Global ETD Search
Search theses and dissertations gathered from participating repositories worldwide. Every result links back to the library that holds it. No account is needed.
Results
Showing 1 to 20 of 38 for “"WE43"”.
-
Dissimilar Joining of Al (AA2139) – Mg (WE43) Alloys Using Friction Stir Welding
… join aluminum alloy AA2139 and magnesium alloy WE43. The 9.5 mm thick plates of AA2139 and WE43 were friction stir butt welded. Different processing parameters were used to optimize processing parameters. Also, various weldings showed a crack at interface due to formation of IMCs caused by …
-
Povrchová úprava 3D tištěných struktur z Mg slitiny WE43 pro zvýšení korozní odolnosti
… a korozního chování 3D tištěné hořčíkové slitiny WE43 připravené metodou SLM. Na povrchu tištěné struktury se nacházely ulpělé částice a resublimovaný hořčík, což vedlo ke zvýšené drsnosti a otevřené pórovitosti. Pro odstranění povrchových nečistot a nenatavených částic prášku z povrchu struktury …
-
Microstructure and Mechanical Properties of WE43 Alloy Produced Via Additive Friction Stir Technology
… Stir (AFS) fabrication was used to fabricate WE43 magnesium alloy, with both atomized powder and rolled plate as filler material, into multilayered structures. It was found that the WE43 alloy made by AFS exhibited nearly isotropic tensile properties. With aging these properties exceeded the …
-
Modeling of Fracture Toughness of Magnesium Alloy WE43 Before and After Friction Stir Processing
… the fracture toughness of a magnesium alloy WE43 before and after friction stir processing (FSP) is developed, and the results are compared to those produced by a digital image correlation (DIC) system during an experiment from another paper. The model results of the material before FSP …
-
Rázové namáhání mikro-prutových struktur vyrobených technologií Selective Laser Melting z hořčíkové slitiny WE43
Mikro-prutové struktury ze slitiny WE43 se díky své pevnosti a nízké hmotnosti jeví jako možné řešení v oblasti biomedicíny i letectví. Doposud provedený výzkum posuzoval hlavně chování těchto struktur při kvazistatickém zatěžování. Dynamické namáhání těchto struktur doposud nebylo hluboce …
-
Příprava a charakterizace fluoridového povlaku na 3D tištěné hořčíkové slitině WE43 pro zvýšení korozní odolnosti
… zaměřuje na povrchovou úpravu hořčíkové slitiny WE43 vyrobené metodou selektivního laserového tavení (SLM). Cílem bylo charakterizovat povrchovou strukturu pomocí rastrovacího elektronového mikroskopu (SEM), odstranit reziduální nespečený prášek z povrchu tištěných součástí a připravit ochranný …
-
Langzeitbeobachtung der Degradation von WE43-basierten Osteosyntheseplatten und -schrauben mit und ohne PEO-Oberflächenmodifikation im Großtiermodell
… dass die Degradation der PEOmodifizierten WE43-Schrauben im Vergleich zu den nicht modifizierten Schrauben nach sechs Monaten signifikant verlangsamt und eine höhere Qualität des umliegenden Knochens vorhanden war. In der vorliegenden Studie wurden Osteosyntheseplatten und -schrauben aus …
-
Vergleich von Osteosyntheseplatten aus Titan und WE43-PEO-oberflächenmodifiziertem Magnesium zur sekundären Knochenheilung des Os frontale am Schaf
… Neben anderen zeigte die Magnesiumlegierung WE43 mit einer Plasma-elektrolytischen Oxidation (PEO) als Oberflächenmodifikation vielversprechende Ergebnisse in in-vitro- und in-vivo-Experimenten. In der aktuellen Studie wurden standardisierte Miniplatten aus dieser Legierung als …
-
6- und 12-Monats-Ergebnisse des Vergleichs zwischen PEO-oberflächenmodifizierten und WE43-basierten Magnesiumimplantaten ohne Oberflächenmodifikation im Schweinemodell
… und der Einfluss auf den umliegenden Knochen von WE43-basierten Magnesiumimplantaten mit und ohne PEO-Oberflächenmodifikation im Langzeitversuch untersucht. Es erfolgte die Implantation von Miniplatten in Humerus und Femur von Göttinger Minipigs und die Entnahme nach einer Standzeit von 6 und 12 …
-
Effects of Microstructure and Alloy Concentration on the Corrosion and Tribocorrosion Resistance of Al-Mn and WE43 Mg Alloys
… on these observations. Magnesium alloys such as WE43 are considered for biomedical applications including cardiovascular stents and bone implants due to their biocompatibility, good cell adhesion, and mechanical properties close to that of bones. Unfortunately, their high degradation rate and …
-
Understanding Solidification Behavior of Selected Aluminum and Magnesium Alloys Additively Manufactured by Laser Powder Bed Fusion
… utilized to evaluate the high strength Mg-alloy, WE43, important for application in lightweight structural components including use as bioresorbable prosthetic implants. Through exhaustive demonstration, dense WE43 parts with good strength and ductility were repetitively produced with AM. …
-
Microstructure for Enhanced Plasticity and Toughness
… FSP was utilized to affect the toughness of WE43 sheets through microstructural modification. Room temperature Kahn-type tests were conducted to measure the toughness of WE43 sheets. Microscopic techniques (SEM, TEM) was utilized to study the effect of various microstructural factors like …
-
Understanding the process-structure-property relationship of lightweight aerospace alloys processed using additive friction stir deposition.
… (PSP) relationship of magnesium alloy WE43 and aluminum alloy 7020, through in-depth characterization of the resulting microstructure and mechanical properties post AFSD processing. The first work on the PSP relations of AFSD processed magnesium alloy WE43 is focused on the …
-
Ductile Fracture of Magnesium Alloys: Characterization and Modeling
… and theoretically, in two Mg alloys, AZ31 and WE43. Material AZ31 exhibits strong basal texture whereas WE43 has a weak non-basal texture with quasiisotropic properties. The microstructural characterization is carried out on the initial materials aiming at determining the texture, the grain …
-
Corrosion behaviour of a biodegradable rare-earth magnesium alloy in modified simulated body fluid
… 4 examines the chemical degradation of Mg alloy WE43 in modified simulated body fluids, revealing that glucose and BSA influence the corrosion rate and formation of corrosion products. Higher glucose concentrations reverse the inhibitory effect of BSA by competitively displacing BSA from binding …
-
Influence of biodegradable Mg-based implants on bone nanoadaptation
… Mg-Ca-Zn (ZX00), Mg- rare earth elements (WE43), and pure Mg—compared to titanium, using synchrotron techniques (XRD, SAXS, XRF, XRD-CT), along with histology and mechanical testing. ZX00 altered the hydroxyapatite lattice, reducing crystallite size and platelet thickness near the implant, …
-
Development and Characterisation of Bioactive Coatings for Magnesium-based Medical Implants: Enhancing Corrosion Resistance and Biofunctionality in Skeletal Repair Applications
… OCP layer. In subsequent research, a 3D-printed WE43 Mg alloy, considered commercially available and clinically utilised, was examined, and novel CaP-phosphoserine (PS) composite coatings were explored to overcome the challenge of low CaP coating adhesion on its surface. The incorporation of a PS …
-
Imaging magnesium-based implants and their biological surroundings
… and plasma electrolytic oxidation (PEO)-treated WE43 screws in sheep bone. PEO-treated implants promote healthier lacunar shapes, while untreated ones yield a more connected LCN, potentially enhancing trauma response. The second study assesses MRI artefacts caused by Mg implants through in vitro, …
-
Mechanical and Corrosion Response of Friction Stir Extruded Magnesium Alloys
… the metal into a rod in single-stage processing. WE43, an important Mg alloy, was selected as a model material in this study. WE43 is already being used in the transportation sector, such as in helicopter transmissions and aero-engines. Also, due to its proven biocompatibility, it has the …
-
Influence of Surface Coating on the Degradation Properties of Metallic Orthopaedic Implants
… coating and apply it to magnesium alloy WE43 specimens using an immersion method, then investigate the degradation of the coated implants in simulated physiological conditions. Octacalcium phosphate was synthesised using the dropwise addition of calcium acetate monohydrate to a sodium …
Page 1 of 2