Global ETD Search
Search theses and dissertations gathered from participating repositories worldwide. Every result links back to the library that holds it. No account is needed.
Results
Showing 1 to 20 of 44 for “"burnishing"”.
-
An analysis of the friction burnishing operation
To reduce the irregularities of machined surface, burnishing is used as a finishing process by the plastic deformation. This process does not only improve surface finish but also generates compressive residual stresses throughout the surface. In this investigation work mechanical (friction) …
-
The Effect of Weak Acid on the Stability of Burnishing Ink
By definition we find "An emulsion being a system containing two liquid phases, one of which is dispersed as globules in the other. That liquid which is broken up into globules is termed the dispersed phase, whilst the liquid surrounding the globules is known as the continuous phase or dispersing …
-
An analysis of the effect of ultrasonic burnishing on surface integrity
… strict quality and tolerance requirements. Burnishing is a process which produces a fine surface finish on a workpiece and commonly applied to improve the surface integrity, i.e. surface roughness, residual stress and hardness of a mechanical components. Burnishing has long been used in the …
-
Finite element modeling of cutting and burnishing processes at micro- and nanoscales
Micro/nano cutting and micro/nano burnishing processes are widely used in the field of manufacturing. Compared to their counterparts in the conventional scale, micro/nano cutting and burnishing processes have unique characteristics. First, there are various size effects, such as the edge radius, …
-
Process mechanics and surface integrity of low plasticity burnishing of SE508 Nitinol alloy
… functionality and performance. Low plasticity burnishing (LPB) is a surface enhancement process to improve surface integrity due to its unique capability to plastically deform material in the deep subsurface on the order of a 500-1000ìm. This thesis focuses on the dynamic mechanical behavior of …
-
CRYOGENIC MACHINING AND BURNISHING OF AZ31B MAGNESIUM ALLOY FOR ENHANCED SURFACE INTEGRITY AND FUNCTIONAL PERFORMANCE
… compressive residual stresses. Dry and cryogenic burnishing experiments of the same material were conducted using a fixed roller setup. The thickness of the processed-influenced layer, where remarkable microstructural changes occurred, was dramatically increased from the maximum value of 20 μm …
-
CRYOGENIC BURNISHING OF Co-Cr-Mo BIOMEDICAL ALLOY FOR ENHANCED SURFACE INTEGRITY AND IMPROVED WEAR PERFORMANCE
… the effect of a SPD process, cryogenic burnishing, on the surface integrity modifications of a Co-Cr-Mo alloy, and the resulting wear performance of this alloy due to the burnishing-induced surface integrity properties. A systematic experimental study was conducted to investigate the …
-
A STUDY ON BURNISHING AND SELF-PILOTING MECHANISM FOR HIGH PRECISION DEEP HOLE DRILLING OF INCONEL 718
… quality. We provide an analytical formulation of burnishing forces for gundrills with single and multi-pad configuration and a procedure to determine its self-piloting efficacy. Drill stability was categorized as positive, neutral, and negative based on the analytical model and the drill’s …
-
ENHANCED SURFACE INTEGRITY WITH THERMALLY STABLE RESIDUAL STRESS FIELDS AND NANOSTRUCTURES IN CRYOGENIC PROCESSING OF TITANIUM ALLOY TI-6AL-4V
Burnishing is a chipless finishing process used to improve surface integrity by severe plastic deformation (SPD) of surface asperities. As surface integrity in large measure defines the functional performance and fatigue life of aerospace alloys, burnishing is thus a means of increasing the fatigue …
-
Superior surface integrity by hybrid dry cutting-hydrostatic burnishing for controlled biofluid corrosion performance of novel biodegradable Magnesium-Calcium implants
… by-products. In this context, hybrid cutting-burnishing process has been utilized to tailor surface integrity of the Mg-Ca implants in such a way which results in gaining control on the corrosion kinetics. A synergistic numerical-experimental investigation was conducted to study process …
-
On-line optimisation and experimental design analysis for the investigations on the surface roughness produced by roller burnishing: a thesis submitted in partial fulfilment of the requirements for the degree of Master of Technology in Manufacturing and Industrial Technology at Massey University
… and plastic deformation process called roller burnishing. Roller burnishing is a popular finishing process. Surface finish has a positive and prolonged effect on the functioning of the machined parts. In this work roller burnishing is used to get a high quality surface finish on different …
-
Cryogenic Processing of <em>Al 7050-T7451</em> Alloy for Improved Surface Integrity
… friction stir processing (FSP), machining and burnishing, on Al 7050-T7451 alloy to solve the inhomogeneity issue and improve its surface integrity. FSP is applied to modify the microstructure of Al 7050-T7451 alloy for achieving more homogeneous structure with near ultra-fine grains (UFG) …
-
Φθορά κινητού ένθετου πολυαιθυλενίου σε ολική αρθροπλαστική γόνατος: κλινική και πειραματική μελέτη
… lesser extend are also present. Little wear of burnishing type and abrasions, develop after 5.5 years mainly in the posterior condyles and in the thin inserts is accompanied by fracture and loss of material. In all bearings, regardless of thickness there is no significant backside wear. 18% of …
-
A theoretical and experimental investigation of the BTA deep hole tool support in the machining zone
… small front-end area of the support pads where burnishing occurs. The study is to explain the inherent feature of the conventional self-piloting tool design to deflect the boring bar in 3D enough to make a difference between the effective area involved in burnishing and the area as designed.
-
Factors Affecting the Durability of 5.25 Inch Floppy Diskette Media and its Mechanisms of Wear
… surface roughnesses by varying the degree of burnishing. It has been found that the mechanisms of wear are related to a fatigue process. Some surprises have been noted in respect of the value of burnishing compared to the observations made elsewhere. Good reasons for these observed differences …
-
Characteristics of Material Removal by Ceramic Media on Metallic Coupons for Mass Finishing Applications
… operations such as polishing, descaling, burnishing, cleaning, and drying. Polishing, descaling, and burnishing are abrasive operations that remove or displace material on parts being processed to attain the expected effect. These material removal operations were idealized as a sequence o …
-
Pattern recognition using robust discrimination and fuzzy set theoretic preprocessing
… grades in place of the original feature. Burnishing tarnished gold standards compensates for the possible imprecision of a well-established reference test by adjusting, if necessary, the class labels in the design set while maintaining the test's vital discriminatory power. The …
-
Tribological Characterisation And Modelling Of Premium Tubular Connections
… that the initial surface topography and the burnishing in repeated sliding have significant effects on friction. iv In order to understand the correlation between the effects of initial surface roughness and burnishing during the sliding process on the coefficient of friction, a theoretical …
-
Abstractions of shapes and space.
… etching, machine engraving, scraping, burnishing, open bite, sugar lift, aquatint, and with several techniques for color printing. The project also involved a study of various media with the purpose of finding a technique as artistically satisfying as intaglio but less physically …
-
MATERIAL PERSPECTIVE AND CUTTING EDGE RADIUS EFFECT ON ULTRA-PRECISION MACHINING PROCESS
… and complete chip formations. Finally, ‘burnishing-like’ finishing regime has been identified by appraising the factors of machined surface integrity, compressive flow stress and improvement of nanometric surface finishing for different materials of Al alloy, Mg alloy and Cu alloy.
Page 1 of 3