Reliability and surface degradation aspects of synthetic insulator materials for HV application
… other things, environmental stresses such as UV, air pollutants, etc. The reliability of an insulator material is governed by the surface and other characteristics that do not drift much as a function of stresses and time. The surface characteristics of various synthetic materials, when these …
-
Viscosity of biogenic secondary organic aerosol and atmospheric implications
… we quantified the effect and magnitude of UV-aging (a photo-oxidation process) on the viscosity of SOA particles. Our results showed that aging of SOA by exposure to UV radiation over multiple days significantly increased the viscosity of SOA particles. Additionally, τmix,org,200nm …
-
Assessing the impact of heavy metals in agricultural plastic mulch film on plant and soil health
… 19 metal elements, with metal contents averaging 0.47 % in LDPE and 3.49 % in biodegradable mulch films. Several metals identified, e.g., As, Cd, Cr, Cu, Ni, Pb, and Zn, are considered to be potentially hazardous by international standards. Most metals, except Cu and Zn, were present at …
-
Ultra-Violet Degradation Behavior of Polymeric Backsheets of Photovoltaic Modules
… is designed to understand the ultra-violet (UV) degradation of polymeric backsheets used in PV modules. Commercial photovoltaic backsheets from four suppliers were UV-aged for up to 3000 hours. The aged samples were tested using optical microscopy, scanning electron microscopy (SEM), …
-
Síntese hidrotérmica assistida por micro-ondas de tiO2, e aplicação em nanocompósito
… impregnated with methylene blue was evaluated by UV- vis spectroscopy from the intensity variation of absorption main peak at 660nm with time of exposure to the UV chamber. Changes in the contact angle and microhardness were analyzed before and after UV aging test. The effect of ultraviolet …
-
Manufacturing of advanced continuous fiber reinforced composites for high temperature applications
… composite material, exposed to an accelerated UV-aging environment, were assessed. The work performed provides valuable information with respect to the processing of continuous fiber reinforced composites using new materials and processes"--Abstract, page iv.
-
Chemo-rheological Characterization of Asphalt Binders Using Different Aging Processes
… of asphalt binders, which are affected by aging, binder modifications, and the incorporation of reclaimed asphalt pavement (RAP) materials. However, significant gaps exist in understanding the long-term chemical and rheological changes induced by aging processes (particularly with respect …
-
Ecotoxicological impacts of polystyrene micro- and nanoplastics in freshwater systems: gender‑specific, aging‑driven, and sediment‑associated effects
… for investigating controlled particle aging and biological responses. A multi-scale approach was adopted to examine responses across interconnected biological and sediment-associated levels. Zebrafish (Danio rerio) exposures examined responses to pristine and UV-aged PS particles, …
-
CHARACTERIZATION AND MECHANICAL MODELING OF UV-AGED SEMICRYSTALLINE POLYMERS
Polymers inevitably undergo various types of aging in service, which depend on environmental factors such as UV radiation, heat, and humidity. Previous work on polymer aging has focused on either its chemical or mechanical features; however, little attention has been paid to the chemo-mechanical …
-
Etude des mécanismes de vieillissement d'un caoutchouc EPDM (Ethylène Propylène Diene Monomer)
… thèse est consacré à l’étude du vieillissement UV d’un caoutchouc EPDM (éthylène propylène diène monomère) avec une attention spéciale sur les additifs du système de vulcanisation. Pour cela nous avons utilisé des techniques particulièrement adaptées à l’analyse de surface telles que le …
-
INTERFACIAL PHENOMENA IN AND OUT-OF-EQUILIBRIUM: COLLOIDAL PRINCIPLES FOR MICROPLASTIC DETECTION AND REMEDIATION
… this strategy encodes polymer identity, UV aging history, concentration, and the presence of natural organic matter into optically readable assembly patterns that can be analyzed using computer vision tools. Specifically, we develop a multi-object detection and tracking framework that …
-
Experimental Characterization and Modeling of Aging-Induced Damage in Semicrystalline Thermoplastics
… environmental conditions, such as ultraviolet (UV) radiation, high temperatures, or moisture, initialize chemical reactions that degrade the material in a process referred to as chemical aging. Eventually, chemical aging leads to a catastrophic loss of ductility, i.e. embrittlement, often …
-
Transport of Microplastics in Shore Substrates: Roles of Polymer Characteristics and Environmental Processes
… environment. The results indicated that seawater aging mainly affected the physical properties of MPs, increasing its surface pores and hydrophilicity. Ultraviolent (UV) aging significantly increased its hydrophilicity and crystallinity and introduced oxygen-containing functional groups onto MPs. …
-
Inter-Relationships Between Chemistry, Network Structure and Properties of Chain Growth Dimethacrylate Thermosets
… undergo reductions in rubbery moduli upon aging under these conditions. X-Ray photoelectron spectroscopy shows higher levels of oxidation on the bisphenol-A vinyl ester networks cured with styrene, especially those containing dimethylaniline and cobalt naphthenate as accelerators. Scanning …
-
Desenvolvimento de tintas intumescentes a base de resinas benzoxazina e epóxi : avaliação da proteção contra fogo após exposição à radiação UV
… dos filmes ao envelhecimento ultravioleta (UV) na resistência contra o fogo. As formulações propostas foram aplicadas em substratos de aço e expostas a testes de queima. As tintas foram caracterizadas por microcalorimetria de combustão, análise termogravimétrica e infravermelho por …
-
Étude des Substances Non Intentionnellement Ajoutées (NIAS) dans le polypropylène et effets potentiels du recyclage et du vieillissement UV
… formulé avec divers additifs (Alkanox 240, BHT, UV326, UV944) dans le but d’identifier et de quantifier les NIAS à l’aide de techniques multi-analytiques. Cinq NIAS dérivés de l’Alkanox 240 ont été identifiés et quantifiés, tandis que des NIAS issus du BHT ont également été observés, bien que …
-
Wood engineering: properties and durability improvement through innovative and sustainable processes
L'abstract è presente nell'allegato / the abstract is in the attachment
-
Σχεδιασμός και ανάπτυξη βιοϋλικών από υβριδικά σύνθετα με βάση το πολυ(γαλακτικό) οξύ
… and TiO2/PLLA nanocomposites under ultraviolet UV-irradiation was also carried out. Moreover, the antibacterial behavior against Escherichia coli (E. coli) bacteria of selected PLLA nanocomposites, was examined. For the preparation of PLA porous scaffolds a salt - leaching technique was applied. …