Global ETD Search

Search theses and dissertations gathered from participating repositories worldwide. Every result links back to the library that holds it. No account is needed.

Results 1 to 17 of 17 for “"Zn coating"”

  1. Soil and pitting corrosion of hot-dip galvanized steel : experimental and mathematical modeling

    … many atmospheric and underground conditions. The Zn coating protects the carbon steel substrate via the formation of a passive layer and by providing a sacrificial anode. Transmission towers are designed to last decades and the slow corrosion rate of the Zn coating plays an important role in …

    ubc Repository record for Soil and pitting corrosion of hot-dip galvanized steel : experimental and mathematical modeling (opens in a new tab)

  2. Aging effects on sheared edge formability

    … testing burr up and burr down. To investigate Zn coating effects on aging sensitivity, aging effects were measured for DP 800 specimens produced in an annealing/galvanizing simulator with the same thermal history and different coating and atmosphere conditions. No consistent microstructure or …

    colo-mines Repository record for Aging effects on sheared edge formability (opens in a new tab)

  3. Zinc-Magnesium and Zinc-Aluminium- Magnesium Coatings Produced by Magnetron Sputtering and Melt Dipping

    Zn coating is the most economic and widely used sacrificial coating to protect steels against corrosion. Since the corrosion resistance of pure Zn coating is not satisfactory under alkaline or high humidity environments, over the past few decades, demands for better corrosion resistance and …

    auckland-ms Repository record for Zinc-Magnesium and Zinc-Aluminium- Magnesium Coatings Produced by Magnetron Sputtering and Melt Dipping (opens in a new tab)

  4. Process optimization of Gas Metal Arc Brazing technology

    … process used in the joining of thin-gauge Zn-coated advanced high strength steels (AHSSs) employed in the automotive industry. Due to its lower heat input capability, the technology offers several benefits over the conventional gas-metal-arc welding (GMAW) process such as minimal Zn-coating …

    waterloo Repository record for Process optimization of Gas Metal Arc Brazing technology (opens in a new tab)

  5. On the Origin of Micro-Cracking in Zn-Coated Press Hardened Steels

    Zn-coated press hardened steels are in high demand in the automotive industry because their high strength enhances passenger safety while supplying cathodic corrosion protection. However, micro-crack formation after thermomechanical processing is an issue that limits full deployment. One of the …

    mcmaster Repository record for On the Origin of Micro-Cracking in Zn-Coated Press Hardened Steels (opens in a new tab)

  6. ATOMISTIC SIMULATION AND FIRST PRINCIPLES CALCULATION OF INTERFACIAL ENERGETICS OF GALVANIZED ADVANCED HIGH STRENGTH STEELS

    … subsequent hot-dipping of the steel into liquid Zn bath to form a Zn coating. During hot-dipping, complex metallurgical reactions happen. As a result, a Zn coating consisting of inhibition layer, Fe-Zn intermetallics and Zn overlay forms. The oxides formed during annealing will influence the …

    unr Repository record for ATOMISTIC SIMULATION AND FIRST PRINCIPLES CALCULATION OF INTERFACIAL ENERGETICS OF GALVANIZED ADVANCED HIGH STRENGTH STEELS (opens in a new tab)

  7. Corrosion Risk Assessment System For Coated Pipeline System

    … of structure. To mitigate the corrosion attacks, coatings are generally applied to protect steel pipelines against corrosion and improve durability of the associated structures for longer service life. Although have higher corrosion resistance, coated pipelines will still get corroded in a long …

    ndsu Repository record for Corrosion Risk Assessment System For Coated Pipeline System (opens in a new tab)

  8. Introduction of the Concept of a Time-Based Threshold of Galvanized Steel in Simulated Concrete Pore Solution Based on Short- and Long-Term Immersion

    … When you galvanize instead of painting or coating something, a metallic link is formed between the zinc and the steel substrate of the rebar. The coating’s integrity stays mostly the same even if it gets damaged during shipping, storage, or use. The steel surface is protected on two …

    tamu Repository record for Introduction of the Concept of a Time-Based Threshold of Galvanized Steel in Simulated Concrete Pore Solution Based on Short- and Long-Term Immersion (opens in a new tab)

  9. Liquid Metal Embrittlement in Resistance Spot Welding: The Thermomechanical Origin and Embrittler Transport Mechanism

    … and ductility. AHSS are often coated with zinc (Zn) to prevent corrosion, however the coating can lead to several complications, such as liquid metal embrittlement (LME). Resistance spot welding (RSW), a common automotive process, has been observed to accentuate LME cracking. During RSW, the heat …

    waterloo Repository record for Liquid Metal Embrittlement in Resistance Spot Welding: The Thermomechanical Origin and Embrittler Transport Mechanism (opens in a new tab)

  10. Investigation of Liquid Metal Embrittlement in Advanced High Strength Steels

    … steels (AHSS) are typically given a zinc coating that provides excellent resistance to corrosion. During the resistance spot welding (RSW) process, the melted zinc coating enables liquid metal embrittlement (LME) where the liquid zinc, acting as an embrittling agent, induces cracking in …

    waterloo Repository record for Investigation of Liquid Metal Embrittlement in Advanced High Strength Steels (opens in a new tab)

  11. Resistance Spot Welding of Al to Mg with Different Interlayers

    … specifically pure Ni foil, Au-coated Ni foil and Zn-coated were investigated in details. While only brief investigation of joints made with Sn-coated steel, Zn foil, and Cu foil interlayers was conducted. No joints were achieved with a bare Ni interlayer during Al to Mg alloy resistance spot …

    waterloo Repository record for Resistance Spot Welding of Al to Mg with Different Interlayers (opens in a new tab)

  12. Production and Characterization of Zn-Ni Nano-Composite Coatings Using Sol-Enhanced Electrodeposition Method

    Zn-Ni coatings provide sacrificial corrosion protection for steel components and are widely used by automotive manufacturers and fasteners industries in particular. It has been reported that Zn-Ni coatings with single γ-Ni5Zn21 phase structure and Ni content in the range of 10-14 wt.% possess five …

    auckland-ms Repository record for Production and Characterization of Zn-Ni Nano-Composite Coatings Using Sol-Enhanced Electrodeposition Method (opens in a new tab)

  13. Advanced Laser Weld Brazing of Zinc-Coated Automotive Steels: Process Optimization for AI-Enhanced Inspection, Tailored Intermetallic Formation, and the Evolution of Mechanical Behavior

    … minimal substrate melting, reduced Zinc (Zn) coating burn-off, and superior joint appearance. However, challenges such as sub-surface defect formation and intermetallic compound (IMC) embrittlement hinder its optimization and broader adoption. Due to LWB's relative novelty for Zn-coated …

    waterloo Repository record for Advanced Laser Weld Brazing of Zinc-Coated Automotive Steels: Process Optimization for AI-Enhanced Inspection, Tailored Intermetallic Formation, and the Evolution of Mechanical Behavior (opens in a new tab)

  14. Effect of Coating Microstructure on the Electrochemical Properties of Continuous Galvanized Coatings on Press Hardened Steels

    … Automotive OEMs have expressed a desire to use Zn-based coatings as they are compatible with the current painting system and have the potential to provide robust cathodic protection. The steel blanks generally undergo direct hot press forming (DHPF) to achieve the necessary martensitic …

    mcmaster Repository record for Effect of Coating Microstructure on the Electrochemical Properties of Continuous Galvanized Coatings on Press Hardened Steels (opens in a new tab)

  15. SELECTIVE OXIDATION AND REACTIVE WETTING OF FE-0.1C-6MN-2SI-xSN ADVANCED HIGH STRENGTH STEELS DURING CONTINUOUS HOT-DIP GALVANIZING

    … step prior to immersion in the galvanizing Zn(Al, Fe) bath, as extensive coverage of the substrate surface by these oxides is detrimental to reactive wetting, good coating adhesion and integrity. Simulated galvanizing treatments were conducted on two prototype Fe-0.1C-6Mn-2Si (wt pct) 3G …

    mcmaster Repository record for SELECTIVE OXIDATION AND REACTIVE WETTING OF FE-0.1C-6MN-2SI-xSN ADVANCED HIGH STRENGTH STEELS DURING CONTINUOUS HOT-DIP GALVANIZING (opens in a new tab)

  16. L'électrochimie et désalliage de Zn-Mg/Al-Zn phase pures et l'importance sur la corrosion de l'alliage Zn-Al-Mg

    … pures, composants des alliages de revêtement Zn-Al-Mg. Les données électrochimiques ont été utilisées pour prédire du comportement à la corrosion des revêtements d’alliage multiphasé. A cette fin, une base de données de courbes de polarisation élémentaire a été établie en fonction du pH en …

    star-france Repository record for L'électrochimie et désalliage de Zn-Mg/Al-Zn phase pures et l'importance sur la corrosion de l'alliage Zn-Al-Mg (opens in a new tab)