Global ETD Search

Search theses and dissertations gathered from participating repositories worldwide. Every result links back to the library that holds it. No account is needed.

Results 1 to 20 of 37 for “"Weak Adhesion"”

  1. Effect Of Weak Adhesion Interface On Mechanical And Dielectric Properties Of Composite Materials

    … of the composite structure as it can become the “weak link”. Adhesive bonding has wide applications in different disciplines including bio-medical, energy, automotive, civil and aerospace structural composites. With growing popularity of adhesive bonding, manufacturing defects at the interfaces of …

    south-carolina Repository record for Effect Of Weak Adhesion Interface On Mechanical And Dielectric Properties Of Composite Materials (opens in a new tab)

  2. Transport behavior and weak adhesion of quantum confined epitaxial Bi and Bi1-xSbx films

    … on Si (111) through the measurement of their weak adhesion to the Si (111) substrate as well as the identification of (012) oriented crystal growth of Bi1-xSbx and the effect of this crystal structure transition on the transport properties of the films. Finally, we report the development of a …

    texas Repository record for Transport behavior and weak adhesion of quantum confined epitaxial Bi and Bi1-xSbx films (opens in a new tab)

  3. Incommensurate Heteroepitaxy by van der Waals and Weak Chemical Interactions for Epitaxial Thin Film Transfer

    … the spontaneous van der Waals epitaxy, driven by weak chemical interaction, of a three-dimensional material on a three-dimensional material system. Despite a 3.7% lattice mismatch, high quality CdTe can be heteroepitaxially deposited on α-Al2O3 but with an incommensurate interface which …

    mcmaster Repository record for Incommensurate Heteroepitaxy by van der Waals and Weak Chemical Interactions for Epitaxial Thin Film Transfer (opens in a new tab)

  4. Phase transitions, transfer and nanoscale growth of epitaxial Bi and Bi1-xSbx thin films

    … 1-x] Sb [subscript x] films exhibit surprisingly weak adhesion to the Si(111) growth substrate, which may originate from the early allotropic transition. This weak adhesion enables the straightforward transfer of these films, opening a route toward the integration of epitaxial-quality Bi and Bi …

    texas Repository record for Phase transitions, transfer and nanoscale growth of epitaxial Bi and Bi1-xSbx thin films (opens in a new tab)

  5. Analysis of the Interface Properties of Multi-material 3D Printed Structures

    … applications. However, MM3DP structures have weak adhesion at the boundary interface. So, the interface characteristics in those structures are a critical factor in determining the strength of the structures and predicting failure. Digital image correlation (DIC) is a full-field strain …

    york Repository record for Analysis of the Interface Properties of Multi-material 3D Printed Structures (opens in a new tab)

  6. Patterning and adhesion characterization of mettalization for a microelectronics packaging application

    … THAT THE GRAFTED 4VP POLYMER SERVES AS A GOOD ADHESION PROMOTION LAYER IN ADDITION TO SERVING AS A PROMOTION LAYER FOR THE ELECTROLESS PLATING PROCESS. THE SECOND PART IS FOCUSED ON THE FABRICATION AND ADHESION CHARACTERIZATION OF FOUR TYPES OF UNDER BUMP METALLIZATIONS (UBMS) (A) CU …

    nus Repository record for Patterning and adhesion characterization of mettalization for a microelectronics packaging application (opens in a new tab)

  7. Development of a solid polymer electrolyte sensor for transcutaneous oxygen monitoring

    … technical problems of limited reaction sites and weak adhesion at the gold-Nafion interface.

    ohiolink Repository record for Development of a solid polymer electrolyte sensor for transcutaneous oxygen monitoring (opens in a new tab)

  8. Adhesion Strength Measurement of Multilayer Structures with Vertical Crack by Four Point Bending Test

    … packages consist of multilayer systems. Adhesion strength is one of the most important factors to the reliability of these systems. Previous studies have used four point bending tests as a method for characterizing the energy release rate to obtain the adhesion strength of bilayer …

    maryland Repository record for Adhesion Strength Measurement of Multilayer Structures with Vertical Crack by Four Point Bending Test (opens in a new tab)

  9. REVERSIBLY SWITCHING ADHESION OF SMART ADHESIVES INSPIRED BY MUSSEL ADHESIVE CHEMISTRY

    … a reduced state under acidic conditions to being weakly adhesive in an oxidized state under basic conditions. Here, we exploit this pH responsive behavior of catechol and demonstrate that its oxidation state can be manipulated by incorporation of boronic acid to facilitate reversible transitions …

    mtu Repository record for REVERSIBLY SWITCHING ADHESION OF SMART ADHESIVES INSPIRED BY MUSSEL ADHESIVE CHEMISTRY (opens in a new tab)

  10. Novel roles of the L-selection receptor on lymphocytes in cell division and signal transduction

    … mechanism involving the initial contact, adhesion, and transmigration of leukocytes through layers of endothelial cells into the surrounding tissue. L-selectin is the peripheral lymph node homing receptor mediating the initial interaction and weak adhesion between lymphocytes and …

    mcgill Repository record for Novel roles of the L-selection receptor on lymphocytes in cell division and signal transduction (opens in a new tab)

  11. Alteração de moléculas de adesão no ceratocisto odontogênico

    … recurrence rate that may be associated with a weak adhesion between cell-cell and cell- extracellular matrix (ECM), causing tissue fragmentation and allowing cells to detach during surgical intervention. A previous proteomic analysis identified alterations in proteases (CTSD), …

    brazil-ufmg Repository record for Alteração de moléculas de adesão no ceratocisto odontogênico (opens in a new tab)

  12. Development of Ni(OH)2 based hybrid nanomaterials for energy storage and conversion applications

    … electrochemical active sites and improve the adhesion of the Ni(OH)2 nucleation process to the graphene substrate. It solves the poor catalytic stability attributed to the weak adhesion between catalysts and the conductive substrate.

    unsw Repository record for Development of Ni(OH)2 based hybrid nanomaterials for energy storage and conversion applications (opens in a new tab)

  13. Influência da quantidade de absorção de água nas propriedades mecânicas de compósitos poliméricos de manta de fibra de vidro, híbrido e tecido juta

    … and thus the presence of moisture, results in a weak adhesion with most arrays and consequently a negative effect on the mechanical properties of these composites. One way to obtain products with desired properties is the hybridization, by setting composites containing layers of natural and …

    brazil-ufrn Repository record for Influência da quantidade de absorção de água nas propriedades mecânicas de compósitos poliméricos de manta de fibra de vidro, híbrido e tecido juta (opens in a new tab)

  14. PHOTOCATALYTIC REGENERATION OF GRANULAR ACTIVATED CARBON SATURATED WITH SULFUR DIOXIDE

    … activated carbon during regeneration, indicating weak adhesion between the particles and the surface. As a result, attachment by chemical bonds was then explored using a hydrothermal synthesis technique. In material TGAC-6, a nano-scale uniform coating was achieved when using activated carbon …

    hawaii Repository record for PHOTOCATALYTIC REGENERATION OF GRANULAR ACTIVATED CARBON SATURATED WITH SULFUR DIOXIDE (opens in a new tab)

  15. Asymmetric Complementary Interface for Enhanced Directional Adhesion

    … structured interfaces have been shown to enhance adhesion by trapping crack propagation along the interface. To propagate the trapped crack, more energy input is required externally and therefore the effective fracture toughness is increased. In many applications, directional adhesion is desired …

    alberta Repository record for Asymmetric Complementary Interface for Enhanced Directional Adhesion (opens in a new tab)

  16. Thiol material selection for better adhesion and reliability for copper/epoxy interface

    … issues. Especially delamination, such as the weak adhesion between copper substrate and epoxy encapsulation, is prone to happened in high temperature and high moisture environment typified by the ageing test undergone by integrated circuit packages.</p><p>In order to solve this problem, …

    hkust Repository record for Thiol material selection for better adhesion and reliability for copper/epoxy interface (opens in a new tab)

  17. Synthesis and characterization of Ta-DLC coatings over CoCrMo alloy

    … to their high internal stresses, which induces weak adhesion and early delamination of the coatings. Metal doping has been widely researched to enhance the adhesion of DLC, but limited research has been done on Tantalum (Ta) doping and its effect on the structural, chemical, mechanical and …

    sask Repository record for Synthesis and characterization of Ta-DLC coatings over CoCrMo alloy (opens in a new tab)

  18. Chemical vapor deposition of diamond thin films on titanium silicon carbide

    … are very difficult and slow. Furthermore, the weak adhesion between the diamond thin films and substrates has been a major problem for widespread application of diamond thin films. Up to now, Si has been the most frequently used substrate for the study of diamond thin films and various methods, …

    sask Repository record for Chemical vapor deposition of diamond thin films on titanium silicon carbide (opens in a new tab)

  19. Composite coils : compliant in-vivo tissue fixation device

    … (drug delivery) are known advantages, but weak adhesion strength in the wet environment and lack of tissue compliant behavior still pose a challenge. In order to address these issues, non-aqueous bioadhesive based on blends of polyamidoamine (PAMAM) dendrimer, conjugated with …

    nanyang Repository record for Composite coils : compliant in-vivo tissue fixation device (opens in a new tab)

  20. Collector transfer between bubble and particle by collision

    … on bubbles. This result was attributed to the weak adhesion of the precipitate to the quartz particles and the detachment of the precipitate from both bubbles and quartz particles as bubbles coalesced and burst in the froth zone. Interaction with quartz and bubbles was further weakened by the …

    ubc Repository record for Collector transfer between bubble and particle by collision (opens in a new tab)

Page 1 of 2