Global ETD Search
Search theses and dissertations gathered from participating repositories worldwide. Every result links back to the library that holds it. No account is needed.
Results 1 to 20 of 36 for “"corrosion morphology"”
-
The role of galvanic coupling effect in determining crevice corrosion morphology
<p>The galvanic nature of crevice corrosion is a generally accepted concept but the coupled electrochemical behaviour and its role in crevice corrosion has not been really studied until recently. Among many arguments regarding the mechanism of crevice corrosion, whether or not being able to …
-
Electrochemical Characterization of Intermetallic Compounds in AA2024-T3 and Localized Corrosion Morphology of Al-Cu-Mg at Elevated Temperature
The localized corrosion behavior of Al-Cu-Mg alloy AA2024-T3 (Al-4.4Cu-2.5Mg-0.6Mn) at temperatures from 10 to 70 oC was characterized using a range of experimental techniques and approaches. Foremost among these was a characterization of the electrochemical behavior of constituent particles …
-
Effects of hydrodynamic variables on corrosion : study of 90/10 Cu-Ni in a circling foil with synthetic seawater
… hydrodynamic variables and fluid properties on corrosion of 90/10 Cu-Ni (CDA 706) in single metal exposures and in galvanic couples with platinum were studied in synthetic seawater. An apparatus utilizing circling foil as the specimen holder was redesigned as an experimental apparatus for this …
-
Embrittlement susceptibility of corroded pre-stressing steel in concrete during cathodic polarization
… as a function of the magnitude of prestrain and corrosion morphology of the wire. These results were tabulated in a format that can be used during field inspection to identify structural elements for which fracture could occur upon application of cathodic protection.
-
Interfacial Electrochemistry of Cu/Al Alloys for IC Packaging and Chemical Bonding Characterization of Boron Doped Hydrogenated Amorphous Silicon Films for Infrared Cameras
… theoretical calculations. The study revealed the corrosion morphology progression on aluminum alloy (Al, 0.5% Cu) under acidic chloride solution. This is due to defects and a higher copper content at the grain boundary. Direct galvanic current measurement, linear sweep voltammetry (LSV), and Tafel …
-
Mechanistic modelling of localised corrosion in multi-phase Al-Zn-Mg-Si coatings for the protection of steel
Corrosion remains a persistent challenge for engineering materials, affecting the longevity of metallic structures across diverse environments. Among the strategies developed to mitigate the corrosion of steel (which is the most widely used metallic material), metallic coatings - often termed …
-
On the intergranular corrosion of 7xxx aluminum alloys
… structure are very susceptible to intergranular corrosion (IGC). From a practical point of view, it is important to understand IGC in these alloys. Measuring the kinetics of IGC is not only a way to evaluate corrosion susceptibility, but also very useful for a predictive model for corrosion. …
-
Study of corrosion-induced failure mechanisms of epoxy-coated reinforcing steel
A study of the corrosion protection afforded by epoxy coatings on reinforcing steel was performed. To accomplish this bars were acquired from ten sources and coatings were characterized in terms of defects, thickness, solvent extraction weight loss and hardness. Testing involved exposure in various …
-
Corrosion evaluation of Super 13Cr martensitic stainless steel under high temperature and high pressure downhole environments
… owing to its excellent mechanical properties and corrosion resistance. Nevertheless, its corrosion behaviour under extreme downhole conditions remains to be further investigation investigated to facilitate its application and modification. The current study aimed to identify the failure modes of …
-
Corrosion Behavior of Automotive Al-Mg-Si Alloys and Assessment of the Ability of Accelerated Corrosion Tests to Predict On-road Corrosion of these Alloys
… steels. Although Al alloys usually have good corrosion resistance, they can be susceptible to localized corrosion when subjected to environments with corrosive salts, like wet winter roads. It is necessary to evaluate the corrosion resistance of Al alloys in a way that properly simulates …
-
Assessment of the corrosion behaviour of alloys 825 and 625 in stagnant seawater-effect of temperature and welding
… wellheads, risers and valves. The outstanding corrosion resistance of alloy 825 against general and localised corrosion attack is attributed to its high Ni, Cr and Mo content. However, corrosion failures of alloy 825 equipment have been observed in offshore environments. Alloy 825 has good …
-
Análise de falhas, monitoramento e controle da corrosão em processo industrial de produção de biodiesel
… of hydrochloric acid solution. Considering that corrosion is an important degradation mechanism in the company's biodiesel plants, in order to develop and implement adequate means for its prevention, this work includes field evaluations, in-service and laboratory tests, involving techniques …
-
Electrochemical Studies of Molten Salt Corrosion
Corrosion mechanisms of Fe-Ni and Fe-22Cr-Ni model alloys with varying Ni contents and Ni-22Cr model alloy were investigated in molten chloride salts at 350-700 °C, simulating the heat transfer circuits of molten salt reactors and thermal solar plants.This study revealed that corrosion properties …
-
Corrosion Behaviour of Electrodeposited Nanocrystalline Nickel (Ni) and Nickel-Iron (NiFe) Alloys Compared to their Polycrystalline Coarse-Grained Counterparts
The corrosion behaviour of electrodeposited nanocrystalline Ni, 85Ni-15Fe, 80Ni-20Fe and 45Ni-55Fe was assessed in sulfate electrolytes and compared to their coarse-grained counterparts. The effect of grain size reduction on the corrosion behaviour of Ni and NiFe alloys was minimal, in particular …
-
Characterization of Copper Coatings at the Closure Weld Zone for Canada’s Used Nuclear Fuel Containers
… of Canada’s spent nuclear fuel. A 3 mm-thick corrosion resistant copper coating on 41 mm-thick structural mild steel core is fabricated using a combination of electrodeposition (ED) and cold spray (CS) technologies. The UFCs will be exposed to corrosive environments transitioning from aerobic …
-
The effect of Ce Microalloying and Thermomechanical Processesing on The Corrosion Behaviour of TS Cast AA5182 Aluminum Alloy
… its low density, good formability, strength, and corrosion resistance. However, its durability in aggressive environments can be compromised by localized corrosion, particularly pitting and intergranular attack. These degradation modes are influenced by microstructural heterogeneities, including …
-
Crevice corrosion behaviour of nickel based alloys in neutral chloride solutions
Crevice corrosion experiments have been conducted on Inconel 600 and Inconel 625 exposed to two principle test solutions of 1 M NaCl and 1 M NaCl + 0.01 M Na₂S₂0₃ (Sodium Thiosulphate) at three temperatures, 22°C, 55 °C and 80°C. The crevice corrosion tests were performed in a corrosion cell which …
-
Corrosion Studies on Lightweight Automotive Alloys: The Effect of Microstructure and Fundamental Mechanisms
… applications is severely hindered by their poor corrosion resistance in aqueous environments. Despite intensive research effort, the underlying mechanism(s) responsible for this poor corrosion resistance remains elusive. Further complicating the situation is the presence of secondary …
-
Stress corrosion cracking and hydrogen embrittlement of baseline and prototype steels in a cyclic corrosion test chamber
… However, their susceptibility to stress corrosion cracking (SCC) and hydrogen embrittlement (HE) under marine exposure remains a significant concern. This thesis investigates the SCC and HE behavior of HY-100, 10Ni QQT*, and 10Ni QQLT* steels subjected to the GMW 14872 cyclic corrosion …
-
Evaluating the Potential for Atmospheric Corrosion of 304 Stainless Steel Used for Dry Storage of Spent Nuclear Fuel
… moisture from the air leading to atmospheric corrosion concerns. While most research has focused on the initial stages of atmospheric corrosion ranging from 1 day to 1 week under singular microliter-sized droplets, there is a gap in understanding the effect of atmospheric exposure on pitting …
Page 1 of 2