Global ETD Search
Search theses and dissertations gathered from participating repositories worldwide. Every result links back to the library that holds it. No account is needed.
Results
Showing 1 to 20 of 150 for “"Stirrups"”.
-
Anchorage of stirrups in prestressed concrete I-girders
… specifically when the lower hooks on the stirrups are oriented parallel to the longitudinal prestressing strands and are not bent around any longitudinal bars. Such detailing does not meet the specifications in the Canadian Highway Bridge Design Code CSA S6-06. An experimental …
-
Shear Resistance of Reinforced Concrete Beams Without Stirrups
Shear failures in concrete structures are very hazardous. These failures can rarely be predicted and often happen explosively. For decades, tests have been done to study this phenomenon, in order to try to solve the riddle that shear is. Researchers have become more knowledgeable about shear and …
-
Concrete beams with stirrups subject to torsion, shear and bending
… The effects of concrete strength, spacing of the stirrups, the amount of longitudinal steel and the breadth of the section on the ultimate torsional capacity are investigated. Based on the skew-bending mechanism, compatibility, and linear stress-strain relationship for the concrete and the steel, …
-
Prestressed concrete beams with stirrups subjected to torsion, bending and shear
… of 37 eccentrically prestressed beams with stirrups. Single variable parameters were investigated including the prestressing force, the prestressing steel area, the concrete strength, the aspect ratio h/b and the stirrups size and spacing. Interaction of bending, torsion and shear was also …
-
High performance fiber reinforced concrete for the replacement of shear stirrups
Corrosion of steel reinforcements, especially stirrups, is considered as one of the most common reasons that shorten the service life of the reinforced concrete, RC, structures. In several cases the rehabilitation of corroded RC structures is so expensive and time consuming that a decision for the …
-
Behavior of slender beams without stirrups: effects of load distribution and member depth
… on slender reinforced concrete members without stirrups have been performed using concentrated loading. Furthermore, the uniform load tests that have been conducted typically involve members with smaller specimen depths (d) and larger reinforcement ratios (ρ) than are commonly used in practice. …
-
Behaviour of fibre-reinforced polymer (FRP) stirrups as shear reinforcement for concrete structures
… reinforcement within a concrete structure, steel stirrups are the first to corrode. Fibre reinforced polymers (FRP) provide an alternative that does not corrode and has many other benefits such as a high strength-to-weight ratio. However, the inherent disadvantages of FRP in certain loading …
-
Seismic Behaviour of Exterior Beam-Column Joints Reinforced with FRP Bars and Stirrups
… of concrete BCJs reinforced with FRP bars and stirrups. An experimental program was conducted at the University of Manitoba to participate in achieving this objective. Eight full-scale exterior T-shaped BCJs prototypes were constructed and tested under simulated seismic load conditions. The …
-
Meso-Scale Simulation of Size-Dependent Shear Behavior in Glass Fiber Reinforced Polymer Reinforced Concrete Beams without Stirrups
… GFRP reinforced concrete (RC) beams without stirrups. The numerical model includes: (1) a calibrated and validated concrete LDPM; (2) orthotropic GFRP bar elements; and (3) a nonlinear bond-slip law for the GFRP barconcrete interface. In the first study, LDPM-based numerical models are …
-
Anchorage of shear reinforcement in prestressed concrete bridge girders
… has typically used epoxy coated straight legged stirrups anchored in the tension zone as transverse reinforcement in prestressed concrete bridge girders. With the straight legs of the U-shaped stirrups anchored into the bottom flange of the girders, this configuration is readily placed after …
-
Behaviour of Shear Critical RC Beams with Corroded Longitudinal Steel Reinforcement
… level (2.5%, 5% and 7.5%) and existence of stirrups (beams without stirrups and beams with stirrups). The feasibility of repairing the corroded shear critical RC beams with CFRP laminates was also investigated. Sixteen specimens were corroded using an accelerated corrosion technique whereas …
-
Shear Behaviour of Slender RC Beams with Corroded Web Reinforcement
… the effect of corrosion of web reinforcement (stirrups) on the shear behaviour of slender reinforced concrete (RC) beams. The experimental program consisted of seventeen slender shear-critical RC beams: five uncorroded and twelve corroded beams. The test variables included: 1) corrosion level …
-
Finite Element Modelling of GFRP Reinforced Concrete Beams
… concrete beams reinforced with and without GFRP stirrups. The analyses of beams without stirrups are presented first. The Hognestad Parabola was effective in modelling the compressive behaviour of the concrete. A fracture mechanics approach was used to model the post-cracking tensile behaviour of …
-
Shear strengthening of reinforced concrete beams using an external Carbon Fibre Reinforced Polymer(CFRP) composites of low elastic modulus
… impractical due to thecongestion of steel stirrups. Currently, CFRP is used for strengthening reinforcedconcrete structures that have reduced integrity due to corrosion of steel reinforcementor unintentional overloading. The aim of this thesis is to mitigate the congestion ofsteel stirrups …
-
Confinement Limits For Tensile Lap Splices Under Static Loading
… lap splices, the benefit provided to the lap by stirrups placed to intercept cracking due to bond splitting action is recognized by the American Concrete Institute (ACI 318-89) and the design recommendations of the ACI Committee 408, on which the American code provisions are partially based. …
-
High cycle (fatigue) resistance of reinforced concrete beams with lap splices
… was the degree of transverse reinforcement (stirrups) which was provided along the lap splice. The specimens used in this experimental program were seven meters in length, with a cross section 330 mm wide and 508 mm deep, and were reinforced with two No. 30 Grade 400 bars, top and bottom. A …
-
Behaviours of polyvinyl alcohol - engineered cementitious composite beams under static and fatigue loadings
… steel reinforced PVA-ECC beams with and without stirrups, steel reinforced normal concrete beams with and without stirrups, and plain PVA-ECC beams. The effects of PVA-ECC matrix, stirrups and longitudinal reinforcement bars on the structural behaviours of the steel reinforced PVA-ECC beams were …
-
An investigation into the punching shear failure in R.C. waffle slabs subjected to concentrated load
… local solid area, and the effectiveness of the stirrups supplied inside the ribs. The experimental results were compared with the calculated results by following the provisions of BS8110.<br/><br/>The theoretical study was carried out in parallel; the Upper Bound Analysis and Nonlinear Finite …
-
Glass Fiber-Reinforced Polymer (GFRP) Reinforced Concrete Corner Joints Subjected to Opening Moments
… perpendicular to the inner corner, c) confining stirrups within the joint panel, or d) both bent bars and confining stirrups. The aim of the study was to determine the effects of each design choice on corner joint behaviour. Test results showed that increasing development length of GFRP using …
Page 1 of 8