Global ETD Search

Search theses and dissertations gathered from participating repositories worldwide. Every result links back to the library that holds it. No account is needed.

Results

Showing 1 to 2 of 2 for “"bare spot defects"”.

  1. Coating of High Strength Steels with a Zn-1.6Al-1.6Mg Bath

    … at 60 s, 100 s and 140 s at 800◦C. The resulting bare spot defects in the Zn-1.6 wt.% Al-1.6 wt.% Mg coating were assessed by means of SAM-AES and FIB, while coating adhesion was analysed by 180◦ bend tests. Annealing the steel substrates resulted in the formation of surface MnO, which varied …

    mcmaster Repository record for Coating of High Strength Steels with a Zn-1.6Al-1.6Mg Bath (opens in a new tab)

  2. Galvanization of Al-Si Trip-Assisted Steels

    … in TRIP steels; Mn, Si and Al, can result in bare spot defects and unacceptable coatings. Both of these issues have been investigated.</p> <p>Heat treatments compatible with continuous hot-dip galvanizing were performed on two high Al - low Si TRIP-assisted steels; one having 1.5% Al and the …

    mcmaster Repository record for Galvanization of Al-Si Trip-Assisted Steels (opens in a new tab)