  1. Synthesis, Processing and Characterization of Polymer Derived Ceramic Nanocomposite Coating Reinforced with Carbon Nanotube Preforms

    … as coating material due to their high hardness, wear and corrosion resistance, and the ability to withstand high temperatures. Critical to the success of these materials is the effective heat transfer through a material to allow for heat diffusion or effective cooling, which is often …

    ucf Repository record for Synthesis, Processing and Characterization of Polymer Derived Ceramic Nanocomposite Coating Reinforced with Carbon Nanotube Preforms (opens in a new tab)

  2. Study of wall thickness and its impact on microstructure on 316L manufactured with Direct Metal Laser Sintering

    … by different wall thicknesses. In addition, hardness and porosity are analyzed with a perspective of wall thickness. In this study 9 different thicknesses, ranging from 0,2 mm up to 3 mm, were selected. The structure was cut in a way so that the middle part of each wall could be observed to …

    chalmers Repository record for Study of wall thickness and its impact on microstructure on 316L manufactured with Direct Metal Laser Sintering (opens in a new tab)

  3. Investtigation of the precipitation hardening behaviour and the corrosion properties of novel aluminium : manganese alloys containing scandium and zirconium

    … changes in specific resistivity at -196°C. The hardness increase due to the Al3(Sc,Zr) precipitates was studied by the Vickers hardness measurement (HV5). As the aluminium-manganese alloys are generally wrought alloys, the corrosion characteristics of the extruded samples quenched from the …

    clausthal Repository record for Investtigation of the precipitation hardening behaviour and the corrosion properties of novel aluminium : manganese alloys containing scandium and zirconium (opens in a new tab)

  4. Threshold Velocity and Incubation Period in Water Droplet Erosion

    … (i.e., roughening) and the rate of change in hardness (i.e., hardening) on the damage accumulation process have experimentally and numerically been investigated in this work. Water droplet erosion tests were carried out on Ti-6Al-4V alloy and 17-4 PH stainless steel. Scanning electron …

    concordia

  5. Characterization of New Rotary Endodontic Instruments Fabricated from Special Thermomechanically Processed NiTi Wire

    … by differential scanning calorimetry (DSC). Vickers hardness measurements were made since hardness variations for the same type of alloy has been found to correlate with variations in mechanical properties. The microstructures of the NiTi alloys were revealed by acid etching and examined with …

    ohiolink Repository record for Characterization of New Rotary Endodontic Instruments Fabricated from Special Thermomechanically Processed NiTi Wire (opens in a new tab)