Results 1 to 20 of 207 for “"capacity-fade"”

  1. Optimal Battery Operations and Design Considering Capacity Fade Mechanisms

    Safely and capacity fade are the key issues that restrict the use of the lithium-ion battery for many applications. These issues are being tackled in a variety of ways. This dissertation focuses on using detailed continuum-level electrochemical models to study transport, kinetics, and mechanical …

    wustl Repository record for Optimal Battery Operations and Design Considering Capacity Fade Mechanisms (opens in a new tab)

  2. Capacity Fade Studies in LixSi, LixGe, LixAl, and LixSn Electrodes

    … such as electric vehicles, requiring higher capacity, safety operation and portable energy storage. This has led to the investigation of possible anode materials such as Si, Sn, Al, and Ge materials, which forms stable intermetallic compound with lithium through several highly lithiated …

    ohiolink Repository record for Capacity Fade Studies in LixSi, LixGe, LixAl, and LixSn Electrodes (opens in a new tab)

  3. Capacity Fade Analysis and Model Based Optimization of Lithium-ion Batteries

    … stress-induced material damage, capacity fade, and the potential for thermal runaway. This dissertation contributes to the efforts in the modeling, simulation and optimization of lithium-ion batteries and their use in the design of better batteries for the future. While …

    wustl Repository record for Capacity Fade Analysis and Model Based Optimization of Lithium-ion Batteries (opens in a new tab)

  4. Studying On Capacity Fade Mechanisms of Li-Ion Batteries Through Modeling

    … based on an in-depth understanding of the fade mechanisms. The purpose of this dissertation is to explore, through a mathematical modeling approach, failure mechanisms of Li-ion batteries. To study the capacity fade of a LiMn2O4 (LMO) electrode, a pseudo-2 dimensional (P2D) model based on …

    south-carolina Repository record for Studying On Capacity Fade Mechanisms of Li-Ion Batteries Through Modeling (opens in a new tab)

  5. Capacity Fade Modeling for Convex Optimization of Battery Charge/Discharge Schedules

    … a battery is used, the more its energy capacity will degrade. This paper introduces a method for including and monetizing capacity fade costs into convex battery scheduling optimization so that they may be taken into account.

    washington Repository record for Capacity Fade Modeling for Convex Optimization of Battery Charge/Discharge Schedules (opens in a new tab)

  6. Investigation of capacity fade in flat-plate rechargeable alkaline MnO₂/Zn cells

    … phase formation and progressive and cumulative capacity fade. This system has many advantages however, such as low cost and environmentally sustainable materials, long shelf life, moderate energy density, and safety. A flat-plate architecture was developed and investigated in half and full-cell …

    ubc Repository record for Investigation of capacity fade in flat-plate rechargeable alkaline MnO₂/Zn cells (opens in a new tab)

  7. A hybrid battery cell voltage equalizer considering thermal behavior and capacity fade characteristics

    The thesis focuses on developing a robust, high-fidelity lithium-ion battery model adaptive to changes in operating temperature, aiming for accurate estimation of state of health (SOH). The thesis proposes two novel methods for lithium-ion battery SOH tracking and estimation using the developed …

    uoit Repository record for A hybrid battery cell voltage equalizer considering thermal behavior and capacity fade characteristics (opens in a new tab)

  8. Green synthesis and capacity fade mechanism of Lithium titanate nanosheet anode for Lithium-ion batteries

    … and (iv) understanding and controlling the capacity fade mechanism of nano-LTO upon cycling. The devised process is a two-step chemical/annealing process. Step 1 involves aqueous solution reaction of LiOH with TiCl4 at < 10 °C, Li/Ti = 1.3 and pH 11.5-12 to produce a hydrous precipitate, …

    mcgill Repository record for Green synthesis and capacity fade mechanism of Lithium titanate nanosheet anode for Lithium-ion batteries (opens in a new tab)

  9. Review of Capacity Fade Models for Lithium-ion Batteries -- Effect of Mechanisms on Numerical Implementation

    … and PHEVs, require long battery life. However, capacity fade always occurs due to unwanted side reactions including electrolyte oxidation at the positive electrode, lithium deposition at the negative electrode, electrolyte decomposition processes, and the formation of the Solid-Electrolyte …

    washington Repository record for Review of Capacity Fade Models for Lithium-ion Batteries -- Effect of Mechanisms on Numerical Implementation (opens in a new tab)

  10. Investigation into the Effect of Thermal Management on the Capacity Fade of Lithium-ion Batteries

    … leading to a fire hazard, and to minimize capacity fade for longer lifetime. In this research, the focus was on the effect of thermal management on the capacity fade of lithium-ion batteries. A battery thermal management system will impact the battery operation through its temperature, …

    waterloo Repository record for Investigation into the Effect of Thermal Management on the Capacity Fade of Lithium-ion Batteries (opens in a new tab)

  11. Modeling of the Solid-electrolyte Interface Layer of Lithium Ion Batteries for Capacity Fade Using Kinetic Monte Carlo

    … of Lithiumion batteries is used to study the capacity fade, ageing, and cycling life and provides significant information to ensure the battery safety. In this work, the model for SEI layer dynamics is developed using the Kinetic Monte Carlo approach, in which four major dynamical processes …

    sdstate Repository record for Modeling of the Solid-electrolyte Interface Layer of Lithium Ion Batteries for Capacity Fade Using Kinetic Monte Carlo (opens in a new tab)

  12. Understanding the capacity fade mechanisms of spinel manganese oxide cathodes and improving their performance in lithium ion batteries

    … benign, but LiMn₂O₄ is plagued by severe capacity fade at elevated temperatures. This dissertation explores the factors that control and limit the electrochemical performance of spinel LiMn₂O₄ cathodes and focuses on improving the performance parameters such as the capacity, cyclability, …

    texas Repository record for Understanding the capacity fade mechanisms of spinel manganese oxide cathodes and improving their performance in lithium ion batteries (opens in a new tab)

  13. DEGRADATION ANALYSIS OF LITHIUM-ION BATTERIES WITH KNEE POINTS

    … electric vehicles to become commonplace. The capacity, which has been used to determine if lithium-ion batteries have reached the end of life, decreases during usage (cycling) and storage (rest). After some charge-discharge cycles, the capacity fade rate has been observed to increase, and the …

    maryland Repository record for DEGRADATION ANALYSIS OF LITHIUM-ION BATTERIES WITH KNEE POINTS (opens in a new tab)

  14. Effects of Rest Time and Temperature on Graphite/LiCoO2 Battery Degradation

    … vehicles. These batteries degrade and lose their capacity, defined as the amount of charge the battery holds, as a result of charge–discharge operations and various degradation mechanisms. Degradation of lithium-ion batteries is affected by various operational and environmental conditions, …

    maryland Repository record for Effects of Rest Time and Temperature on Graphite/LiCoO2 Battery Degradation (opens in a new tab)

  15. A BAYESIAN NETWORK APPROACH TO BATTERY AGING IN ELECTRIC VEHICLE TRANSPORTATION AND GRID INTEGRATION

    … aging evaluation: First, the battery capacity fade factors such as temperature, cycling current, state of charge (SOC) … are dependent to the external variables such as location, vehicle owner’s behavior and availability of the grid connection. Therefore, it is not possible to …

    mtu Repository record for A BAYESIAN NETWORK APPROACH TO BATTERY AGING IN ELECTRIC VEHICLE TRANSPORTATION AND GRID INTEGRATION (opens in a new tab)

  16. Analysis of Battery Degradation Effects on Optimized Torque Splitting in Dual-Motor Electric Vehicles

    … behavior of the energy storage system through capacity fade and internal resistance growth. Capacity fade reduces the usable energy and vehicle range, while resistance growth increases voltage drop, current-related losses, and battery electrical loading. This thesis evaluates how these …

    wvu Repository record for Analysis of Battery Degradation Effects on Optimized Torque Splitting in Dual-Motor Electric Vehicles (opens in a new tab)

  17. Implications of Rapid Charging and Chemo-Mechanical Degradation in Lithium-Ion Battery Electrodes

    … life predictions are realized by developing a capacity fade model consisting of a coupled chemical (irreversible solid electrolyte interface formation) and mechanical (intercalation induced damage) degradation formalism with thermal effect. Primary results with conventional protocol at high …

    tamu Repository record for Implications of Rapid Charging and Chemo-Mechanical Degradation in Lithium-Ion Battery Electrodes (opens in a new tab)

  18. Morphological control of LiNi0.8Mn0.1Co0.1O2 cathodes for lithium-ion cells using biotemplating

    … of net-zero. NMC811, defined by a high specific capacity of >200 mAh/g but a poor capacity retention and structural stability, was synthesised using either dextran or sodium alginate, preheated at 300 °C for 2h and calcined at 800 °C using nitrate precursors or 850 °C using acetate precursors for …

    whiterose Repository record for Morphological control of LiNi0.8Mn0.1Co0.1O2 cathodes for lithium-ion cells using biotemplating (opens in a new tab)

  19. Regeneration of Lithium-Ion Cells

    … work, a study to investigate the potential for capacity regeneration of lithium-ion cells was initiated. The aim was to develop and validate a general non-invasive regenerative approach which in the long run could be implemented into the Volvo battery management system. Lithium-ion cells were …

    chalmers Repository record for Regeneration of Lithium-Ion Cells (opens in a new tab)

  20. Electrolyte/Membrane Design and Engineering for Durable Zinc-Iodine Redox Flow Batteries

    … low efficiency, and high cost. In addition, capacity fade and elusive operational instability over charge-discharge cycling severely hinder their large-scale commercialization of ZIFBs. This thesis focuses on the design and engineering of electrolytes and membranes for durable and low-cost …

    waterloo Repository record for Electrolyte/Membrane Design and Engineering for Durable Zinc-Iodine Redox Flow Batteries (opens in a new tab)