Global ETD Search

Search theses and dissertations gathered from participating repositories worldwide. Every result links back to the library that holds it. No account is needed.

Results

Showing 1 to 20 of 31 for “"Vickers indentation"”.

  1. Efficacy of Vickers indentation method to measure residual stress in additively manufactured IN718 specimens

    … techniques are used in the industry, and the Vickers indentation method has been proposed as a less expensive, rapid evaluation technique of residual stresses. The efficacy of the Vickers indentation method as a residual stress measurement technique was evaluated in the study. It was observed …

    nwu-za Repository record for Efficacy of Vickers indentation method to measure residual stress in additively manufactured IN718 specimens (opens in a new tab)

  2. Investigation of the Lanthanide Sesquioxides as High Temperature Transformation Toughening Agents

    … DTA, dilatometry, ambient and high temperature Vickers indentation, and notched-beam three point flexure.

    uiuc Repository record for Investigation of the Lanthanide Sesquioxides as High Temperature Transformation Toughening Agents (opens in a new tab)

  3. Preparation, microstructure and properties of silicon carbide-dysprosia composites

    … of the composites was determined using the Vickers indentation method. Elastic properties were determined by the ultrasonic pulse echo technique. Flexure strengths were determined using four point bend testing. Fracture toughness was determined by both the three point, single-edge notched …

    uiuc Repository record for Preparation, microstructure and properties of silicon carbide-dysprosia composites (opens in a new tab)

  4. Understanding the Mechanical and Physical Anisotropy of Shales

    … shales as model systems. First, we conducted nanoindentation tests along both the bedding plane parallel (BPP) and bedding plane normal (BPN) directions for all shales. We observed that the bituminous shale has the highest Young’s modulus, followed by argillaceous shale, and then kerogen-rich …

    tamu Repository record for Understanding the Mechanical and Physical Anisotropy of Shales (opens in a new tab)

  5. A Bio-Inspired Self-Healing Polymer System for Sustainable Plastics

    … for propagating preexisting cracks induced by a Vickers indentation in P[3,4-DHS-S], and the effects that different cross-linking agents have on crack growth within the polymer matrix. A Life Cycle Assessment (LCA) is also performed to give component designers supplemental information needed to …

    purdue-thes Repository record for A Bio-Inspired Self-Healing Polymer System for Sustainable Plastics (opens in a new tab)

  6. Mechanical Properties of Sodium and Potassium Activated Metakaolin-Based Geopolymers

    … The mechanical characterization included Micro-indentation, Vickers indentation and fracture toughness measurement, as well as compressive testing. It was found that structure and mechanical properties of GPs depend on their chemical composition. The Na-GPs with ratio 3 have a highest …

    tamu Repository record for Mechanical Properties of Sodium and Potassium Activated Metakaolin-Based Geopolymers (opens in a new tab)

  7. ΜΕΛΕΤΗ ΤΩΝ ΕΠΙΦΑΝΕΙΑΚΩΝ ΚΑΙ ΔΙΕΠΙΦΑΝΕΙΑΚΩΝ ΙΔΙΟΤΗΤΩΝ ΤΗΣ ΣΤΑΘΕΡΟΠΟΙΗΜΕΝΗΣ ΖΙΡΚΟΝΙΑΣ ΚΑΙ ΣΥΣΤΗΜΑΤΩΝ ΖΙΡΚΟΝΙΑΣ ΣΕ ΕΠΑΦΗ ΜΕ ΡΕΥΣΤΑ ΜΕΤΑΛΛΑ

    … AT ROOM TEMPERATURE WASDETERMINED USING THE "VICKERS INDENTATION TECHNIQUE". THE VALUE OBTAINED IS ΓSV=3.1 Z. M-2. A NEW MODEL OF THE WORK OF ADHESION WAS PROPOSED. ACCORDING TO THIS MODEL THE MELTING OF ZRO2 BY THE METALS IN, SN, BI, PB (LOW MELTING POINT METALS) IS ESTABLISHED BY VAN DER …

    greece Repository record for ΜΕΛΕΤΗ ΤΩΝ ΕΠΙΦΑΝΕΙΑΚΩΝ ΚΑΙ ΔΙΕΠΙΦΑΝΕΙΑΚΩΝ ΙΔΙΟΤΗΤΩΝ ΤΗΣ ΣΤΑΘΕΡΟΠΟΙΗΜΕΝΗΣ ΖΙΡΚΟΝΙΑΣ ΚΑΙ ΣΥΣΤΗΜΑΤΩΝ ΖΙΡΚΟΝΙΑΣ ΣΕ ΕΠΑΦΗ ΜΕ ΡΕΥΣΤΑ ΜΕΤΑΛΛΑ (opens in a new tab)

  8. Shear band evolution in Zr/Hf-based bulk metallic glasses under static and dynamic indentations

    … To fully investigate shear band characteristics, indentation tests that can confine the deformation in a limited region have been pursued. In this thesis, a detailed investigation of thermal stability and mechanical deformation behavior of Zr/Hf-based BMGs is conducted. First, systematic studies …

    mtu Repository record for Shear band evolution in Zr/Hf-based bulk metallic glasses under static and dynamic indentations (opens in a new tab)

  9. Sintering methodologies for silicon carbide ceramics

    … 99.66% relative density, 22.76 to 27.66 GPa for Vickers hardness and 3.0 to 4.18 MPa⋅m1/2 for Vickers indentation fracture toughness. The work showed that the merits of increasing B4C addition stopped at the solid solubility limit of B4C in SiC, demonstrated to be at ~0.26 wt%. To investigate the …

    gatech Repository record for Sintering methodologies for silicon carbide ceramics (opens in a new tab)

  10. A Study of Indentation Cracking in Brittle Materials Using Cohesive Zone Finite Elements

    … zone finite element simulations of pyramidal indentation cracking in brittle materials have been carried out in order to: (1) critically examine indentation cracking models that relate fracture toughness to indentation data; (2) determine the underlying physical mechanisms of indentation crack …

    utk-theses Repository record for A Study of Indentation Cracking in Brittle Materials Using Cohesive Zone Finite Elements (opens in a new tab)

  11. Mechanical Properties of Brittle Ceramics: Case Study of Boron Rich Ceramics and Acropora cervicornis Coral Skeleton

    … a strength of 3.56 ± 0.31 GPa obtained through Vickers indentation. Finite element models were developed and validated against experimental results for the ZrB2- 30wt%SiB6 and Acropora cervicornis coral skeleton.

    ucf Repository record for Mechanical Properties of Brittle Ceramics: Case Study of Boron Rich Ceramics and Acropora cervicornis Coral Skeleton (opens in a new tab)

  12. Effect of ceramic density and curing pressure on properties of a resin infused alumina

    … profilometer. Hardness was measured using a Vickers hardness test using Instron-produced indentations at 15 newton load for 30 seconds. Young’s modulus was measured by compressive Young’s modulus method using the Instron machine at 0.5 mm/min crosshead speed. Fracture toughness was measured …

    bu Repository record for Effect of ceramic density and curing pressure on properties of a resin infused alumina (opens in a new tab)

  13. Structure evolution and mechanical properties of ion-exchanged silicate glass

    … against forming surface cracks was studied by Vickers hardness and scratch test. To study the structural evolution, micro-Raman (μ-Raman) spectroscopy was used. The results pointed out that below addition of 0.5 wt% NaNO3, the ion-exchange process is always effective. Indeed, compressive …

    trento Repository record for Structure evolution and mechanical properties of ion-exchanged silicate glass (opens in a new tab)

  14. Novel effects on the fracture strength of poly-crystalline silicon wafers

    … on initially indented specimens by means of Vickers indentation, to simulate surface defects. The mechanical fatigue has been carried out by ball-on-ring test setting with a BOSE equipment of 3kN loading cell, and the number of cycles at crack initiation has been recorded. Optical microscopy …

    unsw Repository record for Novel effects on the fracture strength of poly-crystalline silicon wafers (opens in a new tab)

  15. Mechanical characterization of hydroxyapatite, thermoelectric materials and doped ceria

    … of porosity. The hardness was evaluated by Vickers indentation technique as a function of porosity. The results of the mechanical property versus microstructure relations obtained in this study are of great importance for the design and fabrication of reliable components with service life …

    msu

  16. The 3D Characterisation Of Microscale Indentations On Silicon Nitride

    … Investigations into low load (0.5 kg and 1 kg) Vickers micro-indentations on silicon nitride are first carried out to ascertain which techniques are most applicable to evaluation of star features. This includes the determination of key microstructural parameters including microstructure, …

    whiterose Download PDF for The 3D Characterisation Of Microscale Indentations On Silicon Nitride (opens in a new tab)

  17. Characterisation and Evaluation of Thermally Treated Recycled Glass for Mass Finishing and Superfinishing Processes

    … A study concerned with the tip geometry of the Vickers and Berkovich indenters was completed to ensure an accurate contact area determination. A new method is proposed for the determination of contact area based on residual imprint measurements using 3-D optical profilometry. The outcomes show …

    liverpool-jm Repository record for Characterisation and Evaluation of Thermally Treated Recycled Glass for Mass Finishing and Superfinishing Processes (opens in a new tab) Download PDF for Characterisation and Evaluation of Thermally Treated Recycled Glass for Mass Finishing and Superfinishing Processes (opens in a new tab)

  18. Electrophoretic Deposition (EPD) of Ceramics

    … submitted to preliminary mechanical testing: Vickers indentation and nanoindentation. Scanning electron microscopy (SEM) investigations revealed different types of interfaces in the layered ceramic constructs. The layer quality depends upon the particle size of the electrophoretically …

    fu-berlin Repository record for Electrophoretic Deposition (EPD) of Ceramics (opens in a new tab)

  19. Residual stresses, cracking and stress intensity factors for vickers indentations in ceramics

    <p>Vickers hardness indentations on AI<sub>2</sub>O<sub>3</sub> were studied comprehensively. Beneath indentation, there is a well-defined interface between the plastic zone and the elastic region and the radius of the plastic zone is close to half the indentation diagonal length. The residual …

    oxford Repository record for Residual stresses, cracking and stress intensity factors for vickers indentations in ceramics (opens in a new tab)

Page 1 of 2