Global ETD Search
Search theses and dissertations gathered from participating repositories worldwide. Every result links back to the library that holds it. No account is needed.
Results
Showing 1 to 20 of 25 for “"austempering"”.
-
Development Of High Strength High Toughness Third Generation Advanced High Strength Steels.
… were subjected to single step and two step austempering in the temperature range of 260-399oC to obtain desired microstructures and mechanical properties. Austempering heat treatment was carried out for 2 hours in a molten salt bath. The microstructures were characterized by X-ray …
-
Fatigue analysis of austempered ductile iron suitable for automotive camshaft applications
… one produced by austenitising at 800°C and austempering at 260°C, one by austenitising at 800°C and austempering at 390°C, and the other by austenitising at 900°C and austempering at 390°C. The duration for austenitisation and austempering was two hours. The present results have been …
-
Investigation of bainitic phase transformation and phase evolution during tempering of high strength medium carbon steels
… investigated under both continuous cooling and austempering conditions. For the manufacturing of small steel blocks, continuous cooling followed by double tempering was replaced with the conventional austempering process followed by a single tempering cycle. Experimental results from both …
-
Hole expansion of retained austenite containing CMnSi bainitic/martensitic steels
Austempering and Quenching & Partitioning steels are two processing approaches that may produce third generation advanced high strength steel properties, which are attractive to the automotive industry. Three 0.25C-2Mn-(1.5, 0.6, and 0.1)Si steels were austenitized and subsequently isothermally …
-
Heat treating response of 0.6 C steels for saw chain applications
… range of interest for current saw chain steels. Austempering, quenching and tempering (Q&T), and quenching and partitioning (Q&P) (9260 only) processing methods were simulated. For Q&P processing, the volume fraction of retained austenite decreased with time at higher partitioning temperatures, …
-
Effects of refrigeration and cryogenic treatments on austempered ductile iron
… treated by a series of sub-zero temperatures and austempering cycles at commercial treatment facilities. These specimens were then returned to the university and were subjected to a series of mechanical tests that included tensile and hardness property testing. After analysis of the data, it was …
-
The kinetics of austenite formation during continuous heating of a multi-phase steel
… annealing, followed by subsequent cooling and austempering. The material is first intercritically annealed in the ferrite/ austenite coexistence region, during which the ferrite matrix recrystallizes and austenite is created. Austempering is then performed and some upper bainite is formed, …
-
A Novel Two Step Austenitization Process To Produce Austempered Ductile Iron (adi) With High Strength, Ductility And Fracture Toughness
… fully austenitic temperature range followed by austempering in the bainitic temperature range. This heat treatment was expected to result in a microstructure consisting of proeutectoid ferrite, very fine scale bainitic ferrite, and high-carbon austenite. Tensile and CT test specimens were …
-
Development Of Nanostructured Austempered Ductile Cast Iron
… the same austenitizing temperature followed by austempering. The investigation also examined the effect of cryogenic treatment, effect of intercritical austenitizing followed by single and two step austempering, effect of high temperature plastic deformation on the microstructure and mechanical …
-
Hydrogen embrittlement of 4340 with martensitic and bainitic microstructures for fastener applications
… 4340 was processed via quench and tempering, austempering, and austempering and tempering to achieve martensitic, bainitic, and tempered bainitic microstructures. Bulk hardness, smooth-sided, and notched round bar tensile testing were used to evaluate mechanical properties, while dilatometry, …
-
IMPROVED ROLLING CONTACT FATIGUE OF DUCTILE IRON UTILIZING CHILLS AND CHROMIUM ADDITIONS
… surface hardness through induction hardening, austempering, and chill casting. These procedures produce drastically different iron microstructures, so common RCF microstructural failure mechanisms have not been observed. Chill casting produces a white iron structure with high hardness and wear …
-
Effect of Elemental Additions on the Microstructure, Macrostructure, and Mechanical Properties of Gray iron
… addition as a baseline. The use of a Direct Austempering After Solidification (DAAS) heat treatment permitted austenite grain boundaries to be retained for macrographic analysis, and austenite grain morphology was correlated to tensile and fatigue properties of a gray iron. While most …
-
Machinability and microstructural studies on phase transformations in Austempered Ductile Iron
… subjected to heat treatments - austenitising and austempering. The heat treatment gives ADI its unique ausferrite microstructure through which ADI gets its advantageous material properties. Possibly the most significant hurdle for the engineering community to overcome, to fully realise the …
-
Influence of microstructure and retained austenite on the abrasive wear performance of bainitic 9260 and 6150 steels
… laths. The 6150 alloy formed lower bainite upon austempering heat treatments with visible inter- and intra-lath cementite. The Q&T microstructures featured tempered martensite laths with carbides both within and between these laths. The scratch test results showed that the Q&T microstructures …
-
Mechanical properties of steels with a microstructure of bainite/martensite and austenite islands
… martensite, and austenite an interrupted austempering heat treatment was used. Varying the heat treatment times and temperatures produced microstructures of varying amounts of bainite, martensite, and austenite. Mechanical properties such as strength, ductility, strain hardening, and …
-
Influence of microstructural variation on hydrogen embrittlement susceptibility of 9260 bar steel, The
… generated by quenching and tempering (Q&T), austempering, quenching and partitioning (Q&P), and prior austenite grain size (PAGS) refinement. The target hardness for all testing conditions was 52-54 HRC. All testing conditions were initially austenitized at 880 ºC for 20 min. The Q&T …
-
Improving self-pierce rivet performance through processing and alloy development
… performance after quenching and tempering, austempering and after being intentionally decarburized to varying degrees. The heat-treatments were evaluated through microscopy, fractography, rivet flaring and joining attempts for each case study and alloy under investigation. All of the …
-
Influence Of Dissolved Hydrogen On The Fatigue Crack Growth Behaviour Of Aisi 4140 Steel
… It is also observed that increasing the austempering temperature decreases the resistance to hydrogen embrittlement. An interesting phenomenon was also observed in annealed specimen charged with hydrogen for 250 h which had an unusually high fatigue threshold (ΔKth).
-
EVALUATION OF THERMAL STABILITY OF AUSFERRITE IN AUSTEMPERED DUCTILE IRON USING DIFFERENTIAL SCANNING CALORIMETRY
Austempered Ductile Iron (ADI) is prone to changes in microstructure and mechanical properties when exposed to elevated service temperatures. Differential Scanning Calorimetry has been used to evaluate the stabilizing effects of copper, nickel, molybdenum, and cobalt on the ausferrite structure. …
Page 1 of 2