Durability of HDPE Geomembrane Seams and Sheet in Brine and Landfill Leachate
… the welds connecting the GMB sheets are key factors affecting long-term liner performance. Thus, a series of accelerated immersion tests are used to examine the effect of landfill leachate and brine on HDPE geomembrane (GMB) sheet and seams. The effect of ageing in these solutions was …
-
Durability of HDPE Geomembranes for Municipal Solid Waste Landfill Applications
A series of laboratory accelerated immersion tests are used to examine the effects of different chemicals found in municipal solid waste leachate, geomembrane thickness, and incubation temperatures on the degradation of different high density polyethylene geomembranes. It was found that surfactant …
-
Longevity of Polyethylene Geomembranes in Heap Leaching and Tailings Storage Applications
… tap water. Immersion tests were conducted for up to 10 years at different temperatures. Results show that increasing the pH from 9.5 to 13.5 and from 0.5 to 2.0 in heap leaching environments accelerated antioxidant depletion and reduced the time to nominal failure (tNF) of the same GMB. In …
-
Performance of High-Density Polyethylene and Bituminous Geomembranes in Physically Aggressive Applications
… of antioxidants and stabilizers was monitored using standard and high-pressure oxidative induction time (OIT) tests. All four GMBs had very high off-the-roll stress crack resistance (SCRo) that decreased to stable, more representative values shortly after immersion. The time to nominal …
-
The Performance of HDPE Geomembrane Fusion and Bituminous Geomembrane Seams
… (GMB) sheet material and seams are critical factors controlling the design life of a constructed barrier system. In particular, the resistance to stress cracking and retention of antioxidants in the GMB are critical factors to both the short and long-term performance. Thus, stress crack …
-
Durability of Multilayered Textured and Fortified Smooth Polyethylene Geomembranes in Different Geoenvironmental Applications
… polyethylene geomembranes (GMBs) is examined to explore their degradation behaviour in different geoenvironmental applications. Jar immersion tests are used to accelerate the degradation of the GMBs in the laboratory at a range of temperatures (25 to 95oC) for 4 to 8 years. The degradation of …
-
Assessing the Effects of Texturing, Fusion, and Extrusion Welds on Stress Crack Resistance and the Relation Between Stress Crack Resistance and Work Hardening
… barrier system. In particular, the resistance to stress cracking and the preservation of antioxidants within the GMB are critical factors to both short-term and long-term performance. While the single point notch constant tensile load stress crack resistant (SP-NCTL SCR) test is a conventional …
-
Effect of Chemical and Physical Ageing on the Longevity of Smooth and Textured Geomembranes in Geoenvironmental Applications
… This involved conducting immersion tests to simulate the ageing of GMBs on exposure to chemical solutions simulating field applications. The reduction in stress crack-resistance (SCR) due to physical ageing is examined. It is shown that a reduction in SCR was observed for a 1.5 mm smooth …
-
The Chemical Durability of Elastomeric Bituminous Geomembranes (BGMS) in Different Geoenvironmental Applications at Elevated Temperatures
The chemical durability of elastomeric bituminous geomembranes (BGMs) is investigated using laboratory accelerated immersion tests for different geoenvironmental applications. The effects of elevated temperatures, thickness, and incubation media on the mechanical, rheological, and chemical …