Global ETD Search

Search theses and dissertations gathered from participating repositories worldwide. Every result links back to the library that holds it. No account is needed.

Results 1 to 20 of 21 for “"Thermal debinding"”

  1. Failure analysis of green ceramic bodies during thermal debinding

    In industry, thermal debinding is the traditional mode of binder removal from multilayer ceramic capacitors (MLCs). Binder removal from ceramics takes as long as 50-150 h, thereby contributing significantly to the manufacturing costs and also controlling the production rate. Increasing energy costs …

    missouri Repository record for Failure analysis of green ceramic bodies during thermal debinding (opens in a new tab)

  2. Magnesium Polyolefin Interactions during Thermal Debinding in the MIMProcess of Magnesium

    … of the mechanisms taking place during the thermal debinding of PE and PP based polymers in combination with magnesium powder is developed by using literature and different experimental setups.

    cau-kiel Repository record for Magnesium Polyolefin Interactions during Thermal Debinding in the MIMProcess of Magnesium (opens in a new tab)

  3. Experimental investigation and numerical simulation of thermal debinding and sintering processes in powder injection moulding.

    L'étape de déliantage est une étape importante et parfois critique pour le procédé Moulage par Injection des Poudres. A cet effet, des analyses thermogravimétriques (TGA) ont été réalisées pour bien comprendre les mécanismes du déliantage thermique sous atmosphère imposée (Argon). Les méthodes de …

    star-france Repository record for Experimental investigation and numerical simulation of thermal debinding and sintering processes in powder injection moulding. (opens in a new tab)

  4. Enhancing Investment Casting Through 3D Printing of Silica Molds: A Comparative Study of Thermal Debinding and Sintering Processes

    … and reduced tooling requirements. Two distinct thermal processing routes, thermal debinding alone, and thermal debinding followed by sintering, were applied to the printed molds to assess their influence on mold integrity and final casting quality.The molds were used to cast A356 aluminum alloy, …

    ohiolink Repository record for Enhancing Investment Casting Through 3D Printing of Silica Molds: A Comparative Study of Thermal Debinding and Sintering Processes (opens in a new tab)

  5. The Formulation of Titanium - based Metal Feedstocks and the Fabrication of Parts using the Powder Injection Moulding Process

    … based metal powder feedstock followed by a debinding process and subsequent sintering. The fabrication process in its entirety was investigated in four distinct steps. Feedstock formulation involved combining the metal powders with various carrier components. Injection moulding enabled the …

    waikato-masters Repository record for The Formulation of Titanium - based Metal Feedstocks and the Fabrication of Parts using the Powder Injection Moulding Process (opens in a new tab)

  6. Fabrication and Characterization of Miniaturized Components Based on Extruded Ceramic-Filled Polymer Blends

    … can be sintered to full density. A two-step debinding is introduced to eliminate debinding defects that are commonly observed in thermal debinding (TD). Cracking is a major issue due to a lack of pore spaces for outgassing of pyrolysis products in traditional TD. In two-step debinding, a …

    lsu-thes Repository record for Fabrication and Characterization of Miniaturized Components Based on Extruded Ceramic-Filled Polymer Blends (opens in a new tab)

  7. Experimental Study of Effect of Sintering Conditions on the Quality of Resin-Based 3D Printed SS316L Components

    … between stainless steel 316L metal loads, thermal processing, and the overall final quality. Green parts were produced using two dif-ferent slurries with varying solid loadings: one from a commercial supplier (ADMATEC) and the other was prepared in house. Green bodies were subjected to …

    ohiolink Repository record for Experimental Study of Effect of Sintering Conditions on the Quality of Resin-Based 3D Printed SS316L Components (opens in a new tab)

  8. Study of Fiber-Loaded Slurries for Ceramic Matrix Composite Fabrication by Additive Manufacturing

    … alumina ceramic exhibits a good combination of thermal and mechanical properties, including thermal shock resistance, high melting point, thermal oxidation resistance, good thermal conductivity, hardness, and mechanical strength. However, it is very brittle. Introducing alumina fiber as a …

    ohiolink Repository record for Study of Fiber-Loaded Slurries for Ceramic Matrix Composite Fabrication by Additive Manufacturing (opens in a new tab)

  9. Improving Structural Integrity of Additively Manufactured High-Temperature Gas Turbine Component

    … encompassing design, printing, comprehension of thermal debinding and sintering processes, post-processing, optimization, and characterization, all aimed at achieving complex cooling structures with optimal density using stainless steel material and In718 as a case study. Subsequently, the …

    ucf Repository record for Improving Structural Integrity of Additively Manufactured High-Temperature Gas Turbine Component (opens in a new tab)

  10. Study of rheological and sintering behavior of iron-based feedstock used in low-pressure metal injection molding

    … %) of this powder. Furthermore, to design the debinding cycle (i.e., wick thermal debinding) and define the presintering temperature (i.e., 600ºC), the same powder with optimal binder formulation (i.e., 1 vol. % stearic acid as a surfactant, 2 vol. % ethylene-vinyl acetate as a thickening …

    ets-quebec

  11. Material extrusion 3D printing of metal alloy: Material, methods and application.

    … manufacturing scenarios. A multi-stage thermal debinding protocol was developed based on thermogravimetric analysis, ensuring complete binder removal without introducing defects. The investigation of aluminum-magnesium-tin alloys revealed unique challenges associated with pure aluminum …

    louisville Repository record for Material extrusion 3D printing of metal alloy: Material, methods and application. (opens in a new tab)

  12. 3D printing of aluminum alloys under different extrusion techniques

    … The main objectives were to optimize printing, thermal debinding, and sintering parameters for each feedstock and AM technique, and to assess the resulting mechanical properties and microstructures of the fabricated parts.For printing, AA6061 filament processed via FDM achieved optimal results …

    barcelona Repository record for 3D printing of aluminum alloys under different extrusion techniques (opens in a new tab) Embargoed

  13. Materials and process design for ceramic fused filament fabrication (CF3) of hydroxyapatite.

    … Sintering at 1250 °C for 4 h in air, after thermal debinding, resulted in a relative density of ~85% with HAp and tricalcium phosphate (TCP) as major constituents. Sintered HAp10SN samples also revealed an almost 70% reduction in the grain size and 147% increase in the hardness compared to …

    louisville Repository record for Materials and process design for ceramic fused filament fabrication (CF3) of hydroxyapatite. (opens in a new tab)

  14. Development and optimization of a Low Temperature Co-fired Ceramic suspension for Mask-Image-Projection-based Stereolithography

    … printability by MIP-SLA technology, and the post-thermal treatment of debinding and sintering. The photocurable LTCC suspension consists of ceramic particles dispersed in a suitable photocurable resin, which must polymerize in the visible light range, trapping the ceramic particles. The challenge …

    barcelona Repository record for Development and optimization of a Low Temperature Co-fired Ceramic suspension for Mask-Image-Projection-based Stereolithography (opens in a new tab)

  15. Material development and process optimisation for Digital Light Processing of translucent alumina

    … the green samples was investigated. Afterwards, thermal gravimetric analysis (TGA) and differential scanning calorimetry (DSC) were employed to determine the optimal thermal debinding parameters. Upon examination of various debinding regimes, the debinding heat rate of 0.2 °C/min and increased …

    birmingham Repository record for Material development and process optimisation for Digital Light Processing of translucent alumina (opens in a new tab)

  16. Development of PEG based binders for metal injection moulding with special focus on titanium

    … easily be contaminated by the binders during the debinding and sintering stages. The lack of industrial confidence in the Ti-MIM is likely due to the limited understanding of binder chemistry. As the same binder systems are often used for different powders in MIM, a poor binder may still lead to …

    auckland-ms Repository record for Development of PEG based binders for metal injection moulding with special focus on titanium (opens in a new tab)

  17. Synthesis, Microstructure and Mechanical Properties of Titanium with Controlled Levels of Porosity

    … to form compacts with a green density of 45%. Thermal debinding was carried out at 320°C with an argon flow for 2 hours, followed by vacuum sintering different samples at 1000°C and 1200°C for 0.5 hours, respectively. The porous sintered compacts had satisfactory tensile strength with some …

    waikato-masters Repository record for Synthesis, Microstructure and Mechanical Properties of Titanium with Controlled Levels of Porosity (opens in a new tab)

  18. Future glass factory: precision shaping of glass using amorphous silica nanocomposite prepolymer and replication molding

    … sensing due to its exceptional transparency, thermal stability, and recyclability. Despite the benefits of traditional glass fabrication methods like glass blowing, these approaches face significant challenges, including energy-intensive processes, susceptibility to defects, and limitations in …

    qu-belfast Repository record for Future glass factory: precision shaping of glass using amorphous silica nanocomposite prepolymer and replication molding (opens in a new tab)

  19. Producing near-net shape titanium alloy parts by metal injection moulding

    … injection moulding, removing the binder (debinding) and sintering. The binder affects feedstock rheology, allowing the required shape to be moulded. It then needs to be removed so the object can be sintered to consolidate into a near-net shaped part. As MIM has many advantages, including …

    waikato-masters Repository record for Producing near-net shape titanium alloy parts by metal injection moulding (opens in a new tab)

  20. Développement d'une formulation céramique partiellement biosourcée pour la FA

    Un nouveau feedstock à base de polymères biosourcés et de zircone a été élaboré en vue de son utilisation pour la fabrication de pièces techniques en céramique frittée par un procédé CIM-like (Ceramic Injection Molding-like) plus respectueux de l’environnement (formulation partiellement biosourcée, …

    star-france Repository record for Développement d'une formulation céramique partiellement biosourcée pour la FA (opens in a new tab)

Page 1 of 2