient temperature. Three variables are explored: (i) two rotational speeds, (ii) two normal loads, and …
-
Thermal simulations for the prediction of porosity in investment castings for stellite grade superalloys
… and run to predict the thermal history of a Stellite alloy investment casting prone to the formation of microporosity. The thermal history of the casting was utilized to calculate the thermal gradient at a specified temperature, the rate of cooling during solidification, and the …
-
Electrochemical Study of Corrosion Behavior of Stellite 6 Alloy and 17-4PH Stainless Steel in Amine Solutions
… scientific evidence, the corrosion behavior of Stellite 6 alloy and 17-4PH stainless steel is studied in morpholine, cyclohexylamine and sodium hydroxide solutions at the same pH around 9.5 using electrochemical test methods such as potentiodynamic polarization, cyclic polarization, and EIS in …
-
Comportamento tribológico do par Stellite 6 e Colmonoy 56 utilizado em revestimento de mancal de extrusora monorosca
… ao desgaste adesivo das ligas metálicas Stellite 6 e Colmonoy 56, aplicadas como revestimento resistente ao desgaste em diferentes combinações nos pares de corpos-de-prova ensaiados em laboratório segundo a norma técnica ASTM G-77. Procurou-se assim simular a condição mais crítica de …
-
Additive Manufacturing with Stellite 6 Metal-Cored Wire by Gas Tungsten Arc Welding and Plasma Arc Welding Methods
… and Electron-Beam Processes. In this study, Stellite 6 metal-cored wire was utilized with GTAW to determine printing parameters. However, initial experiment showed that manufacturing thin walls with <3.5 mm thickness would not be possible with continuous weld beads, resulting in poor …
-
Microstructure and Performance Studies of a Novel Cobalt High Entropy Alloy
… (HEA), designated as HE6, is created based on Stellite 6 in this research. The new alloy has the equiatomic Co-Cr-Fe-Ni composition with a large amount of W and other minors. The bulk specimens are fabricated from the alloy powder via spark plasma sintering (SPS) and plasma transferred arc …
-
Tribological Behavior of Spark Plasma Sintered Tic/graphite/nickel Composites and Cobalt Alloys
… determine its effects on tribological behavior. Stellite 21, a cobalt‐chrome‐molybdenum alloy, was also produced by SPS. Stellite 21 has low stacking fault energy and a hexagonal phase which forms during sliding that both contribute to low interfacial shear and friction. Samples were investigated …
-
Long-term performance of pot hardware in continuous galvanizing lines
… line tension. Tests were also conducted on Stellite 6 against Tribaloy T 400 at 50% production line tension. For each test, periodic measurements of wearing rate, surface microstructure and surface hardness were carried out. An unique dross build-up setup which consists of two sleeves …
-
Scaling Up The Tribological Assessment of Laser Clad Rail to Build The Case For Field Implementation
… were martensitic stainless steel (MSS), Stellite 6, R260, and T400. The substrate rail material used was R260 grade rail. Also, some premium rail tests were conducted for comparison: Manganese (Mn), Chromium (Cr) and R400 HT. Small-scale twin disc tests were conducted to find the full …
-
Navařování kobaltové slitiny plazmou
… součásti byla zvolena kobaltová slitina Stellite 21. Následně byl popsán navařovací stroj PPC 250 PTM a hořák PHP 250 S, použitý v praktické části. V praktické části byly odladěny navařovací parametry a navrhnut vhodný navařovací postup pro danou konkrétní součást.
-
Effects of Heat Treatment on Microstructure and Wear Resistance of Stainless Steels and Superalloys
… slurry coating process developed at Kennametal Stellite Inc. on the microstructure, hardness and wear behavior of superalloys and stainless steels. Low-carbon Stellite 22, cobalt-based Tribaloy T-400C, martensitic AISI 420 and AISI 440C stainless steels are studied in this research. The …
-
Mathematical modelling of heat transfer in the vacuum investment casting of superalloy IN718
… of experiments done in collaboration with Deloro Stellite Inc. of Belleville, Ontario. The model was applied to the experimental casting configurations. The model results were most influenced by the value of the mould thermal conductivity, the interface contact function and the radiation …
-
Materials and wear modelling of a cobalt-chromium alloy in self-mated reciprocated sliding
… testing of a cobalt-based hard-facing alloy, Stellite 6TM, was performed under selfmated reciprocating dry room-temperature conditions. The wear-rate as a function of load was not constant, suggesting a different model of wear than typical linear models of wear. Probing the debrWis morphology, …
-
Experimental and Computational Studies of Cobalt-Containing High-Entropy Alloys for Wear-Resistance Application
… conventional Co-based superalloys, particularly Stellite and Tribaloy alloys. Following optimization of milling duration, complete alloying was achieved after 40 h of milling, and the powders were subsequently consolidated by SPS. Carbon introduced from the toluene process control agent (PCA) …
Page 1 of 2